JP2008308422A - 重合防止方法 - Google Patents
重合防止方法 Download PDFInfo
- Publication number
- JP2008308422A JP2008308422A JP2007156644A JP2007156644A JP2008308422A JP 2008308422 A JP2008308422 A JP 2008308422A JP 2007156644 A JP2007156644 A JP 2007156644A JP 2007156644 A JP2007156644 A JP 2007156644A JP 2008308422 A JP2008308422 A JP 2008308422A
- Authority
- JP
- Japan
- Prior art keywords
- copper salt
- solution
- acrylic acid
- polymerization
- meth
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
【解決手段】 ジアルキルジチオカルバミン酸銅塩溶液中の硫酸銅含量を100ppm(質量)以下にして供給する。
【選択図】 なし
Description
(実施例1)
プロピレンを分子状酸素含有ガスにより接触気相酸化して得た混合ガスをアクリル酸捕集塔に導いて水と接触させて得た水溶液をアクロレイン放散塔に導いてアクロレインを放散させ、アクリル酸65質量%、水30質量%、酢酸3.0質量%を含むアクリル酸水溶液を得た。段数60段、段間隔147mmのシーブトレーを備え、塔頂部に留出管、中央部に原料供給管、塔底部に塔底液抜き出し管を備えた共沸分離塔を用い、共沸溶剤としてトルエンを用いて、このアクリル酸水溶液の共沸蒸留運転を行った。
(実施例2)
実施例1において、8質量%のジブチルジチオカルバミン酸銅塩溶液を用いた以外は実施例1と同様にしてアクリル酸水溶液の共沸蒸留運転を行った。なお、ジブチルジチオカルバミン酸銅塩溶液には硫酸銅が80ppm(質量)含まれていた。
(比較例1)
実施例1において、12質量%のジブチルジチオカルバミン酸銅塩溶液を用いた以外は実施例1と同様にしてアクリル酸水溶液の共沸蒸留運転を行った。なお、ジブチルジチオカルバミン酸銅塩溶液には硫酸銅が120ppm(質量)含まれていた。
Claims (3)
- 有機溶媒にジアルキルジチオカルバミン酸銅塩を溶解した溶液を用いて(メタ)アクリル酸および/またはそのエステルの重合を防止するにあたり、該ジアルキルジチオカルバミン酸銅塩溶液中の硫酸銅含量を100ppm(質量)以下にすることを特徴とする(メタ)アクリル酸および/またはそのエステルの重合防止方法。
- ジアルキルジチオカルバミン酸銅塩溶液中のジアルキルジチオカルバミン酸銅塩の濃度が0.1〜10質量%である請求項1記載の重合防止方法。
- ジアルキルジチオカルバミン酸銅塩がジメチルジチオカルバミン酸銅塩、ジエチルジチオカルバミン酸銅塩、ジプロピルジチオカルバミン酸銅塩およびジブチルジチオカルバミン酸銅塩から選ばれる少なくとも1種である請求項1または2記載の重合防止方法。