AT40900B - Verfahren zur Herstellung festhaftender, glänzender, elektrolytischer Zinkniederschläge. - Google Patents
Verfahren zur Herstellung festhaftender, glänzender, elektrolytischer Zinkniederschläge.Info
- Publication number
- AT40900B AT40900B AT40900DA AT40900B AT 40900 B AT40900 B AT 40900B AT 40900D A AT40900D A AT 40900DA AT 40900 B AT40900 B AT 40900B
- Authority
- AT
- Austria
- Prior art keywords
- shiny
- production
- firmly adhering
- electrolytic zinc
- zinc deposits
- Prior art date
Description
<Desc/Clms Page number 1> Verfahren zur Herstellung festhaftender, glänzende, elektrolytischer Zinkniederschläge. Zur Erhöhung der Festigkeit und Dauerhaftigkeit elektrolytischer Metallniederschläge wurden, wie dies z. B. in der deutschen Patentschrift Nr. 61845 erwähnt ist, den Bädern Zuckerarten oder zuckerhaltige Pflanzen säfte beigemengt ; dabei wurde aber die Beobachtung gemacht, dass die günstige Einwirkung des Zuckerzusatzes nur kurze Zeit währt und sich erst. dann wieder in verstärktem Masse zeigt, wenn das Bad durch längere Zeit in Ruhe war. Die diesbezüglich angestellten Versuche haben ergeben, dass der günstige Einfluss des Zusatzes von Zuckerarten oder zuckerhaltiges Pflanzensaftes wesentlich erhöht wird, wenn zu den letzteren ein Zusatz eines Gährungserregers wie z. B. Hefe erfolgt. Es entsteht nämlich unter Anwendung eines mit Hefe vermengten zuckerhaltigen Zinkbades ein festhaftender homogener Zinküberzug mit lebhaftem Metallglanze. Als Ausführungsbeispiel des diesbezüglichen Verfahrens sei die folgende Zusammen- EMI1.1 I ; 11 C abgekühlt ist, zur Verzinkung fertig und entsteht beim Durchgang des elektrischen Stromes unter den, für Zinkniederschläge üblichen Stromverhältnissen, beispielsweise bei einer Spannung von Volt und einer Stromdichte von 3'3 Amp. schon nach 10 Minuten ein äusserst lebhaft glänzender, homogener Zinküberzug auf der Kathode. Das Bad ist bei entsprechender Modifikation des Elektrolyten auch für andere metalle verwendbar. **WARNUNG** Ende DESC Feld kannt Anfang CLMS uberlappen**.
Claims (1)
- PATKNT. ANSPRUCH : EMI1.2 **WARNUNG** Ende CLMS Feld Kannt Anfang DESC uberlappen**.