JP2009536712A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2009536712A5 JP2009536712A5 JP2009510169A JP2009510169A JP2009536712A5 JP 2009536712 A5 JP2009536712 A5 JP 2009536712A5 JP 2009510169 A JP2009510169 A JP 2009510169A JP 2009510169 A JP2009510169 A JP 2009510169A JP 2009536712 A5 JP2009536712 A5 JP 2009536712A5
- Authority
- JP
- Japan
- Prior art keywords
- piston
- crown
- rim
- bowl
- composition
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Applications Claiming Priority (3)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US11/431,297 US7458358B2 (en) | 2006-05-10 | 2006-05-10 | Thermal oxidation protective surface for steel pistons |
| US11/431,297 | 2006-05-10 | ||
| PCT/US2007/068633 WO2007134148A2 (en) | 2006-05-10 | 2007-05-10 | Thermal oxidation protective surface for steel pistons |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2009536712A JP2009536712A (ja) | 2009-10-15 |
| JP2009536712A5 true JP2009536712A5 (enExample) | 2010-06-24 |
| JP5300150B2 JP5300150B2 (ja) | 2013-09-25 |
Family
ID=38683952
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2009510169A Expired - Fee Related JP5300150B2 (ja) | 2006-05-10 | 2007-05-10 | スチールピストンのための熱酸化保護表面 |
Country Status (7)
| Country | Link |
|---|---|
| US (1) | US7458358B2 (enExample) |
| EP (1) | EP2021176B1 (enExample) |
| JP (1) | JP5300150B2 (enExample) |
| KR (1) | KR101383098B1 (enExample) |
| CN (1) | CN101479102B (enExample) |
| BR (1) | BRPI0713095B1 (enExample) |
| WO (1) | WO2007134148A2 (enExample) |
Families Citing this family (56)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US20050261241A1 (en) * | 2004-05-19 | 2005-11-24 | Celsus Biopharmaceuticals, Inc. | Use of dermatan sulfates and/or desulfated heparins to treat or prevent heparinoid-induced autoimmune responses |
| DE102005006671A1 (de) * | 2005-02-15 | 2006-08-17 | Ks Kolbenschmidt Gmbh | Schutzschicht gegen Heißgaskorrision im Verbrennungsraum einer Brennkraftmaschine |
| US20070116889A1 (en) * | 2005-11-18 | 2007-05-24 | Federal Mogul World Wide, Inc. | Laser treatment of metal |
| JP4379503B2 (ja) * | 2007-08-13 | 2009-12-09 | トヨタ自動車株式会社 | 内燃機関用ピストン |
| FR2925114A1 (fr) * | 2007-12-18 | 2009-06-19 | Inst Francais Du Petrole | Moteur a combustion interne a autoinflammation avec stratification de temperature du melange carbure et procede pour realiser un tel melange |
| FR2925604A1 (fr) * | 2007-12-19 | 2009-06-26 | Renault Sas | Chambre de combustion pour moteur thermique a injection directe suralimente |
| KR100920685B1 (ko) * | 2009-04-06 | 2009-10-09 | 거명터빈주식회사 | 터빈 다이아프램 외부링 내벽 코팅방법 및 그 방법에 의하여 코팅된 터빈 다이아프램 |
| GB0907096D0 (en) * | 2009-04-24 | 2009-06-03 | Isentropic Ltd | Improved piston |
| GB201001562D0 (en) * | 2010-01-29 | 2010-03-17 | Ricardo Uk Ltd | Direct injection diesel |
| KR20120065150A (ko) * | 2010-12-10 | 2012-06-20 | 현대자동차주식회사 | 보울이 형성된 피스톤 |
| US8677970B2 (en) | 2011-03-17 | 2014-03-25 | Cummins Intellectual Property, Inc. | Piston for internal combustion engine |
| US9464592B2 (en) * | 2011-04-18 | 2016-10-11 | Achates Power, Inc. | Piston thermal management in an opposed-piston engine |
| US20130025561A1 (en) * | 2011-07-28 | 2013-01-31 | Dieter Gabriel | Bowl rim and root protection for aluminum pistons |
| WO2013066924A1 (en) * | 2011-10-31 | 2013-05-10 | Federal-Mogul Corporation | Coated piston and a method of making a coated piston |
| US9249889B1 (en) | 2012-03-09 | 2016-02-02 | Mogas Industries, Inc. | High pressure ball valve |
| US9500285B2 (en) | 2012-03-09 | 2016-11-22 | Mogas Industries, Inc. | High pressure ball valve and packing |
| DE102012204947A1 (de) * | 2012-03-28 | 2013-10-02 | Mahle International Gmbh | Verfahren zur Herstellung eines Aluminiumkolbens |
| DE102012103206B4 (de) | 2012-04-13 | 2017-08-03 | Caterpillar Energy Solutions Gmbh | Kolben einer Brennkraftmaschine |
| DE102012103195A1 (de) | 2012-04-13 | 2013-10-17 | Mwm Gmbh | Kolben einer Brennkraftmaschine |
| DE102012103212A1 (de) * | 2012-04-13 | 2013-10-17 | Mwm Gmbh | Kolben einer Brennkraftmaschine |
| US10563569B2 (en) * | 2012-05-16 | 2020-02-18 | Dalian University Of Technology | Diesel combustion system |
| CN102717243A (zh) * | 2012-06-18 | 2012-10-10 | 上海交通大学 | 发动机活塞局部表面强化的工艺方法 |
| KR101924811B1 (ko) * | 2012-08-29 | 2018-12-04 | 현대중공업 주식회사 | 디젤엔진용 배기밸브 스핀들의 내부식성 향상을 위한 인코넬-코발트-크롬계 코팅혼합물과, 이를 이용한 배기밸브 스핀들 코팅방법 및 코팅혼합물이 코팅된 배기밸브 스핀들 |
| KR101924810B1 (ko) * | 2012-08-29 | 2018-12-04 | 현대중공업 주식회사 | 디젤엔진용 배기밸브 스핀들의 내부식성 향상을 위한 인코넬-니켈-크롬계 코팅혼합물과, 이를 이용한 배기밸브 스핀들 코팅방법 및 코팅혼합물이 코팅된 배기밸브 스핀들 |
| CN105190000B (zh) * | 2013-03-05 | 2018-11-20 | 费德罗-莫格尔公司 | 带有抗积碳涂料的活塞及其制造方法 |
| WO2014165734A1 (en) | 2013-04-05 | 2014-10-09 | Federal-Mogul Corporation | Piston made using additive manufacturing techniques |
| MX2015016390A (es) * | 2013-06-14 | 2016-04-11 | Ks Kolbenschmidt Gmbh | Metodo para producir una capa de protecion contra oxidacion para un piston para el uso en motores de combustion interna y piston que tiene una capa de proteccion contra oxidacion. |
| JP5858007B2 (ja) * | 2013-07-01 | 2016-02-10 | トヨタ自動車株式会社 | バルブシート用の肉盛方法及びシリンダヘッドの製造方法 |
| DE102013221102A1 (de) | 2013-10-17 | 2015-05-07 | Mahle International Gmbh | Stahlkolben für eine Brennkraftmaschine und Verfahren zu dessen Herstellung |
| EP2865479A1 (en) * | 2013-10-22 | 2015-04-29 | Siemens Aktiengesellschaft | Method and system for generating a component using thermal spraying and laser fusing |
| US9765727B2 (en) * | 2014-03-03 | 2017-09-19 | Federal-Mogul Llc | One-piece piston featuring additive machining produced combustion bowl rim and cooling gallery |
| JP6260492B2 (ja) * | 2014-08-11 | 2018-01-17 | トヨタ自動車株式会社 | 直噴式エンジンのピストンの製造方法 |
| CA2958286C (en) | 2014-08-18 | 2023-05-02 | Woodward, Inc. | Torch igniter |
| DE102014018256A1 (de) * | 2014-12-11 | 2016-06-16 | Mahle International Gmbh | Kolben für einen Verbrennungsmotor |
| US20160169152A1 (en) * | 2014-12-11 | 2016-06-16 | Caterpillar Inc. | Engine Piston |
| US10138840B2 (en) | 2015-02-20 | 2018-11-27 | Ford Global Technologies, Llc | PTWA coating on pistons and/or cylinder heads and/or cylinder bores |
| DE102015221960A1 (de) * | 2015-11-09 | 2017-05-11 | Federal-Mogul Nürnberg GmbH | Schutzschicht gegen die Oxidation des Kolbens eines Verbrennungsmotors |
| US10876475B2 (en) | 2015-11-20 | 2020-12-29 | Tenneco Inc. | Steel piston crown and/or combustion engine components with dynamic thermal insulation coating and method of making and using such a coating |
| US10578014B2 (en) | 2015-11-20 | 2020-03-03 | Tenneco Inc. | Combustion engine components with dynamic thermal insulation coating and method of making and using such a coating |
| US10519854B2 (en) | 2015-11-20 | 2019-12-31 | Tenneco Inc. | Thermally insulated engine components and method of making using a ceramic coating |
| US10578050B2 (en) | 2015-11-20 | 2020-03-03 | Tenneco Inc. | Thermally insulated steel piston crown and method of making using a ceramic coating |
| CN105484892A (zh) * | 2015-12-02 | 2016-04-13 | 湖南江滨机器(集团)有限责任公司 | 一种活塞及发动机及活塞制造方法 |
| JP6288116B2 (ja) * | 2016-01-21 | 2018-03-07 | トヨタ自動車株式会社 | シリンダヘッドの製造方法 |
| JP6384493B2 (ja) * | 2016-01-21 | 2018-09-05 | トヨタ自動車株式会社 | シリンダヘッドの製造方法 |
| EP3440230B1 (en) | 2016-04-08 | 2020-01-08 | Volvo Truck Corporation | A piston for a cylinder for an internal combustion engine |
| US20170355018A1 (en) * | 2016-06-09 | 2017-12-14 | Hamilton Sundstrand Corporation | Powder deposition for additive manufacturing |
| CN106435673A (zh) * | 2016-12-22 | 2017-02-22 | 日照金港活塞有限公司 | 一种内燃机锻钢活塞顶部隔热涂层的制备工艺 |
| US20180238264A1 (en) * | 2017-02-19 | 2018-08-23 | GM Global Technology Operations LLC | Diesel piston with stepped bowl |
| CN107218152A (zh) * | 2017-07-27 | 2017-09-29 | 叶明� | 应用于柴油十六烷值测定机的压缩比塞结构 |
| US10471554B2 (en) | 2017-08-22 | 2019-11-12 | Caterpillar Inc. | Fuel injector bore repair |
| JP2019143497A (ja) * | 2018-02-16 | 2019-08-29 | トヨタ自動車株式会社 | 圧縮自着火式内燃機関 |
| CN112805463B (zh) * | 2018-10-08 | 2023-10-31 | 辉门汽车零部件有限责任公司 | 抗爆活塞 |
| US11421601B2 (en) | 2019-03-28 | 2022-08-23 | Woodward, Inc. | Second stage combustion for igniter |
| BE1027847B1 (nl) * | 2019-12-12 | 2021-07-12 | Unilin Bv | Werkwijze voor het vervaardigen van panelen, en vloerpaneel hierbij bekomen |
| EP4168661A1 (en) | 2020-06-23 | 2023-04-26 | Woodward, Inc. | Ignition system for power generation engine |
| US11719184B1 (en) * | 2022-01-21 | 2023-08-08 | Tenneco Inc. | Piston with engineered crown coating and method of manufacturing |
Family Cites Families (54)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US3892207A (en) * | 1970-01-23 | 1975-07-01 | Carl A Weise | Internal combustion engine |
| JPS5948873B2 (ja) * | 1980-05-14 | 1984-11-29 | ペルメレック電極株式会社 | 耐食性被覆を設けた電極基体又は電極の製造方法 |
| US4434189A (en) * | 1982-03-15 | 1984-02-28 | The United States Of America As Represented By The Adminstrator Of The National Aeronautics And Space Administration | Method and apparatus for coating substrates using a laser |
| JPS61126360A (ja) * | 1984-11-26 | 1986-06-13 | Mitsubishi Heavy Ind Ltd | ピストンの溶射皮膜形成方法 |
| JPS61270335A (ja) * | 1985-05-24 | 1986-11-29 | Toyota Motor Corp | 内燃機関用肉盛バルブ |
| JPS6256562A (ja) * | 1985-09-04 | 1987-03-12 | Toyota Motor Corp | セラミツク溶射ピストンの製造方法 |
| US4781770A (en) * | 1986-03-24 | 1988-11-01 | Smith International, Inc. | Process for laser hardfacing drill bit cones having hard cutter inserts |
| US4708752A (en) * | 1986-03-24 | 1987-11-24 | Smith International, Inc. | Process for laser hardening drilling bit cones having hard cutter inserts placed therein |
| DE3773258D1 (de) * | 1986-05-18 | 1991-10-31 | Daido Steel Co Ltd | Verschleissfeste gegenstaende aus titan oder aus einer titanlegierung. |
| JPH0684548B2 (ja) * | 1986-09-19 | 1994-10-26 | 吉田工業株式会社 | 高耐食アモルファス表面層を有する被覆金属体およびその作製法 |
| JPH0698506B2 (ja) * | 1986-12-08 | 1994-12-07 | トヨタ自動車株式会社 | 金属基体上への分散合金層の形成方法 |
| JPS63143364A (ja) * | 1986-12-08 | 1988-06-15 | Mazda Motor Corp | 内燃機関のピストンの製造法 |
| US4960643A (en) * | 1987-03-31 | 1990-10-02 | Lemelson Jerome H | Composite synthetic materials |
| JPH0649888B2 (ja) * | 1989-03-24 | 1994-06-29 | 新日本製鐵株式会社 | 表面被覆金属の製造方法 |
| ES2053163T3 (es) * | 1990-01-22 | 1994-07-16 | Sulzer Innotec Ag | Capa protectora para un substrato metalico. |
| US5014605A (en) * | 1990-02-21 | 1991-05-14 | Briggs & Stratton Corporation | Magnesium piston coated with a fuel ingition products adhesive |
| CA2037660C (en) * | 1990-03-07 | 1997-08-19 | Tadashi Kamimura | Methods of modifying surface qualities of metallic articles and apparatuses therefor |
| DE59206839D1 (de) | 1991-07-04 | 1996-09-05 | New Sulzer Diesel Ag | Auslassventil einer Diesel-Brennkraftmaschine und Verfahren zum Herstellen des Ventils |
| JPH0525655A (ja) * | 1991-07-15 | 1993-02-02 | Komatsu Ltd | アルミニウム系母材の表面硬化方法および表面硬化アルミニウム系部材 |
| JP3148340B2 (ja) | 1991-08-27 | 2001-03-19 | 福田金属箔粉工業株式会社 | ハードフェーシング用高靱性クロム基合金、その粉末、および該合金を肉盛した自動車用エンジンバルブ |
| US5194304A (en) * | 1992-07-07 | 1993-03-16 | Ford Motor Company | Thermally spraying metal/solid libricant composites using wire feedstock |
| US5554415A (en) * | 1994-01-18 | 1996-09-10 | Qqc, Inc. | Substrate coating techniques, including fabricating materials on a surface of a substrate |
| DK172987B1 (da) * | 1994-12-13 | 1999-11-01 | Man B & W Diesel As | Cylinderelement, nikkelbaseret pålægningslegering og anvendelse af legeringen |
| US5640667A (en) * | 1995-11-27 | 1997-06-17 | Board Of Regents, The University Of Texas System | Laser-directed fabrication of full-density metal articles using hot isostatic processing |
| US6350326B1 (en) * | 1996-01-15 | 2002-02-26 | The University Of Tennessee Research Corporation | Method for practicing a feedback controlled laser induced surface modification |
| EP0956378B1 (en) * | 1996-01-15 | 2003-04-02 | The University Of Tennessee Research Corporation | Laser induced improvement of surfaces |
| US5985056A (en) * | 1996-01-15 | 1999-11-16 | The University Of Tennessee Research Corporation | Method for laser induced improvement of surfaces |
| US5773078A (en) * | 1996-06-24 | 1998-06-30 | General Electric Company | Method for depositing zirconium oxide on a substrate |
| US6001426A (en) * | 1996-07-25 | 1999-12-14 | Utron Inc. | High velocity pulsed wire-arc spray |
| US5715270A (en) * | 1996-09-27 | 1998-02-03 | Mcdonnell Douglas Corporation | High efficiency, high power direct diode laser systems and methods therefor |
| US5759932A (en) * | 1996-11-08 | 1998-06-02 | General Electric Company | Coating composition for metal-based substrates, and related processes |
| DE19740205B4 (de) * | 1997-09-12 | 2004-11-25 | Fraunhofer-Gesellschaft zur Förderung der angewandten Forschung e.V. | Verfahren zum Aufbringen einer Beschichtung mittels Plasmaspritzens |
| JP3491811B2 (ja) * | 1997-10-31 | 2004-01-26 | スズキ株式会社 | 摺動部材及びピストン |
| US6127046A (en) * | 1997-12-04 | 2000-10-03 | Cummins Engine Company, Inc. | Formation of a graphite-free surface in a ferrous material to produce an improved intermetallic bond |
| US6016227A (en) * | 1998-07-31 | 2000-01-18 | The University Of Tennessee Research Corporation | Apparatus and method for producing an improved laser beam |
| US5934174A (en) * | 1998-10-02 | 1999-08-10 | Cummins Engine Company, Inc. | Lightweight articulated piston head and method of making the piston head |
| CN1192123C (zh) * | 1999-02-19 | 2005-03-09 | 大众汽车有限公司 | 处理部件表面的方法 |
| CN1192121C (zh) * | 1999-02-19 | 2005-03-09 | 大众汽车有限公司 | 处理部件表面的方法和装置 |
| US6294225B1 (en) * | 1999-05-10 | 2001-09-25 | The University Of Tennessee Research Corporation | Method for improving the wear and corrosion resistance of material transport trailer surfaces |
| US6299707B1 (en) * | 1999-05-24 | 2001-10-09 | The University Of Tennessee Research Corporation | Method for increasing the wear resistance in an aluminum cylinder bore |
| US6173886B1 (en) * | 1999-05-24 | 2001-01-16 | The University Of Tennessee Research Corportion | Method for joining dissimilar metals or alloys |
| US6284067B1 (en) * | 1999-07-02 | 2001-09-04 | The University Of Tennessee Research Corporation | Method for producing alloyed bands or strips on pistons for internal combustion engines |
| JP2001098989A (ja) * | 1999-09-29 | 2001-04-10 | Mazda Motor Corp | エンジンの制御装置及びエンジンの制御装置の異常診断装置 |
| US6229111B1 (en) * | 1999-10-13 | 2001-05-08 | The University Of Tennessee Research Corporation | Method for laser/plasma surface alloying |
| US6328026B1 (en) * | 1999-10-13 | 2001-12-11 | The University Of Tennessee Research Corporation | Method for increasing wear resistance in an engine cylinder bore and improved automotive engine |
| DE10029810A1 (de) * | 2000-06-16 | 2001-12-20 | Mahle Gmbh | Kolben für Dieselmotoren |
| GB2365507B (en) * | 2000-08-02 | 2004-09-15 | Federal Mogul Technology Ltd | Engine piston and manufacture |
| US6936118B2 (en) * | 2001-08-07 | 2005-08-30 | Northeastern University | Process of forming a composite coating on a substrate |
| US6602550B1 (en) * | 2001-09-26 | 2003-08-05 | Arapahoe Holdings, Llc | Method for localized surface treatment of metal component by diffusion alloying |
| JP2003278597A (ja) * | 2002-03-20 | 2003-10-02 | Mitsubishi Heavy Ind Ltd | エンジン部材、排気弁、ピストンクラウン、及び内燃機関型エンジン |
| US6818532B2 (en) * | 2002-04-09 | 2004-11-16 | Oriol, Inc. | Method of etching substrates |
| JP2003343351A (ja) * | 2002-05-24 | 2003-12-03 | Hitachi Unisia Automotive Ltd | 内燃機関のピストン |
| US6749894B2 (en) * | 2002-06-28 | 2004-06-15 | Surface Engineered Products Corporation | Corrosion-resistant coatings for steel tubes |
| US6973723B2 (en) * | 2003-01-08 | 2005-12-13 | International Engine Intellectual Property Company, Llc | Piston formed by powder metallurgical methods |
-
2006
- 2006-05-10 US US11/431,297 patent/US7458358B2/en active Active
-
2007
- 2007-05-10 BR BRPI0713095A patent/BRPI0713095B1/pt not_active IP Right Cessation
- 2007-05-10 WO PCT/US2007/068633 patent/WO2007134148A2/en not_active Ceased
- 2007-05-10 EP EP07783557.7A patent/EP2021176B1/en not_active Ceased
- 2007-05-10 JP JP2009510169A patent/JP5300150B2/ja not_active Expired - Fee Related
- 2007-05-10 CN CN2007800239237A patent/CN101479102B/zh active Active
- 2007-05-10 KR KR1020087029574A patent/KR101383098B1/ko not_active Expired - Fee Related
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2009536712A5 (enExample) | ||
| JP5300150B2 (ja) | スチールピストンのための熱酸化保護表面 | |
| CN105904068B (zh) | 活塞和/或气缸盖和/或气缸孔上的ptwa涂层 | |
| CN101285162B (zh) | 涂覆活塞环槽的热喷涂方法、喷涂丝的用途和活塞 | |
| CN105431624B (zh) | 产生内燃机中使用的活塞的氧化保护层的方法和具有氧化保护层的活塞 | |
| KR100762526B1 (ko) | 디젤 엔진용 피스톤 | |
| JP2018534479A (ja) | 断熱された鋼ピストンクラウンおよびセラミックコーティングを使用する作製方法 | |
| JP2007016736A5 (enExample) | ||
| JP2018534427A (ja) | 断熱されたエンジン部品およびセラミックコーティングを使用する作製方法 | |
| EP3114343A1 (en) | One-piece piston featuring additive machining produced combustion bowl rim and cooling gallery | |
| JP2003301279A (ja) | 運動噴霧を用いる腐食の選択制御方法 | |
| CN110607495B (zh) | 涂层内燃机气缸曲轴箱的气缸缸套工作面的等离子喷涂法 | |
| SG153818A1 (en) | Smooth outer coating for combustor components and coating method therefor | |
| CN108707853A (zh) | 增强气缸孔机械特性的激光重熔 | |
| EP3071722B1 (fr) | Procédé intégré de frittage pour microfissuration et tenue à l'érosion des barrières thermiques | |
| JP2017015053A (ja) | 内燃機関の製造方法 | |
| CN110777321B (zh) | 基于表面处理的耐磨气缸套的制造方法 | |
| CN109763089A (zh) | 一种提高MCrAlY防护涂层表面Al含量及高温服役性能的处理方法 | |
| Zyazev et al. | Effect of deposition conditions of the heat-resistant AlCo 0. 158 Cr 0. 084 Y 0. 003 coatings on structure and properties of matrix metal ZhS-32. | |
| JP2018009554A (ja) | エンジンのシリンダヘッド | |
| Sivaprahasam et al. | Mechanically alloyed Fe-SiC powder for detonation spray coating |