JPS58222128A - ハロゲン含有ゴムの耐水性改良法 - Google Patents

ハロゲン含有ゴムの耐水性改良法

Info

Publication number
JPS58222128A
JPS58222128A JP57103907A JP10390782A JPS58222128A JP S58222128 A JPS58222128 A JP S58222128A JP 57103907 A JP57103907 A JP 57103907A JP 10390782 A JP10390782 A JP 10390782A JP S58222128 A JPS58222128 A JP S58222128A
Authority
JP
Japan
Prior art keywords
rubber
halogen
water resistance
acid acceptor
vulcanization
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP57103907A
Other languages
English (en)
Other versions
JPH0130856B2 (ja
Inventor
Shigeo Miyata
茂男 宮田
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Kyowa Chemical Industry Co Ltd
KH Neochem Co Ltd
Original Assignee
Kyowa Chemical Industry Co Ltd
Kyowa Kagaku Kogyo KK
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kyowa Chemical Industry Co Ltd, Kyowa Kagaku Kogyo KK filed Critical Kyowa Chemical Industry Co Ltd
Priority to JP57103907A priority Critical patent/JPS58222128A/ja
Priority to EP83105885A priority patent/EP0097330B1/en
Priority to DE8383105885T priority patent/DE3366247D1/de
Priority to CA000430502A priority patent/CA1222591A/en
Publication of JPS58222128A publication Critical patent/JPS58222128A/ja
Priority to US06/636,710 priority patent/US4558102A/en
Publication of JPH0130856B2 publication Critical patent/JPH0130856B2/ja
Granted legal-status Critical Current

Abstract

(57)【要約】本公報は電子出願前の出願データであるた
め要約のデータは記録されません。

Description

【発明の詳細な説明】 本発明は、耐水性さらには耐薬品性、絶縁性などの改善
さnたノ・ロゲン含有ゴム加硫物會提供できるハロゲン
含有ゴムの耐水性改良方法に関する。
硫に際し、受酸剤として下記式(1) %式% 但し式中、M”+BMg及びZnよりなる群からえらば
れ友少なくとも一種の金属元素を示し、Ann価のアニ
オンを示し、nは該アニオンの価数全示し、セしてm、
z、m14夫々下記条件を満足する数に示す、 X≧2の正の数、 2≦2の正の数、 mは正の数、 で表わされるハイドロタルサイト類化合物またはその焼
成物を用いること全特徴とするハロゲン含有がムの耐水
性改良法に関する。
例えば塩素化ポリエチレンゴム、ポリクロログレンゴム
、塩素化ブチルゴム等の如きハロゲン含有ゴムは耐候性
、耐薬品性などのとくに優れたゴムとして利用されてい
る。そして、このようなハロゲン含有ゴムの加硫に際し
てrユ加硫促進剤のほかに受酸剤ケ用いる必要があり、
従来、この目的にQゴたとえば水酸化マグネシウム、水
酸化カルシウム、酸化鉛その他の周期律表第り族及び第
■α族の元素の酸化物、水酸化物、炭酸塩などが用いら
れてきた。
しかしながら、これら受酸剤の利用には種々の難点があ
る。たとえば、周期律表第■族元素の化合物ケ受酸剤と
して使用した場合、加硫処理に際して、これら元素の吸
湿性の強いハロゲン1ヒ物及び/又Ire j4基性ハ
ロゲン化合物が生成するためと推測されるが、得られた
力lllフコ9ム製悪くなるという欠陥がある。そ[2
て、耐水性が悪いということは同時に加硫ゴム製品の絶
縁性能が低下することケ意味する。従って、従来、耐水
性や耐薬品性ケ強く要求される用途に対して?ユ、受酸
剤として酸化鉛の如き鉛化合物全使用する必要があった
。ところが、このような鉛系受酸剤化合物全相いると、
加硫速度が遅い難点及び加硫の根方るという他の問題が
生ずる欠陥があるし、加えて受酸剤それ自体の毒性の問
題もある等のトラブルがあった。
本発明者等は、ハロゲン含有ゴムにおける受酸剤の上述
の如き欠陥を克服すべく竺究を行ってきた。
その結果、前記式(1)で表わされるハイドロタルサイ
ト類化合物又はその焼成物全受酸剤として用いることに
よって、上記欠陥が有利に克服でき、加硫速度の低下や
り0硫の程度の低下を伴うことなしに、改善された耐水
性さらには耐薬品性、絶縁性などの改善された・・ログ
ン含有ゴム加硫物を提供できることケ発見した。
本発明者ケ包む発明者等はζ先に、式(1)化合物の一
部と重複するハイドロタルサイト類似結晶性化合物がゴ
ム用チアゾール系加硫促進剤用の二次 5 − 力旧淵促進剤として優れた特性含有することを知って特
公昭55ー41653号に開示したが、今回、上記弐i
l+化合物又はその焼成物をハロゲン含有ゴム未加硫組
成物の加硫に際し、受酸剤として使用すると、ハロゲン
含有ゴムにおける前述の欠陥が有利に克服できることが
わかった。
本発明者等の研究によf′Lば、F記式(1)化合物げ
天然鉱物ハイドロタルサイトMQaAl t( OH 
l taCO6・lH,Oと類似の結晶構造を示し、弐
(11化合物のアニオンA がイオン交換性を有するこ
と及び式(1)化合物が弱アルカリ性を示す化合物であ
るためと推測しているが、ハロゲン含有ゴムの受酸剤と
して用いた場合に、加硫遅へのトラブルを生ぜずに優れ
た耐水性改善効果が達成できることが発見された。
従来の周期律表第■族金属化合物受酸剤は、ハロゲン含
有ゴムの加硫に際して発生する酸を中和 6 − 反応によって不活性化する機構に依っているため、たと
えば1化マグネシウムの如き極めて吸湿1件の化合物ケ
形成し、その結果、ハロゲン含有ゴム加硫製品の耐水性
を低下させるが、こrLK灼1.て、・上記式(1)化
合物はぞn自体吸湿性が小さく、袖つハロゲン含有ゴム
の力旧艷に際して発生する際會イオン交換反応に工って
該低吸湿性の式+11化合物中に捕捉不活性化する機構
に依るためと推測されるが、後に比較例と共に実施例ケ
挙げて実験的に示すように、顕著に改善さn*、ノ為ロ
ゲン含有ゴムの耐水性改良効果全発揮することがわかっ
た。
従って、本発明の目的はハロゲン含有ゴムの優れた耐水
性改良法を提供するにある。
本発明のハロゲン含有ゴム用受酸剤は下記式(1)で表
ゎさfl、お化合物父ゆそf)J酸物アあ、0MvA’
!(OH)*z+a−Bg (A”−)g ・7JI、
0・・・・・・(1) 但し式中、M2+はMg及びZnよりなる群からえらば
れた少なくとも一種の金属元素を示し、Aun価のアニ
オンを示し% nn該アニオンの価数を示し、そしてX
% 2%mは、夫々、下記条件を満足する数を示す、X
≧2の正の数、 2≦2の正の数、 mは正の数。
上記A の好ましい911として、coH−、ことがで
きる。又、M2−とじてnkfrtが好ましい。Xは、
好1しくり8≧X≧3、特にに6≧X≧4がエリ好まし
い。又、式(11化合物のBIIT法比表面積は適宜に
選択できるか、好ましくは約20〜約100ゴ/Il程
度である。更に、式(1)化合物の粒子サイズは、ゴム
材料中における分散性の良い点から小さい粒子サイズを
選ぶのか好ましい。例えば約0.1μ〜約10μの二次
粒子径全例示することかできる。
式(1)化合物又はその焼成物は、ゴム材料との相容性
を向上させる目的でたとえば高級脂肪酸のアルカリ金属
塩に代表さ扛るアニオン系界面活性剤で表面処理して用
いるのが好ましい。式(1)化合物重数に基いて約05
〜約10%程度の表面付着乃至吸N蓋會ν0示すること
ができる。
表面処理は、例えば、水、低級アルコール、これらの混
合物なとめ溶媒系中で、該溶媒に溶解したアニオン系界
面活性剤と式(1)化合物とを、たとえは攪拌条件下に
、接触させることにより行うことができる。この工りな
表面処理に用いるアニオン系界面活性剤の例としては、
例えばステアリン酸ソーダ、オレイン酸ソーダ、パルミ
チン酸カリ、ラウリン酸ンーダ、Rヘニン酸カリ、ラウ
リルペ 9 − ンゼンスルホン醒ソーダ、オクタデシル硫酸カリ、ラウ
リルスルホン酸ソ′−ダ、ツナトリウム・2−などの如
きアニオン系界面活性剤全例示することができる。
仝発明の耐水性改良法によれば、ゴム用チアゾール系加
硫促進剤不添加のハロゲン官有ゴム未加硫組成物の加硫
に除し、受酸剤としてヒ述の如き式[1)ハイドロタル
サイト類化合物又はその焼成物を用いる。焼成物として
は、たとえば、約800℃までの高度、好11.<は約
300〜約800℃の温度の焼成物ケ例示できる。該受
酸剤の使用量は適宜に選択できるが、ハロゲン含有ゴム
100電歇部に対して約1〜約40重量部好ましくは約
1〜約25電前部、とくには約2〜約20重童部のごと
き使用量を例示することができる。
−10− ハロゲン含有ゴム未加硫組成物は、式(1)受酸剤のほ
かに、力旧流促進剤(但し本発明に於てはゴム用チアゾ
ール系加硫促進剤ケ除外する)、hIF IMf剤、そ
の他各種の配合剤を含有するのが普通である。
加硫剤の例としては、p−キノンヅオキシム、4.4′
−ゾチオソモルホリンT + p’−ヅベンゾイルキノ
ンソオキシム、ポリp−ジニトロベンゼン、イオウ、な
ど葡あげることができる。父、加硫促進剤の例としては
、n−ブチルアルデヒドアニリン、1.3−&フェニル
グアエノン3,5−ソメルカグトー1,2.4− トリ
アゾール、ノカテコールボレートのり一〇−)リルグア
ニノンキシルー2−ベンゾチアゾリルスルフェンアミド
、N−オキシジエチレン−2−ベンゾチアゾリルスルフ
ェンアミド、テトラメチルチウラムノスルフィド、ジペ
ンタメチレンチウラムテトラスルフィド、テトラメチル
チウラムノスルフィド、ソアミノ、ポリアミン、有機過
酸化物、ジブチルソチオ力ルパミンV!唾鉛、など螢あ
げることができる。
更に、他の各種の配合剤たとえr」゛、各種充填剤、補
強剤、可塑剤、カロエ助剤、架橋剤、老化防止剤、@ヤ
ト、難燃剤などの配合剤全例示することができる。これ
らの配合剤の使用量に、この技術分野で公知の範囲量で
適宜に選択利用でき、!!た、配合ゴム組成物は常法に
従って加熱加硫することができる。
本発明でオl用するハロゲン含有ゴムの例としけ、塩素
化ポリエチレン、塩素化ポリプロピレン、クロロスルホ
ン化4.. 、l、エチレン、ポリエピクロルヒドリン
、ポリクロロルン、フッ素ゴム、塩素化ブチルゴム、ブ
ロム化ブチルゴム、t’n素化エチレン−10ピレン共
重合体、@塩素アクリルゴム、エピクロルヒドリン−エ
チレンオキサイド共重合体、エピクロルヒドリン−アリ
ルグリシジルエーテル共重合体、など全例示することが
できる。
以下、実施例にエリ本発明方法実施の数例についてさら
に詳しく説明する。
実施例1−2及び比較例1−2 第1表に示す配合比で、クロロスルホン化ポリエチレ/
ゴム、各種充填材、受酸剤、促進剤その他の配合剤を配
合し、ロールで素練りしたf&160℃で30分間加硫
した。
−13− 第  1  表 配 合 剤       配合部(1愉)クロロスルホ
ン化pすz−y−to。
レン(ハイノぞロン401 老化防止剤 NBC3 ハードクレー              60F’ 
E F  ブラック          15Kenf
las A             10プロセスオ
イル           17ワセリン      
          3マイクロクリスタリン    
      2ワツクス 促進剤 DM              1促進創 
TRA             2受酸剤     
           10加硫物ケ、70℃の温水に
7日間浸漬後の容積−14− の増加率(%)を測定した。容積が増大する程、吸水率
が大きく耐水性が悪いことケ示す。
その結果?第2表に示す。
−15− 実施vl13及び比較例3〜4 第3秋に示す配合比で、塩素化ポリエチレンゴム(塩素
含有量40 ’ult%) を処方し、ロールで素練り
後、155℃で30分間加値した。このようにして得ら
れた加硫物について、70℃で7日間水に陵し耐水性ケ
チストし皮後の、体積の増加率を測定した。その結果を
第4表に示す。
第 3 表 塩素化ポリエチレン の処方 配合剤   配合部(重量) 塩素化ポリエチレン        100充填剤(カ
ーボンブラック)50 可塑剤、TOTAI           j。
加硫剤                  1加硫促
進剤               2受酸剤    
           1〇−17− = 16− −18− 実施例4.5及び比較例5.6 第5表に示す配合比で、フッ素ゴム(ダイエルG−50
11ケ処方し、素練りした債、150℃で30分間加硫
した。加硫物の引張り強度′(i−第6表に示す。
このようにして惧らrした加硫物を、90℃の温水に1
6日間浸し、その僕、体積の増加率及び引張り強度を測
定した。
イの結果ケ第6衣に示す。以上の結果から酸化鉛は、酸
化マグネシウムに比べて耐水性は良いが、加硫が弱いた
め、例えば引張り強度が劣る。こnに対し、ハイドロタ
ルサイト類化合物は、加硫性、耐水性ともにすぐれてい
ることかわかる。
第 5 表 フッ素ゴムの処方 配合剤   配合部(屯営) フッ素ゴム(ダイエルG−5011100カーざンブラ
ック          20加硫剤        
          。
受酸剤               15−21− 手続補正書 昭和58年6月16日 特許庁長官若杉和夫殿 1、事件の表示 特願昭57−103907号 2、発明の名称 ハロゲン含有ゴムの耐水性改良法 3、補正をする渚 事件との関係  特許出願人 住 所   東京都中央区日本橋茅場町弐丁目弐拾番地
名 称   協和化学工業株式会社 (氏 名) 4代 理 人〒107 (ほか1名) 6、 1i4i iE ’) ’41’ !!   明
細墳−の”特許請求の範囲“及び、σ”−\、   ”
発明の詳細な説明“の欄〜師) 7°          別紙のとおり(+]  明細
書の”特許請求の範囲”の欄の記載を以下のとおり訂正
する。
「1.  ゴム用チアゾール系加硫促進剤不添加のハロ
ダン含有ゴム未加硫組成物の加硫に際し、受酸剤として
下記式(1) %式% (11 但し式中、M友十はMg及びZnより々る群からえらば
れた少なくとも一種の金属元素を示し1 .4n−はn価のアニオンを示し、nは該アニオンの価
数を示し、そしてZ、  z。
mは、夫々、下記条件を満足する数を示す、 ”・。
x 〉2の正の数、 zく2の正の数 mは正の数 で表わされるハイドロタルサイト類化合物またはその焼
成物のアニオン系界面活性剤表面処理物を用いることを
特徴とするハロダン含有ゴムの耐水性改良法。
2 該アニオン系界面活性剤表面処理物を、ハロダン含
有ゴム100重量部に基いて約1〜約40重量部配合し
て用いる特許請求の範囲第1項記載の耐水性改良法。」 〔■〕 明細書の”発明の詳細な説明”の欄の記載を、
以下のとおり訂正する。
(1)明細書第3頁10行に、「その焼成物」とある後
に、 「 のアニオン系界面活性剤表面処理物 」と加入する
(2)明細書第5頁9行に、「その焼成物」とある後に
、 「 のアニオン系界面活性剤表面処理物 」と加入する
(3)明細書第7頁下から2行に、「その焼成物」とあ
る後に、 「 のアニオン系界面活性剤表面処理物 」と加入する
(4)明細書第9頁7行に、「表面処理して用いるのが
好ましい。」とあるを、 「 表面処理して用いる。」 と訂正する。
(5)明細書第10頁10行に「その焼成物」とある後
に、 「 のアニオン系界面活性剤表面処理物 」と加入する
(6)  明細書第14頁の第1表中に、「Kenfl
es        10プロセスオイル    17
Jとあるを、 3− 「 プロセスオイル(KenflexA)   27 
」と訂正する。
(7)明細書第14頁の第1表中に、 [促進剤DM        l 促進剤TRA       2 受酸剤        10」 とあるを、「促進剤T
RA       2 受酸剤(第2表に   lO 示した) (註)TEA:Nペンタメチレンチウラムテトラスルフ
ィド 」 と訂正する。
(8)明細書第13頁7行に、「比較例1−2」とある
を、 r 比較例1−4 」 と訂正する。
 4− 顛 明細書第17頁1行に「比較例3〜4」とあるを、 「 比較例5〜7 」 と訂正する。
Qll  明細書第17頁の第3表中に、「可塑剤、T
OTM        30加硫剤     l 加硫促進剤           2 受酸剤     10j とあるを、 「可塑剤(DO,P)        a。
加硫剤(硫黄)         1 加硫促進剤(促進剤22)    2 受酸剤(第4表に示した)10 (註)DOP:ソオクチルフタレート と訂正する。
02)明細書第18頁の第4表を、以下のとお9訂正す
る。
「   第 4 表 塩素化ポリエチレンの耐水性 実施例33)   Mg、Al、(OH’)、4Co3
−4色04.2比較列5           //、
        8.1〃 6   酸化マグネシウム
       16.2〃 7   水酸化マグネシウ
ム      15.13)・・・受酸剤の重量にもと
づいて、2%のポリオキシメチレンスルホン酸ソーダに より、水媒体中で表面処理されている。
尚、比較例に於てはアニオン系界面活性剤による表面処
理が省略されている。      」Q31  明細書
第19頁1行に、「比較例5,6」とあるを、  7− 「 比較例8〜11 」 と訂正する。
04)明細書第20頁の第5表中に、 「加硫剤    3 受酸剤    15」 とあるを、 アミン)           3 受酸剤(第6表に示した)      15」と訂正す
る。
0タ 明細書第21頁の第6表を、以下のとおυ訂正す
る。
 8 − 4)・・・受酸剤の重量にもとづいて、2%のイソプロ
ピルトリイソステアロイルチタ ネートで表面処理されている。
5)・・・受酸剤の重量にもとづいて、1.5%のβ−
(3,4−エポキシシクロヘキシ ル)エチルトリメトキシシランで表面 処理されている。
尚、比較例に於てはアニオン系界面活性剤による表面処
理が省略されている。      」Oe  明細書第
10頁第2〜4行に、「、ツナトリウム・2−スルホエ
チル・α−スルホステアレート、チタン系カップリング
剤、シラン系カップリング剤、」とあるを、 「、ツナトリウム・2−スルホエチル・α−スルホステ
アレートの如きCa””80の高級脂肪酸のアルカリ金
属塩、例えばイソプロピルトリイソステアロイルチタネ
ート、イソゾロビルトリドデシルベンゼンスルホニルチ
タネート、イソプロピルトリス(ソオクチル・セイロホ
スフエート)チタネート、テトラオクチルビス(ソトリ
デシルホスファイト)チタネートの如キチタン系カップ
リング剤、例えばβ−(3,4−エポキシシクロヘキシ
ル)エチルトリメトキシシラン、ビニルトリエトキシシ
ラン、r−アミノプロピルトリメトキシシランの如きシ
ラン系カップリング剤、」 と訂正する。
11−

Claims (1)

  1. 【特許請求の範囲】 L ゴム用チアゾール系加硫促進剤不添加のノ・ロダン
    含有ゴム未加硫組成物の加硫に際し、受酸剤として下記
    式(1) %式% (1) 但し式中、M2+はMQ及びZnよりなる詳からえらば
    れ几少なくとも一種の金属元zt示し、 下記条件を満足する数會示す、 2≦2の1し、 mは正の数、 で表わされるハイドロタルサイト類化合物ま71cは、
    その焼成物を用いることを%徴とするノ10ゲン含有ゴ
    ムの耐水性改良法。 2 核酸(1)で表わされる受酸剤をハロゲン含有ゴム
    100を置部に基いて約1〜約25重量部配■ 合しンαる特許請求の範囲第1項記載の耐水性改良法。
JP57103907A 1982-06-18 1982-06-18 ハロゲン含有ゴムの耐水性改良法 Granted JPS58222128A (ja)