JP2014175261A - 焼結体、及び、その製造方法 - Google Patents
焼結体、及び、その製造方法 Download PDFInfo
- Publication number
- JP2014175261A JP2014175261A JP2013049582A JP2013049582A JP2014175261A JP 2014175261 A JP2014175261 A JP 2014175261A JP 2013049582 A JP2013049582 A JP 2013049582A JP 2013049582 A JP2013049582 A JP 2013049582A JP 2014175261 A JP2014175261 A JP 2014175261A
- Authority
- JP
- Japan
- Prior art keywords
- silicon
- copper
- sintered body
- powder
- carbon
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
【解決手段】シリコン粉末に銅粉末を混合し、加圧すると共に加熱して、シリコン粒子10の周囲にポーラス構造を有する銅(12)による導電性ネットワークを形成する。又は、シリコン粉末にカーボンファイバー32、チューブ、フラーレン、グラファイト又は炭素系微粒子を混合し、焼結して、気孔15を持つポーラス構造の導電性ネットワークを形成する。
【選択図】図1
Description
I(z)=I0exp(−αz) ・・・(1)
ここで、I0、αは、それぞれ材料表面での強度及び材料の吸収係数である。
12…銅粒子
13…銅バインダー
14、38…混合粉末
15…気孔
16…シリコンウエハ
20…プレス機
22…赤外線ランプ
23…赤外線
32…カーボンナノファイバー(CNF)
34…銅基板
36…ガラス板
40…高出力パルスレーザ
42…レーザ
44…複合膜
50…リニアステージ
Claims (7)
- シリコン粒子と、その周囲のポーラス構造を有する銅からなり、前記銅が導電性ネットワークを形成していることを特徴とする焼結体。
- 前記銅がバインダーとして存在することを特徴とする請求項1に記載の焼結体。
- シリコン粉末に銅粉末を混合し、加圧すると共に加熱して、シリコン粒子の周囲にポーラス構造を有する銅による導電性ネットワークを形成することを特徴とする焼結体の製造方法。
- 前記加圧をプレス成形により行い、前記加熱を赤外線により行うことを特徴とする請求項3に記載の焼結体の製造方法。
- シリコン粒子とその周囲の炭素系厚膜からなり、該炭素系厚膜が気孔を持つポーラス構造で導電性ネットワークを形成していることを特徴とする焼結体。
- シリコン粉末にカーボンファイバー、チューブ、フラーレン、グラファイト又は炭素系微粒子を混合し、焼結して、気孔を持つポーラス構造の導電性ネットワークが形成されたことを特徴とする焼結体の製造方法。
- 前記焼結をレーザ照射により行うことを特徴とする請求項6に記載の焼結体の製造方法。