TWI557087B - 具有低軟化溫度及高韌性之玻璃 - Google Patents
具有低軟化溫度及高韌性之玻璃 Download PDFInfo
- Publication number
- TWI557087B TWI557087B TW100117130A TW100117130A TWI557087B TW I557087 B TWI557087 B TW I557087B TW 100117130 A TW100117130 A TW 100117130A TW 100117130 A TW100117130 A TW 100117130A TW I557087 B TWI557087 B TW I557087B
- Authority
- TW
- Taiwan
- Prior art keywords
- glass
- alkali metal
- mol
- metal aluminoborosilicate
- aluminoborosilicate glass
- Prior art date
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C03—GLASS; MINERAL OR SLAG WOOL
- C03C—CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03C3/00—Glass compositions
- C03C3/04—Glass compositions containing silica
- C03C3/076—Glass compositions containing silica with 40% to 90% silica, by weight
- C03C3/089—Glass compositions containing silica with 40% to 90% silica, by weight containing boron
- C03C3/091—Glass compositions containing silica with 40% to 90% silica, by weight containing boron containing aluminium
-
- C—CHEMISTRY; METALLURGY
- C03—GLASS; MINERAL OR SLAG WOOL
- C03C—CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03C21/00—Treatment of glass, not in the form of fibres or filaments, by diffusing ions or metals in the surface
-
- C—CHEMISTRY; METALLURGY
- C03—GLASS; MINERAL OR SLAG WOOL
- C03C—CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03C21/00—Treatment of glass, not in the form of fibres or filaments, by diffusing ions or metals in the surface
- C03C21/001—Treatment of glass, not in the form of fibres or filaments, by diffusing ions or metals in the surface in liquid phase, e.g. molten salts, solutions
-
- C—CHEMISTRY; METALLURGY
- C03—GLASS; MINERAL OR SLAG WOOL
- C03C—CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03C3/00—Glass compositions
- C03C3/04—Glass compositions containing silica
- C03C3/076—Glass compositions containing silica with 40% to 90% silica, by weight
- C03C3/097—Glass compositions containing silica with 40% to 90% silica, by weight containing phosphorus, niobium or tantalum
Landscapes
- Chemical & Material Sciences (AREA)
- Life Sciences & Earth Sciences (AREA)
- Engineering & Computer Science (AREA)
- Chemical Kinetics & Catalysis (AREA)
- General Chemical & Material Sciences (AREA)
- Geochemistry & Mineralogy (AREA)
- Materials Engineering (AREA)
- Organic Chemistry (AREA)
- Ceramic Engineering (AREA)
- Glass Compositions (AREA)
- Surface Treatment Of Glass (AREA)
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US12/788,559 US8778820B2 (en) | 2010-05-27 | 2010-05-27 | Glasses having low softening temperatures and high toughness |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| TW201204670A TW201204670A (en) | 2012-02-01 |
| TWI557087B true TWI557087B (zh) | 2016-11-11 |
Family
ID=44121326
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| TW100117130A TWI557087B (zh) | 2010-05-27 | 2011-05-17 | 具有低軟化溫度及高韌性之玻璃 |
Country Status (7)
| Country | Link |
|---|---|
| US (1) | US8778820B2 (enExample) |
| EP (1) | EP2576467A1 (enExample) |
| JP (2) | JP5948321B2 (enExample) |
| KR (1) | KR101765975B1 (enExample) |
| CN (1) | CN102971266B (enExample) |
| TW (1) | TWI557087B (enExample) |
| WO (1) | WO2011149740A1 (enExample) |
Families Citing this family (68)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US8778820B2 (en) * | 2010-05-27 | 2014-07-15 | Corning Incorporated | Glasses having low softening temperatures and high toughness |
| US20120052271A1 (en) | 2010-08-26 | 2012-03-01 | Sinue Gomez | Two-step method for strengthening glass |
| US9346703B2 (en) | 2010-11-30 | 2016-05-24 | Corning Incorporated | Ion exchangable glass with deep compressive layer and high damage threshold |
| US8889575B2 (en) * | 2011-05-31 | 2014-11-18 | Corning Incorporated | Ion exchangeable alkali aluminosilicate glass articles |
| US9517966B2 (en) | 2011-10-25 | 2016-12-13 | Corning Incorporated | Glass compositions with improved chemical and mechanical durability |
| WO2013063277A1 (en) | 2011-10-25 | 2013-05-02 | Corning Incorporated | Delamination resistant pharmaceutical glass containers containing active pharmaceutical ingredients |
| US9359251B2 (en) | 2012-02-29 | 2016-06-07 | Corning Incorporated | Ion exchanged glasses via non-error function compressive stress profiles |
| US9512029B2 (en) | 2012-05-31 | 2016-12-06 | Corning Incorporated | Cover glass article |
| DE202013012920U1 (de) * | 2012-05-31 | 2022-01-24 | Corning Incorporated | Zirkon-kompatibles, ionenaustauschbares Glas mit hoher Schadensresistenz |
| RU2674269C2 (ru) * | 2012-06-07 | 2018-12-06 | Корнинг Инкорпорейтед | Стойкие к расслаиванию стеклянные контейнеры |
| US9139469B2 (en) | 2012-07-17 | 2015-09-22 | Corning Incorporated | Ion exchangeable Li-containing glass compositions for 3-D forming |
| US9387651B2 (en) | 2012-09-26 | 2016-07-12 | Corning Incorporated | Methods for producing ion exchanged glass and resulting apparatus |
| US20140087193A1 (en) * | 2012-09-26 | 2014-03-27 | Jeffrey Scott Cites | Methods for producing ion exchanged glass and resulting apparatus |
| KR102173671B1 (ko) * | 2012-10-04 | 2020-11-04 | 코닝 인코포레이티드 | 감광성 유리를 통한 압축 응력 적층 유리 제품 및 이의 제조 방법 |
| JP2014133683A (ja) * | 2013-01-10 | 2014-07-24 | Central Glass Co Ltd | 化学強化ガラス板の製造方法 |
| US9603775B2 (en) | 2013-04-24 | 2017-03-28 | Corning Incorporated | Delamination resistant pharmaceutical glass containers containing active pharmaceutical ingredients |
| US9707154B2 (en) | 2013-04-24 | 2017-07-18 | Corning Incorporated | Delamination resistant pharmaceutical glass containers containing active pharmaceutical ingredients |
| US9849066B2 (en) | 2013-04-24 | 2017-12-26 | Corning Incorporated | Delamination resistant pharmaceutical glass containers containing active pharmaceutical ingredients |
| US9700485B2 (en) | 2013-04-24 | 2017-07-11 | Corning Incorporated | Delamination resistant pharmaceutical glass containers containing active pharmaceutical ingredients |
| US9707153B2 (en) | 2013-04-24 | 2017-07-18 | Corning Incorporated | Delamination resistant pharmaceutical glass containers containing active pharmaceutical ingredients |
| US9700486B2 (en) | 2013-04-24 | 2017-07-11 | Corning Incorporated | Delamination resistant pharmaceutical glass containers containing active pharmaceutical ingredients |
| US9839579B2 (en) | 2013-04-24 | 2017-12-12 | Corning Incorporated | Delamination resistant pharmaceutical glass containers containing active pharmaceutical ingredients |
| US9717649B2 (en) | 2013-04-24 | 2017-08-01 | Corning Incorporated | Delamination resistant pharmaceutical glass containers containing active pharmaceutical ingredients |
| US9707155B2 (en) | 2013-04-24 | 2017-07-18 | Corning Incorporated | Delamination resistant pharmaceutical glass containers containing active pharmaceutical ingredients |
| US9713572B2 (en) | 2013-04-24 | 2017-07-25 | Corning Incorporated | Delamination resistant pharmaceutical glass containers containing active pharmaceutical ingredients |
| US9717648B2 (en) | 2013-04-24 | 2017-08-01 | Corning Incorporated | Delamination resistant pharmaceutical glass containers containing active pharmaceutical ingredients |
| KR102144705B1 (ko) * | 2013-05-24 | 2020-08-14 | 니폰 덴키 가라스 가부시키가이샤 | 강화 유리판의 제조 방법 |
| US9512035B2 (en) * | 2013-06-17 | 2016-12-06 | Corning Incorporated | Antimicrobial glass articles with improved strength and methods of making and using same |
| US11079309B2 (en) | 2013-07-26 | 2021-08-03 | Corning Incorporated | Strengthened glass articles having improved survivability |
| KR102236063B1 (ko) * | 2013-08-06 | 2021-04-06 | 삼성디스플레이 주식회사 | 광학 코팅 구조 |
| KR102290967B1 (ko) | 2013-08-27 | 2021-08-19 | 코닝 인코포레이티드 | 높은 열팽창계수를 갖는 내손상성 유리 |
| US10209419B2 (en) | 2013-09-17 | 2019-02-19 | Corning Incorporated | Broadband polarizer made using ion exchangeable fusion drawn glass sheets |
| JPWO2015046113A1 (ja) * | 2013-09-25 | 2017-03-09 | 旭硝子株式会社 | ガラス板及び化学強化ガラス板 |
| WO2015077109A1 (en) * | 2013-11-20 | 2015-05-28 | Corning Incorporated | Scratch-resistant boroaluminosilicate glass |
| KR102391152B1 (ko) * | 2013-11-26 | 2022-04-27 | 코닝 인코포레이티드 | 높은 압입 임계값을 갖는 빠른 이온 교환 가능한 유리 |
| US9517968B2 (en) | 2014-02-24 | 2016-12-13 | Corning Incorporated | Strengthened glass with deep depth of compression |
| WO2016191676A1 (en) * | 2015-05-28 | 2016-12-01 | Corning Incorporated | Strengthened glass with deep depth of compression |
| KR102347803B1 (ko) * | 2014-02-27 | 2022-01-06 | 코닝 인코포레이티드 | 3-차원 형성을 위한 이온 교환 가능한 유리 |
| TWI697403B (zh) * | 2014-06-19 | 2020-07-01 | 美商康寧公司 | 無易碎應力分布曲線的玻璃 |
| CN116282965A (zh) * | 2014-07-25 | 2023-06-23 | 康宁股份有限公司 | 具有深的压缩深度的强化玻璃 |
| CN108046589A (zh) | 2014-10-08 | 2018-05-18 | 康宁股份有限公司 | 包含金属氧化物浓度梯度的玻璃和玻璃陶瓷 |
| US10150698B2 (en) | 2014-10-31 | 2018-12-11 | Corning Incorporated | Strengthened glass with ultra deep depth of compression |
| WO2016073539A1 (en) | 2014-11-04 | 2016-05-12 | Corning Incorporated | Deep non-frangible stress profiles and methods of making |
| WO2016085778A1 (en) * | 2014-11-26 | 2016-06-02 | Corning Incorporated | Thin glass sheet and system and method for forming the same |
| US10259745B2 (en) | 2015-02-27 | 2019-04-16 | Corning Incorporated | Low temperature chemical strengthening process for glass |
| CN104843977A (zh) * | 2015-05-04 | 2015-08-19 | 山东华芯富创电子科技有限公司 | 触控面板强化玻璃改料再加工的方法 |
| US11104602B2 (en) * | 2015-06-26 | 2021-08-31 | Corning Incorporated | Glass with high surface strength |
| KR102640959B1 (ko) | 2015-06-26 | 2024-02-27 | 코닝 인코포레이티드 | 높은 표면 강도를 갖는 유리 |
| US11613103B2 (en) | 2015-07-21 | 2023-03-28 | Corning Incorporated | Glass articles exhibiting improved fracture performance |
| US10579106B2 (en) | 2015-07-21 | 2020-03-03 | Corning Incorporated | Glass articles exhibiting improved fracture performance |
| TWI697463B (zh) | 2015-12-11 | 2020-07-01 | 美商康寧公司 | 具有金屬氧化物濃度梯度之可熔融成形的玻璃基物件 |
| JP7165055B2 (ja) | 2016-01-08 | 2022-11-02 | コーニング インコーポレイテッド | 固有の損傷抵抗を有する化学強化可能なリチウムアルミノケイ酸塩ガラス |
| KR20180103972A (ko) * | 2016-01-13 | 2018-09-19 | 코닝 인코포레이티드 | 초-박형, 비-취약성 유리 및 이의 제조방법 |
| WO2017126605A1 (ja) | 2016-01-21 | 2017-07-27 | 旭硝子株式会社 | 化学強化ガラス及び化学強化ガラスの製造方法 |
| CN115650601B (zh) | 2016-01-21 | 2024-07-12 | Agc株式会社 | 化学强化玻璃以及化学强化用玻璃 |
| CN111423110A (zh) | 2016-04-08 | 2020-07-17 | 康宁股份有限公司 | 包含金属氧化物浓度梯度的玻璃基制品 |
| KR20200091500A (ko) | 2016-04-08 | 2020-07-30 | 코닝 인코포레이티드 | 두 영역을 포함하는 응력 프로파일을 포함하는 유리-계 물품, 및 제조 방법 |
| CN108698909B (zh) | 2016-05-27 | 2022-07-12 | 康宁股份有限公司 | 耐破裂和耐划痕玻璃制品 |
| US10065880B2 (en) | 2016-11-07 | 2018-09-04 | Corning Incorporated | Lithium containing glasses |
| CN110167895B (zh) * | 2016-11-07 | 2022-07-15 | 康宁股份有限公司 | 低粘度玻璃以及制造方法和系统 |
| US11152294B2 (en) | 2018-04-09 | 2021-10-19 | Corning Incorporated | Hermetic metallized via with improved reliability |
| US11591255B2 (en) * | 2018-05-22 | 2023-02-28 | Corning Incorporated | Low temperature moldable sheet forming glass compositions |
| US12200875B2 (en) | 2018-09-20 | 2025-01-14 | Industrial Technology Research Institute | Copper metallization for through-glass vias on thin glass |
| US12037282B2 (en) * | 2018-11-01 | 2024-07-16 | Corning Incorporated | Strengthened glass articles with reduced delayed breakage and methods of making the same |
| KR20250083587A (ko) | 2019-02-21 | 2025-06-10 | 코닝 인코포레이티드 | 구리-금속화된 쓰루 홀을 갖는 유리 또는 유리 세라믹 물품 및 이를 제조하기 위한 공정 |
| KR102815216B1 (ko) * | 2020-04-13 | 2025-05-30 | 코닝 인코포레이티드 | K2o 함유 디스플레이 유리들 |
| CN115734948B (zh) * | 2020-07-03 | 2025-03-18 | Agc株式会社 | 玻璃、微晶玻璃和化学强化玻璃 |
| US12024465B2 (en) * | 2021-06-11 | 2024-07-02 | Corning Incorporated | Glass compositions having improved mechanical durability and low characteristic temperatures |
Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US20090142568A1 (en) * | 2007-11-29 | 2009-06-04 | Matthew John Dejneka | Glasses having improved toughness and scratch resistance |
Family Cites Families (26)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| DE1696063B2 (de) | 1968-02-01 | 1972-07-20 | Jenaer Glaswerk Schott & Gen, 6500 Mainz | Anwendung eines austauschverfahrens von alkaliionen zur mechanischen festigkeitsverbesserung auf ein boroaluminiumsilikatglas mit einem relativ niedrigen waermeausdehnungskoeffizienten unter 60.10 hoch -7/grad c |
| JPS6036349A (ja) * | 1983-08-05 | 1985-02-25 | Ngk Spark Plug Co Ltd | ガラス組成物 |
| US4792535A (en) * | 1987-09-02 | 1988-12-20 | Corning Glass Works | UV-transmitting glasses |
| US4925814A (en) * | 1989-02-27 | 1990-05-15 | Corning Incorporated | Ultraviolet transmitting glasses for EPROM windows |
| US5733622A (en) * | 1995-06-07 | 1998-03-31 | International Business Machines Corporation | Edge strengthened substrate of a data storage disk and method for fabricating same |
| WO1998050315A1 (en) * | 1997-05-07 | 1998-11-12 | Corning Incorporated | Organic lens molds in inorganic glass and novel inorganic glasses |
| JPH11153705A (ja) * | 1997-11-20 | 1999-06-08 | Nippon Sheet Glass Co Ltd | 軸方向屈折率分布型レンズ |
| JP2005162600A (ja) * | 2003-11-11 | 2005-06-23 | Nippon Electric Glass Co Ltd | 半導体パッケージ用カバーガラス |
| DE10361555A1 (de) * | 2003-12-19 | 2005-07-28 | Grintech Gmbh | Alumoborosilikatglas und Verfahren zur Herstellung kristallitfreier Gradientenindexlinsen |
| JP2006298691A (ja) * | 2005-04-20 | 2006-11-02 | Hitachi Ltd | 平面型画像表示装置 |
| CN102898023B (zh) | 2006-05-25 | 2016-11-23 | 日本电气硝子株式会社 | 强化玻璃及其制造方法 |
| JP5875133B2 (ja) * | 2006-10-10 | 2016-03-02 | 日本電気硝子株式会社 | 強化ガラス基板 |
| KR101351366B1 (ko) | 2006-10-10 | 2014-01-14 | 니폰 덴키 가라스 가부시키가이샤 | 강화 유리 기판 |
| JP2008201654A (ja) * | 2007-02-23 | 2008-09-04 | Hitachi Ltd | 表示装置 |
| JP2008273782A (ja) * | 2007-04-27 | 2008-11-13 | Ohara Inc | ガラス |
| JP5743125B2 (ja) | 2007-09-27 | 2015-07-01 | 日本電気硝子株式会社 | 強化ガラス及び強化ガラス基板 |
| JP5339173B2 (ja) | 2007-09-27 | 2013-11-13 | 日本電気硝子株式会社 | 強化ガラス基板及びガラス並びに強化ガラス基板の製造方法 |
| JP2011510903A (ja) * | 2008-02-08 | 2011-04-07 | コーニング インコーポレイテッド | 損傷耐性の化学強化された保護カバーガラス |
| RU2010154445A (ru) * | 2008-05-30 | 2012-07-10 | Фостер Вилер Энергия Ой (Fi) | Способ и система для генерации энергии путем сжигания в чистом кислороде |
| JP5867953B2 (ja) * | 2008-06-27 | 2016-02-24 | 日本電気硝子株式会社 | 強化ガラスおよび強化用ガラス |
| JP2011527661A (ja) * | 2008-07-11 | 2011-11-04 | コーニング インコーポレイテッド | 民生用途のための圧縮面を有するガラス |
| WO2010014163A1 (en) * | 2008-07-29 | 2010-02-04 | Corning Incorporated | Dual stage ion exchange for chemical strengthening of glass |
| JP5614607B2 (ja) | 2008-08-04 | 2014-10-29 | 日本電気硝子株式会社 | 強化ガラスおよびその製造方法 |
| KR20110050522A (ko) * | 2008-08-21 | 2011-05-13 | 코닝 인코포레이티드 | 전자 장치용 내구성 유리 하우징/인클로저 |
| US8341976B2 (en) | 2009-02-19 | 2013-01-01 | Corning Incorporated | Method of separating strengthened glass |
| US8778820B2 (en) * | 2010-05-27 | 2014-07-15 | Corning Incorporated | Glasses having low softening temperatures and high toughness |
-
2010
- 2010-05-27 US US12/788,559 patent/US8778820B2/en active Active
-
2011
- 2011-05-17 TW TW100117130A patent/TWI557087B/zh not_active IP Right Cessation
- 2011-05-18 KR KR1020127033855A patent/KR101765975B1/ko not_active Expired - Fee Related
- 2011-05-18 EP EP11721694.5A patent/EP2576467A1/en not_active Withdrawn
- 2011-05-18 JP JP2013512087A patent/JP5948321B2/ja not_active Expired - Fee Related
- 2011-05-18 WO PCT/US2011/037036 patent/WO2011149740A1/en not_active Ceased
- 2011-05-18 CN CN201180025885.5A patent/CN102971266B/zh active Active
-
2016
- 2016-06-06 JP JP2016112642A patent/JP6776010B2/ja not_active Expired - Fee Related
Patent Citations (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US20090142568A1 (en) * | 2007-11-29 | 2009-06-04 | Matthew John Dejneka | Glasses having improved toughness and scratch resistance |
Also Published As
| Publication number | Publication date |
|---|---|
| WO2011149740A1 (en) | 2011-12-01 |
| JP6776010B2 (ja) | 2020-10-28 |
| CN102971266A (zh) | 2013-03-13 |
| CN102971266B (zh) | 2016-05-25 |
| JP5948321B2 (ja) | 2016-07-06 |
| JP2016155759A (ja) | 2016-09-01 |
| TW201204670A (en) | 2012-02-01 |
| KR101765975B1 (ko) | 2017-08-23 |
| JP2013527115A (ja) | 2013-06-27 |
| US20110294649A1 (en) | 2011-12-01 |
| KR20130098894A (ko) | 2013-09-05 |
| EP2576467A1 (en) | 2013-04-10 |
| US8778820B2 (en) | 2014-07-15 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| TWI557087B (zh) | 具有低軟化溫度及高韌性之玻璃 | |
| KR102325873B1 (ko) | 고강도 초박형 유리 및 이의 제조 방법 | |
| JP6976057B2 (ja) | 耐スクラッチアルミノホウケイ酸ガラス | |
| EP2874959B1 (en) | Ion exchangeable li-containing glass compositions for 3-d forming | |
| US9540278B2 (en) | Ion exchangeable glasses | |
| TWI588113B (zh) | 可離子交換玻璃 | |
| JP2016528152A (ja) | アルカリドープおよび無アルカリホウアルミノケイ酸ガラス | |
| CN111908806A (zh) | 强化玻璃的二步法 | |
| TW200911718A (en) | Hardened glass substrate, and method for production thereof | |
| TW201130755A (en) | Glass plate for display device, plate glass for display device and production process thereof | |
| TW201800352A (zh) | 具有高表面壓縮應力之可離子交換玻璃 | |
| TW201536699A (zh) | 強化玻璃的製造方法以及強化玻璃 | |
| CN108602711B (zh) | 低碱金属含量的硼硅酸盐玻璃 | |
| KR20130143525A (ko) | 알칼리 유리 및 그 제조 방법 | |
| JP5648945B1 (ja) | 強化ガラスの製造方法 | |
| KR101735514B1 (ko) | 알루미노실리케이트 유리 및 그 제조 방법 | |
| KR20130127956A (ko) | 알칼리 유리 및 그 제조 방법 | |
| KR20150040523A (ko) | 알루미노실리케이트 유리 및 그 제조 방법 | |
| KR101738599B1 (ko) | 알루미노실리케이트 유리 및 그 제조 방법 | |
| KR101593097B1 (ko) | 알루미노실리케이트 유리 및 그 제조 방법 | |
| TW202511212A (zh) | 具有較高可化學韌化性且不易結晶之玻璃及玻璃製品以及製造方法 | |
| KR20130127953A (ko) | 알칼리 유리 및 그 제조 방법 | |
| KR20130143523A (ko) | 알칼리 유리 및 그 제조 방법 | |
| KR20130127955A (ko) | 알칼리 유리 및 그 제조 방법 | |
| KR20130143524A (ko) | 알칼리 유리 및 그 제조 방법 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| MM4A | Annulment or lapse of patent due to non-payment of fees |