JP2009030153A5 - - Google Patents
Download PDFInfo
- Publication number
- JP2009030153A5 JP2009030153A5 JP2008010557A JP2008010557A JP2009030153A5 JP 2009030153 A5 JP2009030153 A5 JP 2009030153A5 JP 2008010557 A JP2008010557 A JP 2008010557A JP 2008010557 A JP2008010557 A JP 2008010557A JP 2009030153 A5 JP2009030153 A5 JP 2009030153A5
- Authority
- JP
- Japan
- Prior art keywords
- less
- high alloy
- tube
- mass
- content
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Description
(1) 質量%で、C:0.03%以下、Si:1.0%以下、Mn:0.05〜1.5%、P:0.03%以下、S:0.03%以下、Ni:22%を超えて40%以下、Cr:20〜30%、Mo:0.01%以上4.0%未満、Cu:0.1〜4.0%、Al:0.001〜0.30%、N:0.05%を超えて0.30%以下、O:0.010%以下を含有し、残部がFeおよび不純物であり、かつ、N含有量とO含有量の積が下記(1)式を満足する化学組成を有する高合金素管を熱間加工により形成した後、冷間加工によって高合金管を製造する方法であって、最終の冷間加工工程を断面減少率での加工度Rdが下記(2)式を満足する条件で冷間加工することを特徴とする高合金管の製造方法。
N×O≦0.001 ・・・・・・(1)
15≦Rd(%)≦370×(C+N) ・・・・(2)
但し、式中のN、O及びCはそれぞれの元素の含有量(質量%)を意味し、そして、Rdは断面減少率での加工度(%)を意味する。
N×O≦0.001 ・・・・・・(1)
15≦Rd(%)≦370×(C+N) ・・・・(2)
但し、式中のN、O及びCはそれぞれの元素の含有量(質量%)を意味し、そして、Rdは断面減少率での加工度(%)を意味する。
Claims (2)
- 質量%で、C:0.03%以下、Si:1.0%以下、Mn:0.05〜1.5%、P:0.03%以下、S:0.03%以下、Ni:22%を超えて40%以下、Cr:20〜30%、Mo:0.01%以上4.0%未満、Cu:0.1〜4.0%、Al:0.001〜0.30%、N:0.05%を超えて0.30%以下、O:0.010%以下を含有し、残部がFeおよび不純物であり、かつ、N含有量とO含有量の積が下記(1)式を満足する化学組成を有する高合金素管を熱間加工により形成した後、冷間加工によって高合金管を製造する方法であって、最終の冷間加工工程を断面減少率での加工度Rdが下記(2)式を満足する条件で冷間加工することを特徴とする高合金管の製造方法。
N×O≦0.001 ・・・・・・(1)
15≦Rd(%)≦370×(C+N) ・・・・(2)
但し、式中のN、O及びCはそれぞれの元素の含有量(質量%)を意味し、そして、Rdは断面減少率での加工度(%)を意味する。 - 高合金素管の化学組成が、Feの一部に代えて、質量%で、Ca:0.01%以下、Mg:0.01%以下および希土類元素:0.2%以下のうちの1種または2種以上を含有することを特徴とする、請求項1に記載の高合金管の製造方法。