KR900016325A KR1019890005258A KR890005258A KR900016325A KR 900016325 A KR900016325 A KR 900016325A KR 1019890005258 A KR1019890005258 A KR 1019890005258A KR 890005258 A KR890005258 A KR 890005258A KR 900016325 A KR900016325 A KR 900016325A
Authority
KR
South Korea
Prior art keywords
aromatic
transparent film
amorphous
stretching
aromatic polymer
Prior art date
Application number
KR1019890005258A
Other languages
English (en)
Other versions
KR0133290B1 (ko
Inventor
사다오 후지이
준지 다까세
히데끼 가와이
Original Assignee
신노오 마꼬히또
가네가후찌 가가꾸고교 가부시끼가이샤
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Family has litigation
First worldwide family litigation filed litigation Critical https://patents.darts-ip.com/?family=14291851&utm_source=google_patent&utm_medium=platform_link&utm_campaign=public_patent_search&patent=KR900016325(A) "Global patent litigation dataset” by Darts-ip is licensed under a Creative Commons Attribution 4.0 International License.
Application filed by 신노오 마꼬히또, 가네가후찌 가가꾸고교 가부시끼가이샤 filed Critical 신노오 마꼬히또
Publication of KR900016325A publication Critical patent/KR900016325A/ko
Application granted granted Critical
Publication of KR0133290B1 publication Critical patent/KR0133290B1/ko

Links

Classifications

    • CCHEMISTRY; METALLURGY
    • C08ORGANIC MACROMOLECULAR COMPOUNDS; THEIR PREPARATION OR CHEMICAL WORKING-UP; COMPOSITIONS BASED THEREON
    • C08JWORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H
    • C08J5/00Manufacture of articles or shaped materials containing macromolecular substances
    • C08J5/18Manufacture of films or sheets
    • GPHYSICS
    • G02OPTICS
    • G02BOPTICAL ELEMENTS, SYSTEMS OR APPARATUS
    • G02B5/00Optical elements other than lenses
    • G02B5/30Polarising elements
    • G02B5/3083Birefringent or phase retarding elements

Abstract

내용 없음.

Description

복굴절 투명 필름 및 이의 제조방법
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음

Claims (10)

  1. 주요 성분으로서 비대칭적으로 연신된 무정형 방향족 중합체를 함유하는, 복굴절성을 갖는 투명 필름.
  2. 제1항에 있어서, 무정형 방향족 중합체가 방향족 폴리에스테르, 방향족 폴리설폰 및 방향족 폴리에테르설폰중에서 선택되는 투명 필름.
  3. 제1항에 있어서, 무정형 방향족 중합체가 방향족 폴리에스테르인 투명 필름.
  4. 제1항에 있어서, 필름의 동일 평면내 서로에 대한 직각에서 두 방향사이의 굴절각의 차이가 0.0001 내지 0.2인 투명 필름.
  5. 주요 성분으로서 무정형 방향족 중합체를 함유하는 필름을 비대칭적으로 연신시킴을 특징으로 하여, 복굴절성을 갖는 투명 필름을 제조하는 방법.
  6. 제5항에 있어서, 무정형 방향족 중합체가 방향족 폴리에스테르, 방향족 폴리설폰 및 방향족 폴리에테르 설폰중에서 선택되는 방법.
  7. 제5항에 있어서, 무정형 방향족 중합체가 방향족 폴리에스테르인 방법.
  8. 제5항에 있어서, 비대칭적 연신을 실온 내지 상기 무정형 방향족 중합체의 40℃이상의 유리 전이 온도에서 수행하는 방법.
  9. 제5항에 있어서, 비대칭적 연신이 단축적 연신인 방법.
  10. 제5항에 있어서, 비대칭적 연신이 이축적 연신인 방법.
    ※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.
KR1019890005258A 1988-04-22 1989-04-21 복굴절 투명필름 및 이의 제조방법 KR0133290B1 (ko)

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
JP63101107A JP2968531B2 (ja) 1988-04-22 1988-04-22 複屈折性を有する透明フィルム及びその製造方法
JP63-101107 1989-04-22

Publications (2)

Publication Number Publication Date
KR900016325A true KR900016325A (ko) 1990-11-13
KR0133290B1 KR0133290B1 (ko) 1998-04-13

Family

ID=14291851

Family Applications (1)

Application Number Title Priority Date Filing Date
KR1019890005258A KR0133290B1 (ko) 1988-04-22 1989-04-21 복굴절 투명필름 및 이의 제조방법

Country Status (5)

Country Link
US (1) US4985531A (ko)
EP (1) EP0338575B2 (ko)
JP (1) JP2968531B2 (ko)
KR (1) KR0133290B1 (ko)
DE (1) DE68916683T3 (ko)

Families Citing this family (12)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2988636B2 (ja) * 1990-11-28 1999-12-13 鐘淵化学工業株式会社 光学等方性を有するポリアリレートフィルムおよびその製造方法
JP3051473B2 (ja) * 1991-02-08 2000-06-12 鐘淵化学工業株式会社 透明導電性フィルム
US5645766A (en) * 1995-03-30 1997-07-08 Teijin Limited Film of aromatic polyethersulfone process for the production thereof and solution composition for the production thereof
DE69520936T2 (de) * 1995-03-31 2001-08-30 Teijin Ltd Folie aus einem aromatischen Polyethersulfon, Verfahren zu ihrer Herstellung und Lösungszusammensetzung zu ihrer Herstellung
JPH10332938A (ja) * 1998-06-05 1998-12-18 Kanegafuchi Chem Ind Co Ltd 複屈折性を有する透明フィルム及びその製造方法
JP3719374B2 (ja) * 2000-07-14 2005-11-24 シャープ株式会社 偏光素子の製造方法
JP2002275290A (ja) * 2002-03-07 2002-09-25 Kanegafuchi Chem Ind Co Ltd 耐熱透明フィルム
US20070154654A1 (en) * 2005-12-29 2007-07-05 Eastman Kodak Company Optical compensator film with controlled birefringence dispersion
JP2008169384A (ja) * 2006-12-14 2008-07-24 Kaneka Corp コーティング用樹脂、光学補償用薄膜、光学補償用積層体、光学補償用偏光板、及び液晶表示装置。
US7943219B2 (en) * 2007-03-23 2011-05-17 Kimberly-Clark Worldwide, Inc. Films and articles with reversible opacity change upon stretching, and methods of making and using same
TWI354127B (en) * 2007-11-08 2011-12-11 Ind Tech Res Inst Optical film with low or zero birefringence and me
JP5471249B2 (ja) * 2009-02-06 2014-04-16 大日本印刷株式会社 偏光板保護フィルム、偏光板、および液晶表示装置

Family Cites Families (13)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US2928295A (en) * 1955-04-22 1960-03-15 Boulanger Etienne Variable speed transmission device
CA1017097A (en) * 1962-11-06 1977-09-06 Imperial Chemical Industries Limited Manufacture of polysulphones
JPS56130703A (en) * 1980-03-18 1981-10-13 Toyobo Co Ltd Quarter wavelength film
JPS5762011A (en) 1980-09-30 1982-04-14 Nitto Electric Ind Co Ltd Polarizing plate
JPS5730808A (en) 1980-07-31 1982-02-19 Nitto Electric Ind Co Ltd Polarizing plate
JPS62135338A (ja) * 1985-12-09 1987-06-18 Diafoil Co Ltd 液晶パネル基板用ポリエチレンナフタレ−ト一軸高配向フイルム
CA1307151C (en) * 1987-02-02 1992-09-08 Shuji Kitamura Phase retarder
DE3884291T2 (de) 1987-06-30 1994-03-31 Sumitomo Chemical Co Phasenverzögernde Polymerfilme und polarisierende Bauteile.
JP2686751B2 (ja) * 1987-11-12 1997-12-08 藤森工業 株式会社 光学的位相機能を有する積層体
US4942087A (en) * 1987-12-28 1990-07-17 Mitsui Petrochemical Industries, Ltd. Films of wholly aromatic polyester and processes for preparation thereof
JPH01201607A (ja) * 1988-02-08 1989-08-14 Fuji Photo Film Co Ltd 位相差フイルムの製造方法
JPH01201608A (ja) * 1988-02-08 1989-08-14 Fuji Photo Film Co Ltd 位相差フイルムの製造方法
JPH04112190A (ja) 1990-07-17 1992-04-14 Kobe Steel Ltd 旋回式クレーン

Also Published As

Publication number Publication date
JP2968531B2 (ja) 1999-10-25
EP0338575A3 (en) 1990-05-23
DE68916683D1 (de) 1994-08-18
KR0133290B1 (ko) 1998-04-13
JPH01270004A (ja) 1989-10-27
DE68916683T3 (de) 2004-09-30
EP0338575A2 (en) 1989-10-25
DE68916683T2 (de) 1994-11-03
EP0338575B1 (en) 1994-07-13
US4985531A (en) 1991-01-15
EP0338575B2 (en) 2004-01-07

Similar Documents

Publication Publication Date Title
KR900016325A (ko) 복굴절 투명 필름 및 이의 제조방법
EP0367288A3 (en) Liquid crystal display
KR920010316A (ko) 복굴절성 간섭 편광자
BR9408143A (pt) Filme termo-contrátil polímero processo para a preparação de filme e concentrado de poliéster/plastificante que é usado para preparar o filme
KR910002968A (ko) 폴리이미드필름 및 그 제조 방법
EP0740168A4 (en) NON-BIREFRINGENT OPTICAL RESIN, MANUFACTURING METHOD THEREOF, AND ARTICLE OF LIQUID CRYSTAL ELEMENTS USING SUCH RESIN
EP0363919A3 (en) Shape memory film
KR870006428A (ko) 편광판(polarizing plates)용 1축 고배향(高配向) 폴리에틸렌 나프탈레이트의 필름
KR950019813A (ko) 위상차 필름의 제조방법
WO2003034102A3 (en) Waveplate and optical circuit formed from mesogen-containing polymer
KR940701551A (ko) 액정 디스플레이용 위상판
KR850000227A (ko) 홈이 있는 광전송로
JPH04371903A (ja) 偏光板及び液晶表示装置
KR950033571A (ko) 위상차 필름 및 그의 제조방법
KR900015919A (ko) 배향 복합 폴리에스테르 필름
KR960018621A (ko) 광학 이방체 필름, 이의 제조방법 및 액정 표시장치
KR860003289A (ko) 적층필름의 제조방법
JPH0313916A (ja) 位相差板およびこれを用いた液晶電気光学素子
KR930000576A (ko) 반결정성 폴리올레핀으로 제조된 편광막 및 그를 제조하는 방법
KR880010339A (ko) 상 리타더
KR880004447A (ko) 광학적 정보 기록 매체
KR950002978A (ko) 편광특성을 개선시킨 적층체 및 그를 위한 이형필림
KR900000712A (ko) 플라스틱 광학 위상판
KR930002064A (ko) 이방성이 적고 횡방향으로 배향된 폴리에스테르 필름의 제조방법
KR870000157A (ko) 쌍측연신 폴리―ε―카프라미드 필름의 제조방법

Legal Events

Date Code Title Description
A201 Request for examination
E701 Decision to grant or registration of patent right
GRNT Written decision to grant
FPAY Annual fee payment

Payment date: 20051208

Year of fee payment: 9

LAPS Lapse due to unpaid annual fee