DK1252682T3 - Fremgangsmåde til fremstilling af en indretning omfattende en anodebåret elektrolyt, og en keramisk celle omfattende denne indretning - Google Patents
Fremgangsmåde til fremstilling af en indretning omfattende en anodebåret elektrolyt, og en keramisk celle omfattende denne indretningInfo
- Publication number
- DK1252682T3 DK1252682T3 DK01908443T DK01908443T DK1252682T3 DK 1252682 T3 DK1252682 T3 DK 1252682T3 DK 01908443 T DK01908443 T DK 01908443T DK 01908443 T DK01908443 T DK 01908443T DK 1252682 T3 DK1252682 T3 DK 1252682T3
- Authority
- DK
- Denmark
- Prior art keywords
- layer
- electrolyte
- support
- producing
- zirconia
- Prior art date
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M8/00—Fuel cells; Manufacture thereof
- H01M8/02—Details
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/86—Inert electrodes with catalytic activity, e.g. for fuel cells
- H01M4/90—Selection of catalytic material
- H01M4/9041—Metals or alloys
- H01M4/905—Metals or alloys specially used in fuel cell operating at high temperature, e.g. SOFC
- H01M4/9066—Metals or alloys specially used in fuel cell operating at high temperature, e.g. SOFC of metal-ceramic composites or mixtures, e.g. cermets
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/86—Inert electrodes with catalytic activity, e.g. for fuel cells
- H01M4/88—Processes of manufacture
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M8/00—Fuel cells; Manufacture thereof
- H01M8/06—Combination of fuel cells with means for production of reactants or for treatment of residues
- H01M8/0606—Combination of fuel cells with means for production of reactants or for treatment of residues with means for production of gaseous reactants
- H01M8/0612—Combination of fuel cells with means for production of reactants or for treatment of residues with means for production of gaseous reactants from carbon-containing material
- H01M8/0625—Combination of fuel cells with means for production of reactants or for treatment of residues with means for production of gaseous reactants from carbon-containing material in a modular combined reactor/fuel cell structure
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M8/00—Fuel cells; Manufacture thereof
- H01M8/10—Fuel cells with solid electrolytes
- H01M8/12—Fuel cells with solid electrolytes operating at high temperature, e.g. with stabilised ZrO2 electrolyte
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M8/00—Fuel cells; Manufacture thereof
- H01M8/10—Fuel cells with solid electrolytes
- H01M8/12—Fuel cells with solid electrolytes operating at high temperature, e.g. with stabilised ZrO2 electrolyte
- H01M8/1231—Fuel cells with solid electrolytes operating at high temperature, e.g. with stabilised ZrO2 electrolyte with both reactants being gaseous or vaporised
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M2300/00—Electrolytes
- H01M2300/0088—Composites
- H01M2300/0094—Composites in the form of layered products, e.g. coatings
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/30—Hydrogen technology
- Y02E60/50—Fuel cells
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Chemical Kinetics & Catalysis (AREA)
- General Chemical & Material Sciences (AREA)
- Electrochemistry (AREA)
- Manufacturing & Machinery (AREA)
- Life Sciences & Earth Sciences (AREA)
- Sustainable Development (AREA)
- Sustainable Energy (AREA)
- Materials Engineering (AREA)
- Composite Materials (AREA)
- Ceramic Engineering (AREA)
- Inert Electrodes (AREA)
- Fuel Cell (AREA)
- Compositions Of Oxide Ceramics (AREA)
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
NL1014284A NL1014284C2 (nl) | 2000-02-04 | 2000-02-04 | Werkwijze voor het vervaardigen van een samenstel omvattende een anodegedragen elektrolyt alsmede keramische cel omvattende een dergelijk samenstel. |
Publications (1)
Publication Number | Publication Date |
---|---|
DK1252682T3 true DK1252682T3 (da) | 2006-05-22 |
Family
ID=19770745
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
DK01908443T DK1252682T3 (da) | 2000-02-04 | 2001-02-05 | Fremgangsmåde til fremstilling af en indretning omfattende en anodebåret elektrolyt, og en keramisk celle omfattende denne indretning |
Country Status (12)
Country | Link |
---|---|
US (1) | US6663999B2 (de) |
EP (1) | EP1252682B1 (de) |
JP (1) | JP5101777B2 (de) |
KR (1) | KR100733801B1 (de) |
CN (1) | CN1256784C (de) |
AT (1) | ATE323950T1 (de) |
AU (1) | AU778854B2 (de) |
CA (1) | CA2398711C (de) |
DE (1) | DE60118884T2 (de) |
DK (1) | DK1252682T3 (de) |
NL (1) | NL1014284C2 (de) |
WO (1) | WO2001057945A1 (de) |
Families Citing this family (25)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US7638222B2 (en) * | 2001-03-28 | 2009-12-29 | Hexis Ag | Porous, gas permeable layer substructure for a thin, gas tight layer for use as a functional component in high temperature fuel cells |
JP3841149B2 (ja) * | 2001-05-01 | 2006-11-01 | 日産自動車株式会社 | 固体電解質型燃料電池用単セル |
EP1328035A1 (de) * | 2002-01-09 | 2003-07-16 | HTceramix S.A. - High Technology Electroceramics | PEN einer Festoxidbrennstoffzelle |
JP2004362849A (ja) * | 2003-06-03 | 2004-12-24 | Ngk Insulators Ltd | 電気化学セル用基板および電気化学セル |
EP1513214A1 (de) * | 2003-09-05 | 2005-03-09 | Sulzer Hexis AG | Hochtemperaturbrennstoffzelle mit stabilisierter Cermet-Struktur |
US7595085B2 (en) * | 2004-03-09 | 2009-09-29 | Delphi Technologies, Inc. | Ceramic assembly with a stabilizer layer |
JP2006164821A (ja) * | 2004-12-09 | 2006-06-22 | Toyota Motor Corp | 燃料電池 |
US6994884B1 (en) * | 2004-12-16 | 2006-02-07 | General Electric Company | High performance fuel cell electrode and method for manufacturing same |
US20060172141A1 (en) * | 2005-01-27 | 2006-08-03 | Xinyu Huang | Joints and methods of making and using |
WO2006079558A1 (en) * | 2005-01-31 | 2006-08-03 | Technical University Of Denmark | Redox-stable anode |
EP1760817B1 (de) | 2005-08-31 | 2013-08-21 | Technical University of Denmark | Reversible-festoxydbrennstoffzelle und dessen Herstellungsverfahren |
CN1320677C (zh) * | 2005-10-25 | 2007-06-06 | 哈尔滨工业大学 | 制备氧化钇稳定氧化锆电解质薄膜的方法 |
KR100660218B1 (ko) | 2005-12-23 | 2006-12-21 | 주식회사 포스코 | 고체산화물 연료전지용 음극재의 제조방법 |
US8580453B2 (en) * | 2006-03-31 | 2013-11-12 | General Electric Company | Electrode-supported ceramic fuel cell containing laminar composite electrode including porous support electrode, patterned structure layer and electrolyte |
US20070243451A1 (en) * | 2006-04-14 | 2007-10-18 | Chao-Yi Yuh | Anode support member and bipolar separator for use in a fuel cell assembly and for preventing poisoning of reforming catalyst |
EP1930974B1 (de) | 2006-11-23 | 2012-03-21 | Technical University of Denmark | Methode zur Herstellung von reversiblen Festoxid-Zellen |
KR100858423B1 (ko) * | 2007-07-24 | 2008-09-17 | 한국과학기술원 | 고체산화물 연료전지의 연료극 및 전해질 제조방법 |
JP2010192288A (ja) * | 2009-02-19 | 2010-09-02 | Honda Motor Co Ltd | 電解質・電極接合体及びその製造方法 |
JP5426488B2 (ja) * | 2010-06-24 | 2014-02-26 | 日本電信電話株式会社 | 固体酸化物形燃料電池用単セルの製造方法 |
KR101351221B1 (ko) * | 2011-09-21 | 2014-01-14 | 한국전력공사 | 테이프 캐스팅을 이용한 지지체식 코팅막의 제조방법 |
DE102012103383A1 (de) * | 2012-04-18 | 2013-10-24 | Deutsches Zentrum für Luft- und Raumfahrt e.V. | Verfahren zur Herstellung eines Trägersubstrats, Trägersubstrat und elektrochemische Einrichtung |
WO2013173981A1 (zh) * | 2012-05-22 | 2013-11-28 | Yang Shaohua | 一种阳极支撑固体氧化物燃料电池及其制备方法 |
GB201617494D0 (en) | 2016-10-14 | 2016-11-30 | Coorstek Membrane Sciences As | Process for the manufacture of a solide oxide membrane electrode assembly |
GB201617500D0 (en) | 2016-10-14 | 2016-11-30 | Coorstek Membrane Sciences As | Process |
US20180226659A1 (en) * | 2017-01-26 | 2018-08-09 | United States Department Of Energy | Fuel cell with thermal energy storage for flexibility in hybrids |
Family Cites Families (34)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JP2622261B2 (ja) * | 1987-10-05 | 1997-06-18 | 三菱重工業株式会社 | 固体電解質燃料電池の製作方法 |
JP2841528B2 (ja) * | 1989-08-24 | 1998-12-24 | 株式会社明電舎 | 固体電解質型燃料電池 |
US5106654A (en) * | 1990-07-20 | 1992-04-21 | Westinghouse Electric Corp. | Method of forming a dense, high temperature electronically conductive composite layer on a porous ceramic substrate |
JPH053037A (ja) * | 1990-10-03 | 1993-01-08 | Fuji Electric Co Ltd | 固体電解質型燃料電池 |
JPH05114405A (ja) * | 1991-10-21 | 1993-05-07 | Kyocera Corp | 電極材料膜生成方法および電極材料膜生成装置 |
JP3064087B2 (ja) * | 1992-03-05 | 2000-07-12 | 三菱重工業株式会社 | 固体電解質セルの製造法 |
JPH06135721A (ja) * | 1992-10-28 | 1994-05-17 | Seibu Gas Kk | 固体電解質燃料電池のインターコネクター材料及びその合成方法並びに上記材料を用いて円筒型固体電解質燃料電池の燃料極ににインターコネクターを形成する方法 |
JP2826243B2 (ja) * | 1992-12-01 | 1998-11-18 | 日本電信電話株式会社 | 固体電解質型燃料電池およびその製造方法 |
NL9202087A (nl) * | 1992-12-01 | 1994-07-01 | Stichting Energie | Werkwijze voor het aanbrengen van een cermet electrodelaag op een gesinterd elektroliet. |
JP2848551B2 (ja) * | 1993-03-29 | 1999-01-20 | 日本電信電話株式会社 | 固体電解質型燃料電池の電解質膜製造方法 |
DE4314323C2 (de) * | 1993-04-30 | 1998-01-22 | Siemens Ag | Hochtemperaturbrennstoffzelle mit verbesserter Festelektrolyt/Elektroden-Grenzfläche und Verfahren zur Herstellung eines Mehrschichtaufbaus mit verbesserter Festelektrolyt/Elektroden-Grenzfläche |
JPH06349503A (ja) * | 1993-06-07 | 1994-12-22 | Mitsubishi Heavy Ind Ltd | 固体電解質型電解セル |
US5445903A (en) * | 1993-09-09 | 1995-08-29 | Technology Management, Inc. | Electrochemical apparatus |
JP3548772B2 (ja) * | 1994-03-15 | 2004-07-28 | 株式会社村田製作所 | 固体電解質型燃料電池 |
JP3434883B2 (ja) * | 1994-04-28 | 2003-08-11 | 京セラ株式会社 | 燃料電池セルの製造方法 |
JPH08138690A (ja) * | 1994-11-07 | 1996-05-31 | Tonen Corp | 固体電解質型燃料電池 |
JPH08185882A (ja) * | 1994-12-28 | 1996-07-16 | Mitsubishi Heavy Ind Ltd | 固体電解質型燃料電池の製造方法 |
JP3181206B2 (ja) * | 1995-09-05 | 2001-07-03 | 三菱重工業株式会社 | 固体電解質型電気化学セルの燃料極 |
JPH0992301A (ja) * | 1995-09-19 | 1997-04-04 | Mitsubishi Heavy Ind Ltd | 円筒横縞型固体電解質燃料電池 |
US5753385A (en) * | 1995-12-12 | 1998-05-19 | Regents Of The University Of California | Hybrid deposition of thin film solid oxide fuel cells and electrolyzers |
DE19547700C2 (de) | 1995-12-20 | 1998-09-17 | Forschungszentrum Juelich Gmbh | Elektrodensubstrat für eine Brennstoffzelle |
ATE191815T1 (de) * | 1996-02-02 | 2000-04-15 | Sulzer Hexis Ag | Hochtemperatur-brennstoffzelle mit einem dünnfilm-elektrolyten |
US5702837A (en) * | 1996-02-05 | 1997-12-30 | Alliedsignal Inc. | Bonding materials for anode to anode bonding and anode to interconnect bonding in solid oxide fuel cells |
JP3310867B2 (ja) * | 1996-06-21 | 2002-08-05 | 三菱重工業株式会社 | 円筒横縞型固体電解質燃料電池の製造方法 |
JPH10106608A (ja) * | 1996-10-02 | 1998-04-24 | Murata Mfg Co Ltd | 固体電解質型燃料電池及びその製造方法 |
JPH1173982A (ja) * | 1997-08-28 | 1999-03-16 | Toto Ltd | 固体電解質型燃料電池及びその製造方法 |
JPH1186885A (ja) * | 1997-09-03 | 1999-03-30 | Mitsubishi Heavy Ind Ltd | 固体電解質型燃料電池のセルおよびその製造方法 |
JP3478080B2 (ja) * | 1997-09-16 | 2003-12-10 | 株式会社村田製作所 | 固体電解質型燃料電池の製造方法 |
US5908713A (en) * | 1997-09-22 | 1999-06-01 | Siemens Westinghouse Power Corporation | Sintered electrode for solid oxide fuel cells |
JPH11111309A (ja) * | 1997-10-06 | 1999-04-23 | Mitsubishi Heavy Ind Ltd | 固体電解質燃料電池の製造方法 |
JP3677386B2 (ja) * | 1998-03-26 | 2005-07-27 | 京セラ株式会社 | 固体電解質型燃料電池セル |
DE19819453A1 (de) * | 1998-04-30 | 1999-11-11 | Forschungszentrum Juelich Gmbh | SOFC-Brennstoffzelle mit einer Anodenzwischenschicht |
US6228521B1 (en) * | 1998-12-08 | 2001-05-08 | The University Of Utah Research Foundation | High power density solid oxide fuel cell having a graded anode |
WO2000069008A1 (en) * | 1999-05-07 | 2000-11-16 | Forskningscenter Risø | Electrochemical cell |
-
2000
- 2000-02-04 NL NL1014284A patent/NL1014284C2/nl not_active IP Right Cessation
-
2001
- 2001-02-05 JP JP2001557103A patent/JP5101777B2/ja not_active Expired - Fee Related
- 2001-02-05 CN CNB018045537A patent/CN1256784C/zh not_active Expired - Fee Related
- 2001-02-05 CA CA002398711A patent/CA2398711C/en not_active Expired - Fee Related
- 2001-02-05 EP EP01908443A patent/EP1252682B1/de not_active Expired - Lifetime
- 2001-02-05 AT AT01908443T patent/ATE323950T1/de active
- 2001-02-05 DK DK01908443T patent/DK1252682T3/da active
- 2001-02-05 WO PCT/NL2001/000085 patent/WO2001057945A1/en active IP Right Grant
- 2001-02-05 US US10/203,003 patent/US6663999B2/en not_active Expired - Fee Related
- 2001-02-05 KR KR1020027010034A patent/KR100733801B1/ko not_active IP Right Cessation
- 2001-02-05 DE DE60118884T patent/DE60118884T2/de not_active Expired - Lifetime
- 2001-02-05 AU AU36186/01A patent/AU778854B2/en not_active Ceased
Also Published As
Publication number | Publication date |
---|---|
NL1014284C2 (nl) | 2001-08-13 |
CA2398711A1 (en) | 2001-08-09 |
CA2398711C (en) | 2009-11-03 |
DE60118884T2 (de) | 2006-11-16 |
KR100733801B1 (ko) | 2007-07-02 |
AU3618601A (en) | 2001-08-14 |
AU778854B2 (en) | 2004-12-23 |
EP1252682A1 (de) | 2002-10-30 |
CN1398439A (zh) | 2003-02-19 |
US20030012880A1 (en) | 2003-01-16 |
DE60118884D1 (de) | 2006-05-24 |
JP5101777B2 (ja) | 2012-12-19 |
US6663999B2 (en) | 2003-12-16 |
JP2003522384A (ja) | 2003-07-22 |
CN1256784C (zh) | 2006-05-17 |
WO2001057945A1 (en) | 2001-08-09 |
KR20020081297A (ko) | 2002-10-26 |
EP1252682B1 (de) | 2006-04-19 |
ATE323950T1 (de) | 2006-05-15 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
DK1252682T3 (da) | Fremgangsmåde til fremstilling af en indretning omfattende en anodebåret elektrolyt, og en keramisk celle omfattende denne indretning | |
DE60027192D1 (de) | Strukturen und herstellungsverfahren für festkörperelektrochemische vorrichtungen | |
WO2005057685A3 (en) | Anode-supported sofc with cermet electrolyte | |
DE60032577D1 (de) | Kompositelektroden für festkörperelektrochemische vorrichtungen | |
WO2006062947A3 (en) | Nanowire-based membrane electrode assemblies for fuel cells | |
DK0788175T3 (da) | Højtemperatur-brændstofcelle med en tyndfilmelektrolyt | |
EP1768208A3 (de) | Anodengestützte Hochleistungsbrennstoffzelle | |
ATE498916T1 (de) | Brennstoffzellen | |
ATE461530T1 (de) | Brennstoffzellenanordnung | |
DK1464092T3 (da) | SOFC brændselscelle | |
EP1263071A3 (de) | Verfahren zur Verhinderung der Oxidation der Anoden in Brennstoffzellen | |
EP1255318A3 (de) | Einheitszelle für Festoxidelektrolyt-Brennstoffzelle und Verfahren zu ihrer Herstellung | |
EP1261059A3 (de) | Zellen-Plattenstruktur für Brennstoffzelle, Verfahren zu ihrer Herstellung und Festelektrolytbrennstoffzelle | |
EP1575105A3 (de) | Polymerelektrolyt Brennstoffzelle | |
EP1414094A3 (de) | Brennstoffzellenstruktur | |
TW200511633A (en) | Electrolyte membrane, electrolyte membrane composite, method of manufacturing electrolyte membrane composite, electrolyte membrane-electrode assembly for fuel cell, method of manufacturing electrolyte membrane-electrode assembly for fuel cell, and fuel | |
EP1478041A3 (de) | Brennstoffzelle | |
EP1079451A3 (de) | Festpolymerelektrolytbrennstoffzelle und Herstellungsverfahren | |
WO2005015675A3 (en) | A solid oxide fuel cell | |
KR20140116029A (ko) | 막-전극 조립체의 제조방법 | |
KR100953102B1 (ko) | 다공질 금속의 후막 지지체를 이용한 금속 지지체형고체산화물 연료전지 및 이의 제조 방법 | |
EP0997961A3 (de) | Laminierung bei Zimmertemperatur von Polymer enthaltenden Li-Ionen Elektroden | |
JP2008086910A (ja) | 水素分離膜−電解質膜接合体の製造方法 | |
WO2004015805A3 (en) | Electrochemical cell support structure | |
EP1059686A3 (de) | Polymer-Elektrolyt-Brennstoffzelle |