JP2011509349A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2011509349A5 JP2011509349A5 JP2010541600A JP2010541600A JP2011509349A5 JP 2011509349 A5 JP2011509349 A5 JP 2011509349A5 JP 2010541600 A JP2010541600 A JP 2010541600A JP 2010541600 A JP2010541600 A JP 2010541600A JP 2011509349 A5 JP2011509349 A5 JP 2011509349A5
- Authority
- JP
- Japan
- Prior art keywords
- corrosion
- metal substrate
- resistant metal
- resistant
- manufacturing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Applications Claiming Priority (7)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US1965708P | 2008-01-08 | 2008-01-08 | |
| US61/019,657 | 2008-01-08 | ||
| US2327308P | 2008-01-24 | 2008-01-24 | |
| US61/023,273 | 2008-01-24 | ||
| US8923308P | 2008-08-15 | 2008-08-15 | |
| US61/089,233 | 2008-08-15 | ||
| PCT/US2009/030475 WO2009089376A2 (en) | 2008-01-08 | 2009-01-08 | Highly electrically conductive surfaces for electrochemical applications |
Related Child Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2014004549A Division JP5995882B2 (ja) | 2008-01-08 | 2014-01-14 | 電気化学的用途のための高導電性表面 |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2011509349A JP2011509349A (ja) | 2011-03-24 |
| JP2011509349A5 true JP2011509349A5 (enExample) | 2012-03-01 |
| JP5512542B2 JP5512542B2 (ja) | 2014-06-04 |
Family
ID=40844828
Family Applications (2)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2010541600A Active JP5512542B2 (ja) | 2008-01-08 | 2009-01-08 | 電気化学的用途のための高導電性表面 |
| JP2014004549A Active JP5995882B2 (ja) | 2008-01-08 | 2014-01-14 | 電気化学的用途のための高導電性表面 |
Family Applications After (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2014004549A Active JP5995882B2 (ja) | 2008-01-08 | 2014-01-14 | 電気化学的用途のための高導電性表面 |
Country Status (7)
| Country | Link |
|---|---|
| US (2) | US9765421B2 (enExample) |
| EP (1) | EP2229471B1 (enExample) |
| JP (2) | JP5512542B2 (enExample) |
| KR (1) | KR101559604B1 (enExample) |
| CN (2) | CN101918619A (enExample) |
| DK (1) | DK2229471T3 (enExample) |
| WO (1) | WO2009089376A2 (enExample) |
Families Citing this family (48)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN101918619A (zh) | 2008-01-08 | 2010-12-15 | 特来德斯通技术公司 | 用于电化学应用的高导电性表面 |
| KR20120041198A (ko) * | 2009-06-18 | 2012-04-30 | 타타 스틸 리미티드 | 강 스트립상에 탄소 나노튜브(cnt) 및 탄소 나노섬유(cnf)의 직접 성장 방법 |
| JP2013506050A (ja) * | 2009-09-28 | 2013-02-21 | トレッドストーン テクノロジーズ インク. | 電気化学分野の製品のための高い電気伝導性を有する表面の形成方法 |
| JP2013514967A (ja) * | 2009-12-21 | 2013-05-02 | ウルトラ インコーポレイテッド | 高性能カーボンナノチューブエネルギー蓄積装置 |
| US8542465B2 (en) | 2010-03-17 | 2013-09-24 | Western Digital Technologies, Inc. | Suspension assembly having a microactuator electrically connected to a gold coating on a stainless steel surface |
| US8885299B1 (en) | 2010-05-24 | 2014-11-11 | Hutchinson Technology Incorporated | Low resistance ground joints for dual stage actuation disk drive suspensions |
| US8665567B2 (en) | 2010-06-30 | 2014-03-04 | Western Digital Technologies, Inc. | Suspension assembly having a microactuator grounded to a flexure |
| CN103534387B (zh) * | 2011-05-16 | 2016-03-16 | 松下知识产权经营株式会社 | 光电极及其制造方法、光电化学电池及使用该电池的能量系统、以及氢生成方法 |
| WO2012164992A1 (ja) * | 2011-06-03 | 2012-12-06 | パナソニック株式会社 | 電気接点部品 |
| US20130160948A1 (en) * | 2011-12-23 | 2013-06-27 | Lam Research Corporation | Plasma Processing Devices With Corrosion Resistant Components |
| FI2823079T3 (fi) | 2012-02-23 | 2023-05-04 | Treadstone Tech Inc | Korrosiota kestävä ja sähköä johtava metallin pinta |
| WO2013138619A1 (en) | 2012-03-16 | 2013-09-19 | Hutchinson Technology Incorporated | Mid-loadbeam dual stage actuated (dsa) disk drive head suspension |
| CN104205216A (zh) | 2012-03-22 | 2014-12-10 | 哈特奇桑科技公司 | 用于磁盘驱动器磁头悬架挠性件的接地特征 |
| US20140272566A1 (en) * | 2012-07-13 | 2014-09-18 | Konstyantyn Kylyvnyk | Weldability of aluminum alloys |
| WO2014043498A2 (en) | 2012-09-14 | 2014-03-20 | Hutchinson Technology Incorporated | Co-located gimbal-based dual stage actuation disk drive suspensions |
| JP6356682B2 (ja) | 2012-10-10 | 2018-07-11 | ハッチンソン テクノロジー インコーポレイテッドHutchinson Technology Incorporated | 二段作動構造を有するサスペンション |
| US8941951B2 (en) | 2012-11-28 | 2015-01-27 | Hutchinson Technology Incorporated | Head suspension flexure with integrated strain sensor and sputtered traces |
| US8891206B2 (en) | 2012-12-17 | 2014-11-18 | Hutchinson Technology Incorporated | Co-located gimbal-based dual stage actuation disk drive suspensions with motor stiffener |
| US9567681B2 (en) * | 2013-02-12 | 2017-02-14 | Treadstone Technologies, Inc. | Corrosion resistant and electrically conductive surface of metallic components for electrolyzers |
| WO2014134019A1 (en) * | 2013-02-26 | 2014-09-04 | Treadstone Technologies, Inc. | Corrosion resistance metallic components for batteries |
| US8896969B1 (en) | 2013-05-23 | 2014-11-25 | Hutchinson Technology Incorporated | Two-motor co-located gimbal-based dual stage actuation disk drive suspensions with motor stiffeners |
| US8717712B1 (en) | 2013-07-15 | 2014-05-06 | Hutchinson Technology Incorporated | Disk drive suspension assembly having a partially flangeless load point dimple |
| CN103811240B (zh) * | 2013-12-24 | 2017-01-25 | 兰州空间技术物理研究所 | 碳纳米管阴极的制备方法 |
| US8896970B1 (en) | 2013-12-31 | 2014-11-25 | Hutchinson Technology Incorporated | Balanced co-located gimbal-based dual stage actuation disk drive suspensions |
| US8867173B1 (en) | 2014-01-03 | 2014-10-21 | Hutchinson Technology Incorporated | Balanced multi-trace transmission in a hard disk drive flexure |
| CN104195496B (zh) * | 2014-08-20 | 2016-12-28 | 青岛申达众创技术服务有限公司 | 一种耐海水腐蚀金属涂层的制备方法 |
| US9070392B1 (en) | 2014-12-16 | 2015-06-30 | Hutchinson Technology Incorporated | Piezoelectric disk drive suspension motors having plated stiffeners |
| US9318136B1 (en) | 2014-12-22 | 2016-04-19 | Hutchinson Technology Incorporated | Multilayer disk drive motors having out-of-plane bending |
| US9296188B1 (en) | 2015-02-17 | 2016-03-29 | Hutchinson Technology Incorporated | Partial curing of a microactuator mounting adhesive in a disk drive suspension |
| WO2016168649A2 (en) * | 2015-04-15 | 2016-10-20 | Treadstone Technologies, Inc. | Method of metallic component surface moodification for electrochemical applications |
| JP6689294B2 (ja) | 2015-06-30 | 2020-04-28 | ハッチンソン テクノロジー インコーポレイテッドHutchinson Technology Incorporated | 金誘電体接合部の信頼性を向上させたディスクドライブヘッドサスペンション構造 |
| US10801097B2 (en) * | 2015-12-23 | 2020-10-13 | Praxair S.T. Technology, Inc. | Thermal spray coatings onto non-smooth surfaces |
| DE102016202372A1 (de) | 2016-02-17 | 2017-08-17 | Friedrich-Alexander-Universität Erlangen-Nürnberg | Schicht und Schichtsystem, sowie Bipolarplatte, Brennstoffzelle und Elektrolyseur |
| US9646638B1 (en) | 2016-05-12 | 2017-05-09 | Hutchinson Technology Incorporated | Co-located gimbal-based DSA disk drive suspension with traces routed around slider pad |
| CN106435324A (zh) * | 2016-10-31 | 2017-02-22 | 张家港沙工科技服务有限公司 | 一种机械设备用低电阻复合管 |
| KR102013836B1 (ko) * | 2017-07-03 | 2019-08-23 | 한국생산기술연구원 | 탄소계 물질 코팅층을 포함하는 탈염용 전극 및 이의 제조방법 |
| CN107681173A (zh) * | 2017-08-03 | 2018-02-09 | 上海交通大学 | 一种用于燃料电池金属极板的点状导电复合涂层 |
| DE102017118319A1 (de) * | 2017-08-11 | 2019-02-14 | Friedrich-Alexander-Universität Erlangen | Beschichtung und Schichtsystem, sowie Bipolarplatte, Brennstoffzelle und Elektrolyseur |
| CN108155258B (zh) * | 2017-12-22 | 2019-10-18 | 苏州佳亿达电器有限公司 | 一种耐腐蚀性强的薄膜太阳能电池柔性衬底 |
| US11885026B2 (en) | 2020-02-26 | 2024-01-30 | Treadstone Technologies, Inc. | Component having improved surface contact resistance and reaction activity and methods of making the same |
| JP7151892B2 (ja) | 2020-03-02 | 2022-10-12 | Jfeスチール株式会社 | 固体酸化物型燃料電池用フェライト系ステンレス鋼 |
| DE102020106742A1 (de) * | 2020-03-12 | 2021-09-16 | Auto-Kabel Management Gmbh | Elektrisches Kontaktteil sowie Verfahren zur Herstellung eines elektrischen Kontaktteils |
| DE102020210209A1 (de) | 2020-08-12 | 2022-02-17 | Ekpo Fuel Cell Technologies Gmbh | Bipolarplatte, Brennstoffzelle und Verfahren zur Herstellung einer Bipolarplatte |
| US12202723B2 (en) * | 2021-05-18 | 2025-01-21 | Analog Devices International Unlimited Company | Microelectromechanical systems (MEMS) switch and related methods |
| DE102022108476A1 (de) | 2022-04-07 | 2023-10-12 | Ekpo Fuel Cell Technologies Gmbh | Bipolarplatte, Brennstoffzelle und Verfahren zur Herstellung einer Bipolarplatte |
| CN115440407A (zh) * | 2022-08-03 | 2022-12-06 | 上海交通大学 | 一种耐腐蚀导电材料及其制备方法 |
| US20240072266A1 (en) * | 2022-08-31 | 2024-02-29 | Jfe Steel Corporation | Component for solid oxide fuel cell |
| CN115595605B (zh) * | 2022-10-27 | 2025-08-22 | 江阴市珞珈绿碳科技有限公司 | 一种用于熔盐电解二氧化碳制备碳材料体系的复合涂层阴极及其制备方法 |
Family Cites Families (81)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CH533691A (de) * | 1971-01-07 | 1973-02-28 | Metaux Precieux Sa | Procédé pour déposer une couche d'un alliage d'or violet sur un objet |
| US3755105A (en) * | 1971-06-28 | 1973-08-28 | G Messner | Vacuum electrical contacts for use in electrolytic cells |
| JPS582453B2 (ja) | 1975-02-28 | 1983-01-17 | 日本電気株式会社 | ダイキボハンドウタイシユウセキカイロソウチ |
| US4031268A (en) * | 1976-01-05 | 1977-06-21 | Sirius Corporation | Process for spraying metallic patterns on a substrate |
| JPS5569278A (en) * | 1978-11-17 | 1980-05-24 | Kureha Chem Ind Co Ltd | Frame of carbon fiber-high molecular composite material electrolytic cell |
| US4463818A (en) * | 1982-09-07 | 1984-08-07 | Applied Power Inc. | Tilt cab truck in which the cab is partially supported by the tilting cylinder while in the drive position |
| US4643818A (en) | 1984-08-07 | 1987-02-17 | Asahi Kasei Kogyo Kabushiki Kaisha | Multi-cell electrolyzer |
| CN1010760B (zh) * | 1984-11-13 | 1990-12-12 | 三菱电机株式会社 | 装饰板的制造方法 |
| US4706870A (en) * | 1984-12-18 | 1987-11-17 | Motorola Inc. | Controlled chemical reduction of surface film |
| JPS62107054A (ja) * | 1985-11-01 | 1987-05-18 | Sharp Corp | 精密パタ−ン製造方法 |
| JPH01301878A (ja) | 1988-05-31 | 1989-12-06 | Tanaka Kikinzoku Kogyo Kk | 電解用電極の製造方法 |
| US5314601A (en) * | 1989-06-30 | 1994-05-24 | Eltech Systems Corporation | Electrodes of improved service life |
| US5098485A (en) | 1990-09-19 | 1992-03-24 | Evans Findings Company | Method of making electrically insulating metallic oxides electrically conductive |
| JP2719049B2 (ja) | 1991-01-28 | 1998-02-25 | 日本碍子株式会社 | ランタンクロマイト膜の製造方法及び固体電解質型燃料電池用インターコネクターの製造方法 |
| SE505714C2 (sv) | 1991-09-19 | 1997-09-29 | Permascand Ab | Elektrod med kanalbildande trådar, sätt att tillverka elektroden, elektrolyscell försedd med elektroden samt sätt vid elektrolys |
| JPH09125292A (ja) * | 1995-11-01 | 1997-05-13 | Permelec Electrode Ltd | 電極基体 |
| US5624769A (en) | 1995-12-22 | 1997-04-29 | General Motors Corporation | Corrosion resistant PEM fuel cell |
| US5682067A (en) | 1996-06-21 | 1997-10-28 | Sierra Applied Sciences, Inc. | Circuit for reversing polarity on electrodes |
| EP0958410B1 (en) | 1997-01-31 | 2006-05-17 | Elisha Holding LLC | An electrolytic process for forming a mineral containing coating |
| US6153080A (en) | 1997-01-31 | 2000-11-28 | Elisha Technologies Co Llc | Electrolytic process for forming a mineral |
| US6322687B1 (en) | 1997-01-31 | 2001-11-27 | Elisha Technologies Co Llc | Electrolytic process for forming a mineral |
| US6599643B2 (en) | 1997-01-31 | 2003-07-29 | Elisha Holding Llc | Energy enhanced process for treating a conductive surface and products formed thereby |
| US6592738B2 (en) | 1997-01-31 | 2003-07-15 | Elisha Holding Llc | Electrolytic process for treating a conductive surface and products formed thereby |
| EP0935265A3 (en) * | 1998-02-09 | 2002-06-12 | Wilson Greatbatch Ltd. | Thermal spray coated substrate for use in an electrical energy storage device and method |
| GB9803561D0 (en) * | 1998-02-19 | 1998-04-15 | Monitor Coatings & Eng | Surface treatment of rotors |
| US6207522B1 (en) | 1998-11-23 | 2001-03-27 | Microcoating Technologies | Formation of thin film capacitors |
| WO2000044059A1 (en) | 1999-01-21 | 2000-07-27 | Asahi Glass Company, Limited | Solid polymer electrolyte fuel cell |
| KR100361548B1 (ko) | 1999-04-19 | 2002-11-21 | 스미토모 긴조쿠 고교 가부시키가이샤 | 고체고분자형 연료전지용 스텐레스 강재 |
| US6245390B1 (en) * | 1999-09-10 | 2001-06-12 | Viatcheslav Baranovski | High-velocity thermal spray apparatus and method of forming materials |
| US6649031B1 (en) | 1999-10-08 | 2003-11-18 | Hybrid Power Generation Systems, Llc | Corrosion resistant coated fuel cell bipolar plate with filled-in fine scale porosities and method of making the same |
| DE19957981A1 (de) * | 1999-12-02 | 2001-06-07 | Abb Research Ltd | Hochtemperatursupraleiteranordnung und Verfahren zu deren Herstellung |
| US6372376B1 (en) | 1999-12-07 | 2002-04-16 | General Motors Corporation | Corrosion resistant PEM fuel cell |
| JP4035968B2 (ja) * | 2000-06-30 | 2008-01-23 | セイコーエプソン株式会社 | 導電膜パターンの形成方法 |
| US7968251B2 (en) | 2000-11-24 | 2011-06-28 | GM Global Technology Operations LLC | Electrical contact element and bipolar plate |
| CN100493267C (zh) * | 2000-11-29 | 2009-05-27 | 萨莫希雷梅克斯公司 | 具有控制电阻率的电阻加热器及其制备方法 |
| US6915964B2 (en) * | 2001-04-24 | 2005-07-12 | Innovative Technology, Inc. | System and process for solid-state deposition and consolidation of high velocity powder particles using thermal plastic deformation |
| US6685988B2 (en) * | 2001-10-09 | 2004-02-03 | Delphi Technologies, Inc. | Kinetic sprayed electrical contacts on conductive substrates |
| US7005214B2 (en) * | 2001-11-02 | 2006-02-28 | Wilson Greatbatch Technologies, Inc. | Noble metals coated on titanium current collectors for use in nonaqueous Li/CFx cells |
| CA2468510C (en) | 2001-12-18 | 2011-11-29 | Honda Giken Kogyo Kabushiki Kaisha | Method of producing fuel cell-use separator and device for producing it |
| JP2003268567A (ja) | 2002-03-19 | 2003-09-25 | Hitachi Cable Ltd | 導電材被覆耐食性金属材料 |
| EP1369504A1 (en) * | 2002-06-05 | 2003-12-10 | Hille & Müller | Metal strip for the manufacture of components for electrical connectors |
| WO2004025751A2 (en) | 2002-09-11 | 2004-03-25 | Moltech Invent S.A. | Non-carbon anodes for aluminium electrowinning and other oxidation resistant components with iron oxide-containing coatings |
| US7338699B2 (en) * | 2002-10-31 | 2008-03-04 | Tosoh Corporation | Island projection-modified part, method for producing the same, and apparatus comprising the same |
| US7144648B2 (en) | 2002-11-22 | 2006-12-05 | The Research Foundation Of State University Of New York | Bipolar plate |
| WO2004052559A2 (en) | 2002-12-06 | 2004-06-24 | Eikos, Inc. | Optically transparent nanostructured electrical conductors |
| US6924002B2 (en) | 2003-02-24 | 2005-08-02 | General Electric Company | Coating and coating process incorporating raised surface features for an air-cooled surface |
| US7070833B2 (en) | 2003-03-05 | 2006-07-04 | Restek Corporation | Method for chemical vapor deposition of silicon on to substrates for use in corrosive and vacuum environments |
| JP4327489B2 (ja) | 2003-03-28 | 2009-09-09 | 本田技研工業株式会社 | 燃料電池用金属製セパレータおよびその製造方法 |
| JP3988936B2 (ja) | 2003-05-13 | 2007-10-10 | 信越化学工業株式会社 | シラン表面処理球状シリカチタニア系微粒子、その製造方法、および、それを用いた静電荷像現像用トナー外添剤 |
| US7670707B2 (en) * | 2003-07-30 | 2010-03-02 | Altergy Systems, Inc. | Electrical contacts for fuel cells |
| US20050158621A1 (en) * | 2003-09-30 | 2005-07-21 | Benoit Stephen A. | Battery with flat housing |
| US7344798B2 (en) | 2003-11-07 | 2008-03-18 | General Motors Corporation | Low contact resistance bonding method for bipolar plates in a pem fuel cell |
| US7846591B2 (en) | 2004-02-17 | 2010-12-07 | Gm Global Technology Operations, Inc. | Water management layer on flowfield in PEM fuel cell |
| KR100794294B1 (ko) | 2004-03-04 | 2008-01-14 | 고경현 | 내마모성 금속-세라믹 복합체 코팅 형성 방법 |
| US7052741B2 (en) | 2004-05-18 | 2006-05-30 | The United States Of America As Represented By The Secretary Of The Navy | Method of fabricating a fibrous structure for use in electrochemical applications |
| US7309540B2 (en) | 2004-05-21 | 2007-12-18 | Sarnoff Corporation | Electrical power source designs and components |
| US20060003174A1 (en) | 2004-06-30 | 2006-01-05 | Kabushiki Kaisha Kobe Seiko Sho (Kobe Steel, Ltd.) | Titanium material and method for manufacturing the same |
| US7955754B2 (en) | 2004-07-20 | 2011-06-07 | GM Global Technology Operations LLC | Enhanced stability bipolar plate |
| KR100578981B1 (ko) | 2004-09-08 | 2006-05-12 | 삼성에스디아이 주식회사 | 연료전지용 전극, 이를 포함하는 연료전지 시스템 |
| US20060222777A1 (en) * | 2005-04-05 | 2006-10-05 | General Electric Company | Method for applying a plasma sprayed coating using liquid injection |
| KR100802328B1 (ko) | 2005-04-07 | 2008-02-13 | 주식회사 솔믹스 | 내마모성 금속기지 복합체 코팅층 형성방법 및 이를이용하여 제조된 코팅층 |
| US7758921B2 (en) | 2005-05-26 | 2010-07-20 | Uchicago Argonne, Llc | Method of fabricating electrode catalyst layers with directionally oriented carbon support for proton exchange membrane fuel cell |
| DE112006001385B4 (de) * | 2005-06-03 | 2012-06-28 | Honda Motor Co., Ltd. | Separator für eine Brennstoffzelle und Verfahren zu dessen Herstellung |
| KR101380793B1 (ko) * | 2005-12-21 | 2014-04-04 | 슐저메트코(유에스)아이엔씨 | 하이브리드 플라즈마-콜드 스프레이 방법 및 장치 |
| US20070160899A1 (en) | 2006-01-10 | 2007-07-12 | Cabot Corporation | Alloy catalyst compositions and processes for making and using same |
| EP1808920A1 (en) | 2006-01-12 | 2007-07-18 | Stichting PowerPlus | Nanosized catalysts for the anode of a PEM fuel cell |
| KR101344990B1 (ko) * | 2006-04-20 | 2013-12-24 | 신에쓰 가가꾸 고교 가부시끼가이샤 | 도전성 내플라즈마 부재 |
| US20080145633A1 (en) | 2006-06-19 | 2008-06-19 | Cabot Corporation | Photovoltaic conductive features and processes for forming same |
| US20100151267A1 (en) | 2006-06-19 | 2010-06-17 | Cabot Corporation | Metal-containing nanoparticles, their synthesis and use |
| JP4198726B2 (ja) | 2006-09-06 | 2008-12-17 | クロリンエンジニアズ株式会社 | イオン交換膜電解槽 |
| US20080085439A1 (en) | 2006-09-28 | 2008-04-10 | Hilliard Donald B | Solid oxide electrolytic device |
| US20090087549A1 (en) * | 2007-09-27 | 2009-04-02 | Motorola, Inc. | Selective coating of fuel cell electrocatalyst |
| CN101918619A (zh) | 2008-01-08 | 2010-12-15 | 特来德斯通技术公司 | 用于电化学应用的高导电性表面 |
| FR2928492B1 (fr) | 2008-03-06 | 2011-10-21 | Ceram Hyd | Materiau pour un dispositif electrochimique. |
| CN102224279A (zh) | 2008-10-08 | 2011-10-19 | 麻省理工学院 | 用于水电解和其它电化学技术的催化材料、光电阳极和光电化学电池 |
| WO2010065938A1 (en) | 2008-12-05 | 2010-06-10 | Deeya Energy Technologies, Inc. | Preparation of electrolytes for redox flow batteries |
| WO2010129957A2 (en) | 2009-05-08 | 2010-11-11 | Treadstone Technologies, Inc. | High power fuel stacks using metal separator plates |
| WO2011011064A2 (en) | 2009-07-24 | 2011-01-27 | Stc.Unm | Efficient hydrogen production by photocatalytic water splitting using surface plasmons in hybrid nanoparticles |
| JP2013506050A (ja) | 2009-09-28 | 2013-02-21 | トレッドストーン テクノロジーズ インク. | 電気化学分野の製品のための高い電気伝導性を有する表面の形成方法 |
| CN102074715B (zh) | 2009-11-19 | 2015-07-22 | 上海空间电源研究所 | 用于一体式可再生燃料电池的双效膜电极及其制备方法 |
| WO2014134019A1 (en) | 2013-02-26 | 2014-09-04 | Treadstone Technologies, Inc. | Corrosion resistance metallic components for batteries |
-
2009
- 2009-01-08 CN CN2009801018813A patent/CN101918619A/zh active Pending
- 2009-01-08 WO PCT/US2009/030475 patent/WO2009089376A2/en not_active Ceased
- 2009-01-08 KR KR1020107017499A patent/KR101559604B1/ko active Active
- 2009-01-08 EP EP09700943.5A patent/EP2229471B1/en active Active
- 2009-01-08 JP JP2010541600A patent/JP5512542B2/ja active Active
- 2009-01-08 US US12/350,896 patent/US9765421B2/en active Active
- 2009-01-08 DK DK09700943.5T patent/DK2229471T3/da active
- 2009-01-08 CN CN201510055694.3A patent/CN104674153B/zh active Active
-
2014
- 2014-01-14 JP JP2014004549A patent/JP5995882B2/ja active Active
-
2017
- 2017-08-28 US US15/688,423 patent/US11208713B2/en active Active
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2011509349A5 (enExample) | ||
| KR101559604B1 (ko) | 전기화학 용도에 사용되는 고전기전도성 표면 | |
| JP5708182B2 (ja) | 固体電解質膜を用いた金属膜形成方法 | |
| CN107681173A (zh) | 一种用于燃料电池金属极板的点状导电复合涂层 | |
| CN110487166A (zh) | 薄膜应变传感器制备方法 | |
| CN102632031A (zh) | 一种超疏水表面的制备方法 | |
| JP2011174184A5 (enExample) | ||
| CN104662207A (zh) | 接触元件 | |
| CN101235531B (zh) | 再活化用于电解的电极的方法 | |
| JP2016517611A (ja) | 電池用の耐腐食性金属コンポーネント | |
| JP7078232B2 (ja) | 表面に電気めっき層を有する難溶融金属またはステンレス鋼、および難溶融金属またはステンレス鋼の表面の電気めっきプロセス | |
| CN103345958B (zh) | 含反应等离子喷涂纳米TiN中间层的复合电极材料及其制备方法 | |
| Liu et al. | Interfacial Engineering for Highly Stable and Stretchable Electrodes Enabled by Printing/Writing Surface‐Embedded Silver and Its Selective Alloying with Liquid Metals | |
| CN115376757B (zh) | 一种抗氧化的铜纳米线透明电极及其制备方法和应用 | |
| TWI552171B (zh) | 導電薄膜及其製備方法 | |
| JP2014189872A (ja) | 金属部品の製造方法並びにそれに用いられる鋳型および離型膜 | |
| Navik et al. | Facile synthesis of highly oxidation stable nanosilver-coated copper nanowires for transparent flexible electrodes | |
| JP5072019B2 (ja) | 燃料電池用セパレータ材料及び燃料電池用セパレータ | |
| CN208899010U (zh) | 一种铜底具有银合金镀层的电镀镀层、端子及电子接口 | |
| US20040103813A1 (en) | Paste for electroless plating and method of producing metallic structured body, micrometallic component, and conductor circuit using the paste | |
| CN102691092A (zh) | 金属多孔材料的制备方法及由该方法制得的金属多孔材料 | |
| KR101571844B1 (ko) | 밀착력이 우수한 cnt-모재 복합구조를 가지는 전기도금 또는 전해용 양극의 제조방법 | |
| TWI490932B (zh) | 導電性互連結構之製作方法 | |
| JP4847179B2 (ja) | 貴金属めっきを施したチタン又はチタン合金材料 | |
| CN117996484A (zh) | 接触元件、连接组件、喷涂介质用途和接触元件制造方法 |