DE1621337B2 - Bad fuer die stromlose nickelabscheidung - Google Patents
Bad fuer die stromlose nickelabscheidungInfo
- Publication number
- DE1621337B2 DE1621337B2 DE19671621337 DE1621337A DE1621337B2 DE 1621337 B2 DE1621337 B2 DE 1621337B2 DE 19671621337 DE19671621337 DE 19671621337 DE 1621337 A DE1621337 A DE 1621337A DE 1621337 B2 DE1621337 B2 DE 1621337B2
- Authority
- DE
- Germany
- Prior art keywords
- nickel
- hypophosphite
- liter
- bath
- ions
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C18/00—Chemical coating by decomposition of either liquid compounds or solutions of the coating forming compounds, without leaving reaction products of surface material in the coating; Contact plating
- C23C18/16—Chemical coating by decomposition of either liquid compounds or solutions of the coating forming compounds, without leaving reaction products of surface material in the coating; Contact plating by reduction or substitution, e.g. electroless plating
- C23C18/31—Coating with metals
- C23C18/32—Coating with nickel, cobalt or mixtures thereof with phosphorus or boron
- C23C18/34—Coating with nickel, cobalt or mixtures thereof with phosphorus or boron using reducing agents
- C23C18/36—Coating with nickel, cobalt or mixtures thereof with phosphorus or boron using reducing agents using hypophosphites
Landscapes
- Chemical & Material Sciences (AREA)
- General Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Engineering & Computer Science (AREA)
- Materials Engineering (AREA)
- Mechanical Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Chemically Coating (AREA)
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US54106066A | 1966-04-08 | 1966-04-08 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| DE1621337B2 true DE1621337B2 (de) | 1971-05-13 |
| DE1621337A1 DE1621337A1 (OSRAM) | 1971-05-13 |
Family
ID=24158027
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| DE19671621337 Pending DE1621337B2 (de) | 1966-04-08 | 1967-04-04 | Bad fuer die stromlose nickelabscheidung |
Country Status (6)
| Country | Link |
|---|---|
| US (1) | US3420680A (OSRAM) |
| BE (1) | BE695663A (OSRAM) |
| DE (1) | DE1621337B2 (OSRAM) |
| FR (1) | FR1515425A (OSRAM) |
| GB (1) | GB1107146A (OSRAM) |
| NL (1) | NL6704756A (OSRAM) |
Families Citing this family (8)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE1521350C3 (de) * | 1966-08-06 | 1975-09-11 | Hoechst Ag, 6000 Frankfurt | Verfahren zur chemischen Vernickelung von nichtmetallischen Gegenständen |
| US3649350A (en) * | 1970-06-29 | 1972-03-14 | Gen Electric | Electroless copper plating |
| DE2650873A1 (de) * | 1976-11-06 | 1978-05-11 | Philips Patentverwaltung | Verfahren zur herstellung eines elektromagneten |
| US4188227A (en) * | 1977-05-27 | 1980-02-12 | Bauer Randy L | Method of preparing multi-component chemical compositions |
| US4467067A (en) * | 1982-12-27 | 1984-08-21 | Shipley Company | Electroless nickel plating |
| US4997686A (en) * | 1987-12-23 | 1991-03-05 | Surface Technology, Inc. | Composite electroless plating-solutions, processes, and articles thereof |
| JP2000503354A (ja) * | 1996-11-14 | 2000-03-21 | アトテク ドイツェラント ゲーエムベーハー | 無電解ニッケルめっき浴からのオルト亜燐酸塩イオンの除去 |
| EP1306465B1 (en) * | 2001-10-24 | 2011-03-16 | Rohm and Haas Electronic Materials LLC | Stabilizers for electroless plating solutions and methods of use thereof |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE1243493B (de) * | 1961-02-04 | 1967-06-29 | Bayer Ag | Waessriges Bad zur chemischen Abscheidung von borhaltigen Metallueberzuegen |
-
1966
- 1966-04-08 US US541060A patent/US3420680A/en not_active Expired - Lifetime
-
1967
- 1967-02-28 GB GB9476/67A patent/GB1107146A/en not_active Expired
- 1967-03-17 FR FR99291A patent/FR1515425A/fr not_active Expired
- 1967-03-17 BE BE695663D patent/BE695663A/xx unknown
- 1967-04-04 DE DE19671621337 patent/DE1621337B2/de active Pending
- 1967-04-04 NL NL6704756A patent/NL6704756A/xx unknown
Also Published As
| Publication number | Publication date |
|---|---|
| FR1515425A (fr) | 1968-03-01 |
| US3420680A (en) | 1969-01-07 |
| NL6704756A (OSRAM) | 1967-10-09 |
| BE695663A (OSRAM) | 1967-09-18 |
| GB1107146A (en) | 1968-03-20 |
| DE1621337A1 (OSRAM) | 1971-05-13 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| DE1197720B (de) | Verfahren zur Vorbehandlung von insbesondere dielektrischen Traegern vor der stromlosen Metallabscheidung | |
| DE3601698C2 (OSRAM) | ||
| DE1001078B (de) | Galvanische Baeder zur Herstellung von Metallueberzuegen | |
| DE2049038C3 (de) | Wäßriges saures galvanisches Verchromungsbad | |
| DE2229012C3 (de) | Wässrige, Benztriazol und Tolyltriazol enthaltende Lösung mit die Korrosion von Metallen hemmender Wirkung | |
| DE1621337B2 (de) | Bad fuer die stromlose nickelabscheidung | |
| DE2943049C2 (OSRAM) | ||
| DE2559059A1 (de) | Stabilisierte metallplattierungsloesung und verfahren zu ihrer herstellung | |
| DE3400670A1 (de) | Waessriges goldsulfit enthaltendes galvanisches bad und verfahren zur galvanischen abscheidung von gold unter verwendung dieses bades | |
| DE3038805A1 (de) | Neutrale zinnelektroplattierungsbaeder | |
| DE1621337C (de) | Bad fur die stromlose Nickelabschei dung | |
| DE3421646A1 (de) | Waessriges bad zur stromlosen vernickelung und ein verfahren zur stromlosen vernickelung eines substrats mit diesem bad | |
| DE2650389A1 (de) | Bad fuer die chemische nickelabscheidung | |
| DE1194674B (de) | Verfahren zum Regenerieren von Chromatierungsloesungen | |
| DE3135597C2 (de) | Verfahren zur Auffrischung einer Palladium/Nickel-Legierung-Plattierungslösung mit Palladium | |
| DE1908595A1 (de) | Stromlosplattierbad | |
| DE1521490C3 (OSRAM) | ||
| DE843785C (de) | Verfahren zur Herstellung harter galvanischer Silberueberzuege | |
| DE1796110C3 (de) | Wässriges Bad zur galvanischen Abscheidung glänzender und porenfreier Palladiumüberzüge | |
| DE1920152C3 (de) | Chemisches Nickelbad | |
| DE1928307C (de) | Bad und Verfahren zum Glänzen von Werkstücken mit Oberflächen aus Eisen oder Eisenlegierungen | |
| DE1496904B2 (de) | Verfahren zur verhinderung einer nebelbildung beim betrieb von galvanischen chrombaedern | |
| DE2112936C3 (de) | Mittel zum Beizen von Kupfer oder Kupferlegierung, enthaltend Schwefelsäure, Wasserstoffperoxid und mindestens einen organischen Stabilisator | |
| DE1032636B (de) | Ergaenzungsloesung zur Verringerung der Zunahme der Alkalitaet in cyanidischen Baedern zur galvanischen Abscheidung von Goldlegierungen | |
| DE1521491C2 (de) | Wäßriges, alkalisches Bad zur stromlosen Kupferabscheldung |