JPS63199055A - 異鋼種の連続連続鋳造方法 - Google Patents
異鋼種の連続連続鋳造方法Info
- Publication number
- JPS63199055A JPS63199055A JP2931487A JP2931487A JPS63199055A JP S63199055 A JPS63199055 A JP S63199055A JP 2931487 A JP2931487 A JP 2931487A JP 2931487 A JP2931487 A JP 2931487A JP S63199055 A JPS63199055 A JP S63199055A
- Authority
- JP
- Japan
- Prior art keywords
- tundish
- steel
- casting
- remaining
- molten steel
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Continuous Casting (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2931487A JPS63199055A (ja) | 1987-02-10 | 1987-02-10 | 異鋼種の連続連続鋳造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2931487A JPS63199055A (ja) | 1987-02-10 | 1987-02-10 | 異鋼種の連続連続鋳造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS63199055A true JPS63199055A (ja) | 1988-08-17 |
| JPH0455770B2 JPH0455770B2 (enExample) | 1992-09-04 |
Family
ID=12272757
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2931487A Granted JPS63199055A (ja) | 1987-02-10 | 1987-02-10 | 異鋼種の連続連続鋳造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS63199055A (enExample) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH06114509A (ja) * | 1992-10-01 | 1994-04-26 | Nippon Steel Corp | タンディッシュ小ロット材の水素低減方法 |
| CN104625024A (zh) * | 2013-11-11 | 2015-05-20 | 林州市林丰铝电有限责任公司 | 一种铸件成型方法及其敞口包加热装置 |
-
1987
- 1987-02-10 JP JP2931487A patent/JPS63199055A/ja active Granted
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH06114509A (ja) * | 1992-10-01 | 1994-04-26 | Nippon Steel Corp | タンディッシュ小ロット材の水素低減方法 |
| CN104625024A (zh) * | 2013-11-11 | 2015-05-20 | 林州市林丰铝电有限责任公司 | 一种铸件成型方法及其敞口包加热装置 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0455770B2 (enExample) | 1992-09-04 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| CN1061275C (zh) | 金属带材的铸造 | |
| JP4102352B2 (ja) | 熱間再使用タンディッシュを用いたステンレス溶鋼の連続鋳造方法 | |
| CN112296292A (zh) | 一种双流板坯连铸的作业方法 | |
| US4064930A (en) | Continuous casting method using a ladle bogie | |
| JPH0829402B2 (ja) | 連続鋳造方法 | |
| JP3395706B2 (ja) | 連続鋳造方法 | |
| JPH0455770B2 (enExample) | ||
| JP4600095B2 (ja) | タンディッシュの熱間再使用方法 | |
| JPH0675756B2 (ja) | スライディングノズルの開孔方法 | |
| JPS61103653A (ja) | タンデイツシユのスラグ除去方法 | |
| JP4189313B2 (ja) | 熱間回転タンディッシュを用いた溶鋼の連続鋳造方法 | |
| JPH03210948A (ja) | タンディッシュ | |
| JP2786814B2 (ja) | 鋼の連続鋳造におけるタンディッシュの再使用方法 | |
| JP2923477B2 (ja) | 連続鋳造法 | |
| JPH01107949A (ja) | タンデイツシユ無補修再使用方法 | |
| JPH11277193A (ja) | 連続鋳造用タンディッシュの熱間再使用方法 | |
| JPH0526589B2 (enExample) | ||
| CN111570744A (zh) | 连铸机浇注装置及浇注方法 | |
| JPH0626760B2 (ja) | 連続鋳造におけるタンデイツシユの再使用方法 | |
| JPH01157747A (ja) | 連続鋳造用タンディッシュからの注入開始方法 | |
| JPH05237614A (ja) | 環状鋼製品の連続鋳造方法および連続鋳造装置 | |
| JPH01237061A (ja) | 連続鋳造用タンディッシュの再使用方法 | |
| JPH02151352A (ja) | 連続鋳造におけるタンデイツシユの再使用方法およびその装置 | |
| JPH01107950A (ja) | 水平連続鋳造用タンデイッシュ | |
| JPS61279338A (ja) | 造塊操業法 |