JPS62290823A - 密着性に優れた表面被膜をそなえる超低鉄損一方向性けい素鋼板の製造方法 - Google Patents

密着性に優れた表面被膜をそなえる超低鉄損一方向性けい素鋼板の製造方法

Info

Publication number
JPS62290823A
JPS62290823A JP13108186A JP13108186A JPS62290823A JP S62290823 A JPS62290823 A JP S62290823A JP 13108186 A JP13108186 A JP 13108186A JP 13108186 A JP13108186 A JP 13108186A JP S62290823 A JPS62290823 A JP S62290823A
Authority
JP
Japan
Prior art keywords
steel sheet
silicon steel
annealing
ion plating
mirror
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP13108186A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0327632B2 (enrdf_load_stackoverflow
Inventor
Masao Iguchi
征夫 井口
Kazuhiro Suzuki
一弘 鈴木
Yasuhiro Kobayashi
康宏 小林
Ujihiro Nishiike
西池 氏裕
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JFE Steel Corp
Original Assignee
Kawasaki Steel Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kawasaki Steel Corp filed Critical Kawasaki Steel Corp
Priority to JP13108186A priority Critical patent/JPS62290823A/ja
Publication of JPS62290823A publication Critical patent/JPS62290823A/ja
Publication of JPH0327632B2 publication Critical patent/JPH0327632B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Chemical Treatment Of Metals (AREA)
  • Physical Vapour Deposition (AREA)
  • Manufacturing Of Steel Electrode Plates (AREA)
JP13108186A 1986-06-07 1986-06-07 密着性に優れた表面被膜をそなえる超低鉄損一方向性けい素鋼板の製造方法 Granted JPS62290823A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP13108186A JPS62290823A (ja) 1986-06-07 1986-06-07 密着性に優れた表面被膜をそなえる超低鉄損一方向性けい素鋼板の製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP13108186A JPS62290823A (ja) 1986-06-07 1986-06-07 密着性に優れた表面被膜をそなえる超低鉄損一方向性けい素鋼板の製造方法

Publications (2)

Publication Number Publication Date
JPS62290823A true JPS62290823A (ja) 1987-12-17
JPH0327632B2 JPH0327632B2 (enrdf_load_stackoverflow) 1991-04-16

Family

ID=15049544

Family Applications (1)

Application Number Title Priority Date Filing Date
JP13108186A Granted JPS62290823A (ja) 1986-06-07 1986-06-07 密着性に優れた表面被膜をそなえる超低鉄損一方向性けい素鋼板の製造方法

Country Status (1)

Country Link
JP (1) JPS62290823A (enrdf_load_stackoverflow)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2012035302A (ja) * 2010-08-06 2012-02-23 Jfe Steel Corp 電子ビーム照射装置

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2012035302A (ja) * 2010-08-06 2012-02-23 Jfe Steel Corp 電子ビーム照射装置

Also Published As

Publication number Publication date
JPH0327632B2 (enrdf_load_stackoverflow) 1991-04-16

Similar Documents

Publication Publication Date Title
WO1986002950A1 (en) Method of manufacturing unidirectional electromagnetic steel plates of low iron loss
JPH0672266B2 (ja) 超低鉄損一方向性珪素鋼板の製造方法
JP2653638B2 (ja) 鉄損の低い方向性電磁鋼板の製造方法
JPS61235514A (ja) 熱安定性、超低鉄損一方向性珪素鋼板の製造方法
JPS621821A (ja) ひずみ取り焼鈍を施しても特性劣化のない超低鉄損一方向性珪素鋼板の製造方法
JPS637333A (ja) グラス皮膜特性のすぐれた低鉄損方向性電磁鋼板の製造方法
JPS62290823A (ja) 密着性に優れた表面被膜をそなえる超低鉄損一方向性けい素鋼板の製造方法
JPS61201732A (ja) 熱安定性、超低鉄損一方向性珪素鋼板の製造方法
JP3148092B2 (ja) 鉄損の低い鏡面方向性電磁鋼板の製造方法
JP3148093B2 (ja) 鉄損の低い鏡面方向性電磁鋼板の製造方法
JPS63227719A (ja) 超低鉄損一方向性珪素鋼板の製造方法
JPS621822A (ja) 熱安定性、超低鉄損一方向性珪素鋼板の製造方法
JPS62192581A (ja) 超低鉄損一方向性けい素鋼板の製造方法
JPH01159322A (ja) 超低鉄損一方向性珪素鋼板の製造方法
JPH0699823B2 (ja) 超低鉄損一方向性珪素鋼板の製造方法
JPS6230302A (ja) 超低鉄損一方向性けい素鋼板の製造方法
JPS6318087A (ja) 低鉄損一方向性けい素鋼板の製造方法
JPH0335377B2 (enrdf_load_stackoverflow)
JPS6229107A (ja) 超低鉄損一方向性珪素鋼板の製造方法
JPH0327633B2 (enrdf_load_stackoverflow)
JPH01198430A (ja) 極めて鉄損が優れ、被膜密着性の優れた方向性電磁鋼板の製造方法
JPS61246321A (ja) 超低鉄損一方向性珪素鋼板の製造方法
JPS6263408A (ja) 超低鉄損一方向性けい素鋼板の製造方法
JPS6324017A (ja) 低鉄損一方向性けい素鋼板の製造方法
JPS6222409A (ja) 超低鉄損一方向性珪素鋼板の製造方法