JP2011524946A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2011524946A5 JP2011524946A5 JP2011511601A JP2011511601A JP2011524946A5 JP 2011524946 A5 JP2011524946 A5 JP 2011524946A5 JP 2011511601 A JP2011511601 A JP 2011511601A JP 2011511601 A JP2011511601 A JP 2011511601A JP 2011524946 A5 JP2011524946 A5 JP 2011524946A5
- Authority
- JP
- Japan
- Prior art keywords
- sol
- film
- heating
- gel
- raw
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Applications Claiming Priority (3)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| US12/128,080 | 2008-05-28 | ||
| US12/128,080 US20090297923A1 (en) | 2008-05-28 | 2008-05-28 | Sol-gel derived high performance catalyst thin films for sensors, oxygen separation devices, and solid oxide fuel cells |
| PCT/US2009/003001 WO2009151528A1 (en) | 2008-05-28 | 2009-05-14 | Sol-gel derived high performance catalyst thin films for sensors, oxygen separation devices, and solid oxide fuel cells |
Publications (3)
| Publication Number | Publication Date |
|---|---|
| JP2011524946A JP2011524946A (ja) | 2011-09-08 |
| JP2011524946A5 true JP2011524946A5 (enExample) | 2014-01-16 |
| JP5465240B2 JP5465240B2 (ja) | 2014-04-09 |
Family
ID=40974510
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP2011511601A Expired - Fee Related JP5465240B2 (ja) | 2008-05-28 | 2009-05-14 | センサー、酸素分離装置、および固体酸化物燃料電池のためのゾルゲル由来の高性能触媒薄膜 |
Country Status (5)
| Country | Link |
|---|---|
| US (1) | US20090297923A1 (enExample) |
| EP (1) | EP2294645A1 (enExample) |
| JP (1) | JP5465240B2 (enExample) |
| CN (1) | CN102047477A (enExample) |
| WO (1) | WO2009151528A1 (enExample) |
Families Citing this family (12)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| KR20110109104A (ko) * | 2010-03-30 | 2011-10-06 | 삼성전기주식회사 | 금속 산화물-이트리아 안정화 지르코니아 복합체 및 이를 포함하는 고체산화물 연료전지 |
| CN102012394B (zh) * | 2010-10-14 | 2013-03-13 | 北京科技大学 | 一种氧传感器用纳米级氧扩散障混合导体粉体的制备方法 |
| WO2012162642A2 (en) | 2011-05-26 | 2012-11-29 | Advenira Enterprises, Inc. | System and process for coating an object |
| EP2726186B1 (en) * | 2011-09-27 | 2017-05-24 | Dow Global Technologies LLC | Branched alkoxylate surfactant composition |
| KR20130097962A (ko) * | 2012-02-27 | 2013-09-04 | 한국생산기술연구원 | 졸겔법에 의한 중·저온형 고체산화물 연료전지용 공기극 분말 합성방법 |
| CN103887520A (zh) * | 2012-12-21 | 2014-06-25 | 中国科学院大连化学物理研究所 | 一种低温烧结制备固体氧化物燃料电池复合阴极的方法 |
| CN104091960B (zh) * | 2014-07-25 | 2016-05-11 | 哈尔滨工业大学 | 一种在燃料电池工作期间调控氧化物电极微观形貌的方法 |
| US10374227B2 (en) | 2014-12-05 | 2019-08-06 | Lg Chem, Ltd. | Positive electrode active material, method for preparing the same and lithium secondary battery including the same |
| CN107004846B (zh) | 2014-12-05 | 2020-04-24 | 株式会社Lg 化学 | 正极活性材料、制备其的方法以及包含其的锂二次电池 |
| KR101835956B1 (ko) * | 2015-03-06 | 2018-03-08 | 주식회사 엘지화학 | 전극의 제조방법, 이로 제조된 전극, 상기 전극을 포함하는 전극 구조체, 상기 전극을 포함하는 연료 전지 또는 금속 공기 이차 전지, 상기 연료 전지 또는 금속 공기 이차 전지를 포함하는 전지 모듈, 및 전극 제조용 조성물 |
| US11635404B2 (en) | 2019-04-04 | 2023-04-25 | Battelle Energy Alliance, Llc | Methods for manufacturing electrochemical sensors, and related electrochemical sensors |
| CN111370708B (zh) * | 2020-03-20 | 2021-09-07 | 四川轻化工大学 | 一种固体氧化物燃料电池电极及其制备方法 |
Family Cites Families (19)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US5527480A (en) * | 1987-06-11 | 1996-06-18 | Martin Marietta Corporation | Piezoelectric ceramic material including processes for preparation thereof and applications therefor |
| DE3922673A1 (de) * | 1989-07-10 | 1991-01-24 | Siemens Ag | Hochtemperaturbrennstoffzelle |
| US5132253A (en) * | 1990-12-17 | 1992-07-21 | Corning Incorporated | Sol-gel method for making ceramic materials |
| JPH0927330A (ja) * | 1995-07-11 | 1997-01-28 | Tokyo Gas Co Ltd | 固体電解質燃料電池の燃料極 |
| JP2000243405A (ja) * | 1999-02-23 | 2000-09-08 | Fuji Electric Corp Res & Dev Ltd | 固体電解質型燃料電池の製造方法 |
| JP2002289248A (ja) * | 2001-01-17 | 2002-10-04 | Nissan Motor Co Ltd | 燃料電池用単セル及び固体電解質型燃料電池 |
| US6677070B2 (en) * | 2001-04-19 | 2004-01-13 | Hewlett-Packard Development Company, L.P. | Hybrid thin film/thick film solid oxide fuel cell and method of manufacturing the same |
| US6803138B2 (en) * | 2001-07-02 | 2004-10-12 | Nextech Materials, Ltd. | Ceramic electrolyte coating methods |
| JP2003068321A (ja) * | 2001-08-27 | 2003-03-07 | Toyota Motor Corp | 燃料電池セルとその製造方法 |
| JP2003132906A (ja) * | 2001-10-24 | 2003-05-09 | Nissan Motor Co Ltd | 燃料電池用単セル及び固体電解質型燃料電池 |
| JP2005531885A (ja) * | 2002-04-23 | 2005-10-20 | フラウンホフェル−ゲゼルシャフト ツ−ル フォルダルング デル アンゲバンドテン フォルシュング エー.ファウ. | ナノ多孔性薄層電極と構造化電解質との複合物を含んでなる高温固体電解質燃料電池 |
| US7351492B2 (en) * | 2002-05-22 | 2008-04-01 | Nippon Shokubai Co., Ltd. | Solid oxide type fuel cell-use electrode support substrate and production method therefor |
| US20040214070A1 (en) * | 2003-04-28 | 2004-10-28 | Simner Steven P. | Low sintering lanthanum ferrite materials for use as solid oxide fuel cell cathodes and oxygen reduction electrodes and other electrochemical devices |
| RU2236722C1 (ru) * | 2003-06-10 | 2004-09-20 | Мятиев Ата Атаевич | Электрод-электролитная пара на основе двуокиси церия (варианты), способ ее изготовления (варианты) и органогель |
| US7157165B2 (en) * | 2003-11-18 | 2007-01-02 | Uchicago Argonne, Llc | Iron-based perovskite cathodes for solid oxide fuel cells |
| US8435694B2 (en) * | 2004-01-12 | 2013-05-07 | Fuelcell Energy, Inc. | Molten carbonate fuel cell cathode with mixed oxide coating |
| US20050238796A1 (en) * | 2004-04-22 | 2005-10-27 | Armstong Tad J | Method of fabricating composite cathodes for solid oxide fuel cells by infiltration |
| US20080057356A1 (en) * | 2004-05-17 | 2008-03-06 | Masatoshi Shimomura | Anode Support Substrate For Solid Oxide Fuel Cell And Process For Producing The Same |
| US8580453B2 (en) * | 2006-03-31 | 2013-11-12 | General Electric Company | Electrode-supported ceramic fuel cell containing laminar composite electrode including porous support electrode, patterned structure layer and electrolyte |
-
2008
- 2008-05-28 US US12/128,080 patent/US20090297923A1/en not_active Abandoned
-
2009
- 2009-05-14 JP JP2011511601A patent/JP5465240B2/ja not_active Expired - Fee Related
- 2009-05-14 WO PCT/US2009/003001 patent/WO2009151528A1/en not_active Ceased
- 2009-05-14 CN CN200980120119XA patent/CN102047477A/zh active Pending
- 2009-05-14 EP EP09762825A patent/EP2294645A1/en not_active Withdrawn
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP5978448B2 (ja) | 固体酸化物燃料電池または固体酸化物燃料電池サブコンポーネントおよびその製造方法 | |
| CN103183513B (zh) | 一种质子导电陶瓷电解质薄膜的制备方法 | |
| CN102510846A (zh) | 具有减小的厚度并含有金属氧化物的自支撑陶瓷材料的制造 | |
| CN108370041A (zh) | 质子导体、电池结构体、质子导体和电池结构体的制造方法、燃料电池以及水电解装置 | |
| JP2009091232A (ja) | 重合された無機−有機前駆物質溶液および焼結膜 | |
| CN102503419B (zh) | 一种ysz基复合热障涂层材料及其制备方法 | |
| JP5214907B2 (ja) | 固体電解質膜およびその製造方法 | |
| JP2011524946A (ja) | センサー、酸素分離装置、および固体酸化物燃料電池のためのゾルゲル由来の高性能触媒薄膜 | |
| JP2014516461A (ja) | 電気化学半電池の調製方法 | |
| CN102842722A (zh) | 固体氧化物燃料电池用材料、阴极和固体氧化物燃料电池 | |
| KR101662211B1 (ko) | 연료극, 연료극 지지형 전해질막, 연료전지 및 연료극 지지형 전해질막의 제조방법 | |
| CN111205079B (zh) | 一种镧掺杂钇铝石榴石陶瓷及其制备方法 | |
| JP3661676B2 (ja) | 固体電解質型燃料電池 | |
| CN106463749B (zh) | 致密度改进的无机电解质膜制造方法、制造该膜的组合物及使用该组合物制造的膜 | |
| JP6031308B2 (ja) | 固体酸化物形燃料電池用電解質支持型セル、並びに、それに用いられる電解質シート及びそれを備えた固体酸化物形燃料電池 | |
| CN108947529A (zh) | 一种非金属离子掺杂的钨酸镧型混合质子-电子导体透氢材料及其制备方法与应用 | |
| CN109382113B (zh) | 一种钙钛矿型氧化物催化剂、其制备方法与应用 | |
| KR20180017718A (ko) | 고체산화물 연료전지용 코어-쉘 구조의 복합 분말 | |
| KR20180018231A (ko) | 고체산화물 연료전지용 코어-쉘 구조의 복합 분말의 제조 방법 | |
| CN113121227A (zh) | 一种钆镍共掺杂镁基六铝酸镧陶瓷及制备方法 | |
| JP6561454B2 (ja) | 固体酸化物燃料電池用電解質の製造方法 | |
| CN103137979A (zh) | 中温固体氧化物燃料电池复合阴极及其制备方法 | |
| JP2016069237A (ja) | スカンジア安定化ジルコニア膜の製造方法およびスカンジア安定化ジルコニア膜 | |
| CN103708547A (zh) | 一种利用掺杂晶型诱导剂制备室温稳定四方相ZrO2纳米粉体的方法 | |
| JPH04170363A (ja) | 多結晶焼結体固体電解質 |