JP5517622B2 - モノマー溶液の液滴の重合による吸収性ポリマー粒子の製造法 - Google Patents
モノマー溶液の液滴の重合による吸収性ポリマー粒子の製造法 Download PDFInfo
- Publication number
- JP5517622B2 JP5517622B2 JP2009530870A JP2009530870A JP5517622B2 JP 5517622 B2 JP5517622 B2 JP 5517622B2 JP 2009530870 A JP2009530870 A JP 2009530870A JP 2009530870 A JP2009530870 A JP 2009530870A JP 5517622 B2 JP5517622 B2 JP 5517622B2
- Authority
- JP
- Japan
- Prior art keywords
- droplets
- monomer solution
- monomer
- polymer particles
- water
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Description
a)少なくとも1つのエチレン性不飽和モノマー、
b)少なくとも1つの架橋剤、
c)少なくとも1つの開始剤、
d)水
を含有する液滴を、該液滴を取り囲んでいる気相中で重合させることによって吸水性ポリマー粒子を製造する方法において、開始剤c)をモノマー溶液に、液滴作製の0.5〜60秒前に添加することを特徴とする方法によって解決された。
残留モノマー(Residual monomers)
吸水性ポリマー粒子の残留モノマーは、EDANA(European Disposables and Nonwovens Association)により推奨された試験方法No.410.2−02"Residual monomers"に従って測定される。
吸水性ポリマー粒子の遠心保持容量は、EDANA(European Disposables and Nonwovens Association)により推奨された試験法No.441.2−02"Centrifuge retention capacity"に従って測定される。
吸水性ポリマー粒子の抽出分の含有率(抽出可能な割合)は、EDANA(European Disposables and Nonwovens Association)により推奨された試験法No.470.2−02"Extractable"に従って測定される。
実施例1
アクリル酸ナトリウム14.3kg(水中で37.5質量%の溶液)、アクリル酸1.4kgおよび水350gを、15箇所エトキシル化されたトリメチロールプロパントリアクリレート22gと混合した。該溶液を、加熱され、窒素雰囲気で満たされた液滴化塔(Vertropfungsturm)(180℃、高さ12m、幅2m、並流で0.1m/sのガス速度)内に液滴化した。モノマー溶液の配量速度は32kg/hで、モノマー溶液の温度は25℃であった。液滴化プレートは、200μmのサイズ毎に60個の穿孔を有していた。液滴化装置は、40mmの内径と2mmの内法高さを有していた。開始剤を、液滴化装置の前で、スタティックミキサーを介してモノマー溶液中に配量した。開始剤として、水中で3質量%の2,2′−アゾビス[2−(2−イミダゾリン−2−イル)プロパン]ジヒドロクロリドの溶液を使用した。開始剤溶液の配量速度は2.2kg/hで、開始剤溶液の温度は25℃であった。ミキサーと液滴化装置とは直接互いに接続していた。
アクリル酸ナトリウム14.3kg(水中で37.5質量%の溶液)、アクリル酸1.4kgおよび水350gを、15箇所エトキシル化されたトリメチロールプロパントリアクリレート22gと混合した。該溶液を、加熱され、窒素雰囲気で満たされた液滴化塔(180℃、高さ12m、幅2m、並流で0.1m/sのガス速度)内に液滴化した。モノマー溶液の配量速度は16kg/hで、モノマー溶液の温度は25℃であった。液滴化プレートは、200μmのサイズ毎に30個の穿孔を有していた。液滴化装置は、40mmの内径と2mmの内法高さを有していた。開始剤を、液滴化装置の前で、スタティックミキサーを介してモノマー溶液中に配量した。開始剤として、水中で3質量%の2,2′−アゾビス[2−(2−イミダゾリン−2−イル)プロパン]ジヒドロクロリドの溶液を使用した。開始剤溶液の配量速度は1.1kg/hで、開始剤溶液の温度は25℃であった。開始剤添加から液滴作製までの滞留時間は、ミキサーから液滴化装置までの管路の長さによって調整される。
Claims (10)
- a)少なくとも1つのエチレン性不飽和モノマー、
b)少なくとも1つの架橋剤、
c)少なくとも1つの開始剤、
d)水
を含有する液滴を、該液滴を取り囲んでいる気相中で重合させることによる吸水性ポリマー粒子の製造法において、開始剤c)をモノマー溶液に、液滴作製の0.5〜60秒前に添加することを特徴とする、吸水性ポリマー粒子の製造法。 - 前記開始剤c)を前記モノマー溶液に添加した後、前記液滴作製の前にスタティックミキサーで混合することを特徴とする、請求項1記載の方法。
- 前記モノマー溶液の酸素含有量が少なくとも1質量ppmであることを特徴とする、請求項1または2記載の方法。
- 前記モノマー溶液が、前記エチレン性不飽和モノマーa)に対して、160質量ppm未満の重合禁止剤を含有することを特徴とする、請求項1から3までのいずれか1項記載の方法。
- 前記重合禁止剤がヒドロキノンモノメチルエーテルであることを特徴とする、請求項4記載の方法。
- 前記液滴が少なくとも200μmの平均直径を有することを特徴とする、請求項1から5までのいずれか1項記載の方法。
- 前記モノマーa)が少なくとも1個の酸基を有することを特徴とする、請求項1から6までのいずれか1項記載の方法。
- 前記モノマーa)の酸基が、少なくとも部分的に中和されていることを特徴とする、請求項7記載の方法。
- 前記モノマーa)の少なくとも50モル%がアクリル酸であることを特徴とする、請求項1から8までのいずれか1項記載の方法。
- 得られた前記ポリマー粒子を、少なくとも1つのさらに別の方法工程において乾燥および/または後架橋させることを特徴とする、請求項1から9までのいずれか1項記載の方法。