JP2011089002A - 冶金用コークスの製造方法 - Google Patents
冶金用コークスの製造方法 Download PDFInfo
- Publication number
- JP2011089002A JP2011089002A JP2009242933A JP2009242933A JP2011089002A JP 2011089002 A JP2011089002 A JP 2011089002A JP 2009242933 A JP2009242933 A JP 2009242933A JP 2009242933 A JP2009242933 A JP 2009242933A JP 2011089002 A JP2011089002 A JP 2011089002A
- Authority
- JP
- Japan
- Prior art keywords
- coal
- coke
- strength
- yield stress
- parameter
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
【解決手段】複数種類の石炭を配合した配合炭を乾留してコークスを製造する際に、前記各石炭の石炭化度パラメータと粘結性パラメータとを用いて製造されるコークスの強度を推定し、該推定した強度が所定範囲内となるように前記石炭を配合する冶金用コークスの製造方法であって、前記粘結性パラメータとして石炭の軟化溶融状態の降伏応力を用いることを特徴とする冶金用コークスの製造方法を用いる。配合炭の降伏応力の値が40〜150Paとなるように石炭を配合することが好ましい。
【選択図】図3
Description
(1)複数種類の石炭を配合した配合炭を乾留してコークスを製造する際に、前記各石炭の石炭化度パラメータと粘結性パラメータとを用いて製造されるコークスの強度を推定し、該推定した強度が所定範囲内となるように前記石炭を配合する冶金用コークスの製造方法であって、前記粘結性パラメータとして石炭の軟化溶融状態の降伏応力を用いることを特徴とする冶金用コークスの製造方法。
(2)配合炭の降伏応力の値が40〜150Paとなるように石炭を配合することを特徴とする(1)に記載の冶金用コークスの製造方法。
Claims (2)
- 複数種類の石炭を配合した配合炭を乾留してコークスを製造する際に、前記各石炭の石炭化度パラメータと粘結性パラメータとを用いて製造されるコークスの強度を推定し、該推定した強度が所定範囲内となるように前記石炭を配合する冶金用コークスの製造方法であって、前記粘結性パラメータとして石炭の軟化溶融状態の降伏応力を用いることを特徴とする冶金用コークスの製造方法。
- 配合炭の降伏応力の値が40〜150Paとなるように石炭を配合することを特徴とする請求項1に記載の冶金用コークスの製造方法。