CN1322615C - 掺杂和表面包覆的镍钴酸锂的制备方法 - Google Patents
掺杂和表面包覆的镍钴酸锂的制备方法 Download PDFInfo
- Publication number
- CN1322615C CN1322615C CNB2005100195528A CN200510019552A CN1322615C CN 1322615 C CN1322615 C CN 1322615C CN B2005100195528 A CNB2005100195528 A CN B2005100195528A CN 200510019552 A CN200510019552 A CN 200510019552A CN 1322615 C CN1322615 C CN 1322615C
- Authority
- CN
- China
- Prior art keywords
- doping
- alms bowl
- preparation
- lithium
- oxide
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
Description
Claims (4)