JPH0566401B2 - - Google Patents
Info
- Publication number
- JPH0566401B2 JPH0566401B2 JP60139143A JP13914385A JPH0566401B2 JP H0566401 B2 JPH0566401 B2 JP H0566401B2 JP 60139143 A JP60139143 A JP 60139143A JP 13914385 A JP13914385 A JP 13914385A JP H0566401 B2 JPH0566401 B2 JP H0566401B2
- Authority
- JP
- Japan
- Prior art keywords
- hydrocarbon resin
- weight
- bromine number
- copolymer
- hydrocarbon
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP13914385A JPS62506A (ja) | 1985-06-27 | 1985-06-27 | 炭化水素樹脂の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP13914385A JPS62506A (ja) | 1985-06-27 | 1985-06-27 | 炭化水素樹脂の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS62506A JPS62506A (ja) | 1987-01-06 |
| JPH0566401B2 true JPH0566401B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | 1993-09-21 |
Family
ID=15238559
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP13914385A Granted JPS62506A (ja) | 1985-06-27 | 1985-06-27 | 炭化水素樹脂の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS62506A (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) |
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN104945560A (zh) * | 2015-06-29 | 2015-09-30 | 安徽同心化工有限公司 | 一种加氢的苯乙烯改性双环戊二烯石油树脂及其制备方法 |
Families Citing this family (6)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP2599406B2 (ja) * | 1987-12-21 | 1997-04-09 | 荒川化学工業株式会社 | 石油樹脂の水素化脱色方法 |
| JPH0289432U (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) * | 1988-12-27 | 1990-07-16 | ||
| US5171793A (en) * | 1990-02-22 | 1992-12-15 | Exxon Chemical Patents Inc. | Hydrogenated resins, adhesive formulations and process for production of resins |
| WO1994002521A1 (en) * | 1992-07-28 | 1994-02-03 | Nippon Zeon Co., Ltd. | Hydrogenated resin |
| WO2004003041A1 (ja) * | 2002-06-26 | 2004-01-08 | Idemitsu Kosan Co., Ltd. | 高軟化点共重合体、その製造方法及びその水素添加物 |
| WO2007148530A1 (ja) * | 2006-06-22 | 2007-12-27 | Kansai Paint Co., Ltd. | 粉体塗料、粉体塗料の製造方法、及び粉体塗料を用いた塗膜形成方法 |
Family Cites Families (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS52140591A (en) * | 1976-05-20 | 1977-11-24 | Nippon Zeon Co Ltd | Novel hydrogenated hydrocarbon resisn |
| JPS6128508A (ja) * | 1984-07-18 | 1986-02-08 | Mitsui Petrochem Ind Ltd | 新規炭化水素樹脂およびそれを用いた接着剤用添加剤 |
-
1985
- 1985-06-27 JP JP13914385A patent/JPS62506A/ja active Granted
Cited By (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CN104945560A (zh) * | 2015-06-29 | 2015-09-30 | 安徽同心化工有限公司 | 一种加氢的苯乙烯改性双环戊二烯石油树脂及其制备方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPS62506A (ja) | 1987-01-06 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| DE69403775T2 (de) | Blockcopolymer mit Endblöcken verschiedenen Molekulargewichts | |
| US4780367A (en) | Tackified star block copolymer pressure-sensitive adhesive composition and the sheet materials coated therewith | |
| US3554940A (en) | Pressure-sensitive adhesives | |
| US7385018B2 (en) | Hydrogenated copolymer, process for producing the same, and hot-melt adhesive composition containing the same | |
| JP2000103820A (ja) | 水素化c9系石油樹脂の製造方法および当該製造方法により得られた水素化c9系石油樹脂 | |
| JP2977942B2 (ja) | 粘着付与剤樹脂およびその製造方法 | |
| US20060063892A1 (en) | Method for producing petroleum resin and hydrogenated petroleum resin | |
| KR100366972B1 (ko) | 점·접착제용 공중합 석유수지 및 그의 제조방법 | |
| EP0240762A1 (en) | Vinyl aromatic/terpene/phenol/terpolymers | |
| JPH0566401B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) | ||
| JP3173841B2 (ja) | 水添石油樹脂 | |
| JPH06184249A (ja) | ホットメルト接着剤組成物 | |
| JP3387612B2 (ja) | ブロック共重合体組成物および粘着剤組成物 | |
| JPH03259981A (ja) | ホットメルト接着剤組成物 | |
| JPH08157794A (ja) | スチレン−共役ジエン系ブロック共重合体用粘着付与剤および粘着剤組成物 | |
| JP3427912B2 (ja) | スチレン−共役ジエン系ブロック共重合体用粘着付与剤、その製造方法および粘着剤組成物 | |
| JPH01213380A (ja) | 粘着剤組成物 | |
| JPH0625212B2 (ja) | 水素化炭化水素樹脂の製造方法 | |
| JPS608379A (ja) | 感圧接着組成物とそれを用いた被覆シ−ト材料 | |
| JPH0651740B2 (ja) | 粘接着特性の優れた水添石油樹脂の製造方法 | |
| JPS588432B2 (ja) | セツチヤクザイソセイブツ | |
| JPH02153987A (ja) | 粘着剤組成物 | |
| JP3339171B2 (ja) | ブロック共重合体の製造方法 | |
| JPS6128508A (ja) | 新規炭化水素樹脂およびそれを用いた接着剤用添加剤 | |
| JPH02160886A (ja) | ホットメルト粘着剤組成物 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| S111 | Request for change of ownership or part of ownership |
Free format text: JAPANESE INTERMEDIATE CODE: R313111 |
|
| R350 | Written notification of registration of transfer |
Free format text: JAPANESE INTERMEDIATE CODE: R350 |
|
| EXPY | Cancellation because of completion of term |