DE523161C - Anoden fuer galvanische Vernicklungsbaeder - Google Patents
Anoden fuer galvanische VernicklungsbaederInfo
- Publication number
- DE523161C DE523161C DE1930523161D DE523161DD DE523161C DE 523161 C DE523161 C DE 523161C DE 1930523161 D DE1930523161 D DE 1930523161D DE 523161D D DE523161D D DE 523161DD DE 523161 C DE523161 C DE 523161C
- Authority
- DE
- Germany
- Prior art keywords
- anodes
- nickel
- plating baths
- galvanic nickel
- galvanic
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
- Anoden für galvanische Vernicklungsbäder Es ist bekannt, Anoden für galvanische Vernicklungsbäder aus Nickel, das durch Zersetzung von Nickelcarbonvl erhalten wird, herzustellen. Diese Anoden werden in der Weise hergestellt, daß das Nickel gegossen oder gewalzt wird. Sie haben den Nachteil, daß bei ihrer Herstellung mit besonderer Vorsicht verfahren werden muß, damit sie eine geeignete gleichmäßige Struktur erhalten. Außerdem sind sie mit einer Guß- oder Walzhaut behaftet, welche vor ihrer Verwendung entfernt werden muß. Auch die im Mondprozeß anfallenden schrotförmigen Gebilde sind schon, in ein durchlöchertes Gefäß eingefüllt, direkt als Anode benutzt worden.
- Es wurde nun gefunden, daß man besonders vorteilhaft verwendbare Anoden erhalten kann, wenn man Nickelcarbonyl derart zersetzt, daß das Nickel in äußerst fein verteilter Pulverform erhalten wird und anschließend das erhaltene Pulver bei höherer Temperatur zusammensintert, zweckmäßig zu einer zusammenhängenden Platte. Die Sinterung kann z. B. in einer Wasserstoffatmosphäre vorgenommen werden, .wobei dann gleichzeitig eine weitgehende Entfernung von etwaigen kleinen Verunreinigungen stattfindet. Die durch die Sinterung bedingte besondere Struktur gibt den Anoden, im Vergleich zu den bisher bekannten Anoden, eine viel größere Oberfläche. Infolge ihrer großen wirksamen Oberfläche und der infolge ihrer Sinterung bei hoher Temperatur an sich leicht löslichen Form des Nickels besitzen die Anoden eine besonders große anodische Löslichkeit; deshalb ist es bei ihrer Verwendung meistens zweckmäßig, Chloridzusätze in den Bädern zu vermeiden und nur die besonders vorteilhaft arbeitenden Bäder mit schwefelsauren Salzen zu verwenden. Die mit solchen Nickelanoden betriebenen Bäder ergeben besonders schöne Nickelniederschläge und erfordern wenig Wartung.
Claims (1)
- PATENTANSPRUCH: Anoden für galvanische Vernicklungsbäder, dadurch gekennzeichnet, daß sie aus zusammengesintertem Nickelpulver, zweckmäßig durch Zersetzung von Nickelcarbonvl erhalten, bestehen.