JPS6130007B2 - - Google Patents
Info
- Publication number
- JPS6130007B2 JPS6130007B2 JP53078580A JP7858078A JPS6130007B2 JP S6130007 B2 JPS6130007 B2 JP S6130007B2 JP 53078580 A JP53078580 A JP 53078580A JP 7858078 A JP7858078 A JP 7858078A JP S6130007 B2 JPS6130007 B2 JP S6130007B2
- Authority
- JP
- Japan
- Prior art keywords
- less
- steel
- temperature
- stress corrosion
- cracking
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Classifications
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02P—CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02P10/00—Technologies related to metal processing
- Y02P10/20—Recycling
Landscapes
- Heat Treatment Of Steel (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP7858078A JPS558404A (en) | 1978-06-30 | 1978-06-30 | Manufacture of austenitic stainless steel used in atmosphere of high-temperature and high-pressure water |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP7858078A JPS558404A (en) | 1978-06-30 | 1978-06-30 | Manufacture of austenitic stainless steel used in atmosphere of high-temperature and high-pressure water |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS558404A JPS558404A (en) | 1980-01-22 |
JPS6130007B2 true JPS6130007B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | 1986-07-10 |
Family
ID=13665835
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP7858078A Granted JPS558404A (en) | 1978-06-30 | 1978-06-30 | Manufacture of austenitic stainless steel used in atmosphere of high-temperature and high-pressure water |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS558404A (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN103469114A (zh) * | 2013-08-02 | 2013-12-25 | 安徽三联泵业股份有限公司 | 水泵泵壳用高韧性不锈钢材料及其制造方法 |
Families Citing this family (8)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS57169069A (en) * | 1981-04-10 | 1982-10-18 | Hitachi Ltd | Bwr plant |
DE3407307A1 (de) * | 1984-02-24 | 1985-08-29 | Mannesmann AG, 4000 Düsseldorf | Verwendung einer korrosionsbestaendigen austenitischen eisen-chrom-nickel-stickstoff-legierung fuer mechanisch hoch beanspruchte bauteile |
DE3407305A1 (de) * | 1984-02-24 | 1985-08-29 | Mannesmann AG, 4000 Düsseldorf | Verwendung einer korrosionsbestaendigen austenitischen legierung fuer mechanisch hoch beanspruchte, schweissbare bauteile |
WO1987002388A1 (en) * | 1985-10-15 | 1987-04-23 | Aichi Steel Works Ltd. | High strength stainless steel, and process for its production |
JPS62287051A (ja) * | 1986-06-03 | 1987-12-12 | Kobe Steel Ltd | 耐粒界腐食性並びに耐粒界応力腐食割れ性の優れたオ−ステナイト系ステンレス鋼 |
JP2811255B2 (ja) * | 1992-05-20 | 1998-10-15 | 新日本製鐵株式会社 | 高温クリープ破断特性の優れたオーステナイト系ステンレス鋼の製造方法 |
JP5014915B2 (ja) * | 2007-08-09 | 2012-08-29 | 日新製鋼株式会社 | Ni節減型オーステナイト系ステンレス鋼 |
EP2562284B1 (en) * | 2010-04-19 | 2020-06-03 | JFE Steel Corporation | Cr-CONTAINING STEEL PIPE FOR LINE PIPE AND HAVING EXCELLENT INTERGRANULAR STRESS CORROSION CRACKING RESISTANCE AT WELDING-HEAT-AFFECTED PORTION |
Family Cites Families (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5333916A (en) * | 1976-09-10 | 1978-03-30 | Nippon Steel Corp | Austenitic stainless steel with excellent intra- and intergranular stress corrosion cracking resistance |
JPS592739B2 (ja) * | 1976-09-21 | 1984-01-20 | 新日本製鐵株式会社 | 耐粒界応力腐食割れ性のすぐれたオ−ステナイトステンレス鋼 |
JPS5476412A (en) * | 1977-11-30 | 1979-06-19 | Nippon Steel Corp | Austenitic stainless steel having superior resistance to intragranular and intergranular corrosion cracking in high temperature, high pressure water |
-
1978
- 1978-06-30 JP JP7858078A patent/JPS558404A/ja active Granted
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN103469114A (zh) * | 2013-08-02 | 2013-12-25 | 安徽三联泵业股份有限公司 | 水泵泵壳用高韧性不锈钢材料及其制造方法 |
Also Published As
Publication number | Publication date |
---|---|
JPS558404A (en) | 1980-01-22 |