CN105950020A - 松香酯的生产方法 - Google Patents

松香酯的生产方法 Download PDF

Info

Publication number
CN105950020A
CN105950020A CN201610355804.2A CN201610355804A CN105950020A CN 105950020 A CN105950020 A CN 105950020A CN 201610355804 A CN201610355804 A CN 201610355804A CN 105950020 A CN105950020 A CN 105950020A
Authority
CN
China
Prior art keywords
rosin ester
reaction
catalyst
production method
cavitation machine
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201610355804.2A
Other languages
English (en)
Inventor
黄桂彬
蒋茵荣
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guangxi Zhongchang Resin Co Ltd
Original Assignee
Guangxi Zhongchang Resin Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Guangxi Zhongchang Resin Co Ltd filed Critical Guangxi Zhongchang Resin Co Ltd
Priority to CN201610355804.2A priority Critical patent/CN105950020A/zh
Publication of CN105950020A publication Critical patent/CN105950020A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种松香酯的生产方法,涉及松香深加工技术领域。本发明方法包括以下步骤:将松香加入反应釜中,充入惰性气体,升温至165℃~170℃,加热融化,冷却至室温,然后转入空化机中,加入多元醇和催化剂,开启空化机,调节反应温度至120℃~130℃,反应至产物纯度大于90%,过滤,除去催化剂,即得到松香酯。本发明将酯化反应转入空化机中进行反应,反应过程中产生的高温高压使得高分子分解、化学键断裂和产生自由基等,从而较大程度的促进酯化反应的发生,使得反应在较短时间内即可完成,提高了原料的转化率,减少副反应的发生,所制备的产品纯度较高。

Description

松香酯的生产方法
技术领域
本发明涉及松香深加工技术领域,尤其是一种松香酯的生产方法。
背景技术
松香具有防腐、防潮、绝缘、粘合和乳化等许多优良性能,广泛应用于油墨、油漆、胶黏剂、涂料以及助焊等工业中。但由于松香本身的不稳定性,如易结晶、易被氧化变色及软化点低等,使其性能和应用领域受到一定的限制。对松香进行酯化改性是其中重要的方式之一。
松香酯是松香酸的多元醇酯,常用的多元醇有甘油和季戊四醇。多元醇松香酯是浅黄色的透明固体,软化点在90~110℃,酸值为10~20。用以制漆,质量比松香钙皂所制者略高。
目前松香酯制备方法一般将熔融后的松香与多元醇、催化剂等混合,进行酯化反应,其酯化反应时间较长,其生产成本较高;另外,长时间的高温酯化反应使得副反应增多,所得产品纯度较低。
发明内容
本发明的目的是提供一种松香酯的生产方法,这种方法可以解决松香酯产品纯度低的问题。
为了解决上述问题,本发明采用的技术方案是:
这种松香酯的生产方法为:将松香加入反应釜中,充入惰性气体,升温至165℃~170℃,加热融化,冷却至室温,然后转入空化机中,加入多元醇和催化剂,开启空化机,调节反应温度至120℃~130℃,反应至产物纯度大于90%,过滤,除去催化剂,即得到松香酯。
上述技术方案中,更具体的技术方案还可以是:多元醇为甘油、季戊四醇、山梨醇中的一种或多种。
进一步的,催化剂为二氧化锰。
进一步的,松香、多元醇的质量之比为1:1.5~4,催化剂的质量为松香总重量的0.01%~0.2%。
更进一步的,空化机工作时的压力为0.3兆帕~0.6兆帕。
由于采用了上述技术方案,本发明与现有技术相比具有如下有益效果:
本发明将酯化反应转入空化机中进行反应,反应过程中产生的高温高压使得高分子分解、化学键断裂和产生自由基等,从而较大程度的促进酯化反应的发生,使得反应在较短时间内即可完成,提高了原料的转化率,减少副反应的发生,所制备的产品纯度较高。
具体实施方式
下面结合实施例对本发明作进一步详述:
实施例1
本实施例松香酯的生产方法为:将松香加入反应釜中,充入惰性气体,升温至165℃,加热融化,冷却至室温,然后转入空化机中,涡流空化装置工作时的压力为0.3兆帕,加入山梨醇和二氧化锰,开启空化机,调节反应温度至125℃,反应至产物纯度为92%,过滤,除去催化剂,即得到松香酯。
本实施例松香、多元醇的质量之比为1:4,二氧化锰的质量为松香总重量的0.01%。
实施例2
本实施例松香酯的生产方法为:将松香加入反应釜中,充入惰性气体,升温至165℃,加热融化,冷却至室温,然后转入空化机中,涡流空化装置工作时的压力为0.4兆帕,加入甘油和二氧化锰,开启空化机,调节反应温度至130℃,反应至产物纯度为94%,过滤,除去催化剂,即得到松香酯。
本实施例松香、多元醇的质量之比为1:3,甘油的质量为松香总重量的0.1%。
实施例3
本实施例松香酯的生产方法为:将松香加入反应釜中,充入惰性气体,升温至170℃,加热融化,冷却至室温,然后转入空化机中,涡流空化装置工作时的压力为0.6兆帕,加入季戊四醇和二氧化锰,开启空化机,调节反应温度至120℃,反应至产物纯度为93%,过滤,除去催化剂,即得到松香酯。
本实施例松香、多元醇的质量之比为1:1.5,季戊四醇的质量为松香总重量的0.2%。

Claims (6)

1.一种松香酯的生产方法,其特征在于:将松香加入反应釜中,充入惰性气体,升温至165℃~170℃,加热融化,冷却至室温,然后转入空化机中,加入多元醇和催化剂,开启空化机,调节反应温度至120℃~130℃,反应至产物纯度大于90%,过滤,除去催化剂,即得到松香酯。
2.根据权利要求1所述的松香酯的生产方法,其特征在于:所述多元醇为甘油、季戊四醇、山梨醇中的一种或多种。
3.根据权利要求1或2所述的松香酯的生产方法,其特征在于:所述催化剂为二氧化锰。
4.根据权利要求1所述的松香酯的生产方法,其特征在于:松香、多元醇的质量之比为1:1.5~4,催化剂的质量为松香总重量的0.01%~0.2%。
5.根据权利要求1或2或4所述的松香酯的生产方法,其特征在于:所述空化机工作时的压力为0.3兆帕~0.6兆帕。
6.根据权利要求3所述的松香酯的生产方法,其特征在于:所述空化机工作时的压力为0.3兆帕~0.6兆帕。
CN201610355804.2A 2016-05-26 2016-05-26 松香酯的生产方法 Pending CN105950020A (zh)