CN103303371A - 一种车顶篷的生产工艺 - Google Patents

一种车顶篷的生产工艺 Download PDF

Info

Publication number
CN103303371A
CN103303371A CN2013102317242A CN201310231724A CN103303371A CN 103303371 A CN103303371 A CN 103303371A CN 2013102317242 A CN2013102317242 A CN 2013102317242A CN 201310231724 A CN201310231724 A CN 201310231724A CN 103303371 A CN103303371 A CN 103303371A
Authority
CN
China
Prior art keywords
vehicle
roof
air
vehicle canopy
shell
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN2013102317242A
Other languages
English (en)
Other versions
CN103303371B (zh
Inventor
张晓钟
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
DONGGUAN UPAL OUTDOORS MANUFACTURING Co Ltd
Original Assignee
DONGGUAN UPAL OUTDOORS MANUFACTURING Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by DONGGUAN UPAL OUTDOORS MANUFACTURING Co Ltd filed Critical DONGGUAN UPAL OUTDOORS MANUFACTURING Co Ltd
Priority to CN201310231724.2A priority Critical patent/CN103303371B/zh
Publication of CN103303371A publication Critical patent/CN103303371A/zh
Application granted granted Critical
Publication of CN103303371B publication Critical patent/CN103303371B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种车顶篷的生产工艺,其步骤如下:步骤一,对车顶篷外壳进行钻孔处理;步骤二,对经步骤一处理后的车顶篷外壳进行清洗,以除去加工及运输过程中的油渍和污渍,然后将清洗好的车顶篷外壳进行风干处理;步骤三,将经步骤二的车顶篷置于喷胶房中,然后压缩空气并控制空气压力在55~64kg/cm2之间,利用空气压力对车顶篷进行喷胶处理;步骤四,将面料粘在车顶篷的内侧,然后进行热压成型。本发明在接近室温的环境下完成,有机物质不易挥发,改善了生产作业环境。通过本发明生产的车顶篷的合格率较高,同时本发明生产效率高,较常规方法其产品的生产效率提高了30%,降低了生产成本,满足了客户需求。

Description

一种车顶篷的生产工艺
技术领域
本发明涉及一种车顶篷的生产工艺,具体的说是一种改善作业环境、提高生产效率的车顶篷的生产工艺。
背景技术
  随着人们生活水平的提高,汽车已经慢慢的进入大部分人的家庭,在越来越追求高性能、环保型、节能型的时代,汽车内饰与汽车外形一样已经成为了人们选车时的一个重要标准,人们对汽车的内饰件的要求也越来越高。车顶篷是安装于汽车车顶的部件,其主要作用是提高车内的装饰性,同时还可以提高与车外的隔热、绝热效果,降低车内的噪声,提高人们的舒适度和安全度。然而现有的车顶篷的生产还存在一些问题,其生产作业环境差,制造过程中单体面料通过火焰或胶水与PU复合成型,该过程中容易造成有机物的挥发,气味不能满足车间的环境要求,对生产员工的健康具有极大的安全隐患。现有技术中生产的车顶篷的性能较差,产品合格率较低,次品含量大,这样就导致生产厂家的经济效益低。
发明内容
本发明提出一种改善作业环境、提高生产效率的车顶篷的生产工艺。
为了解决现有技术问题,本发明是通过以下技术方案实现的。
一种车顶篷的生产工艺,其步骤如下:
    步骤一,在风速为12~20m/s、排风量为300~500m3/min的风房中对车顶篷外壳进行钻孔处理;
步骤二,对经步骤一处理后的车顶篷外壳进行清洗,以除去加工及运输过程中的油渍和污渍,然后将清洗好的车顶篷外壳进行风干处理,风干温度为40~45℃、相对湿度低于18~25%,风干时间为35~45min;
步骤三,将经步骤二的车顶篷置于喷胶房中,喷胶房中温度为20~25℃、相对湿度为18~25%,然后压缩空气并控制空气压力在55~64Kg/cm2之间,利用空气压力对车顶篷进行喷胶处理;
步骤四,将面料粘在车顶篷的内侧,然后进行热压成型,成型压力为6.2~7.4Mpa,成型时间为25~30s。
步骤三喷胶过程中,车顶篷内侧胶水厚度保持在0.05~0.08mm之间。
步骤四中所述面料为棉花布或密度为180~190g/m2的聚氨酯泡棉复合面料。
与现有技术相比,本发明的有益效果如下:
本发明在接近室温的环境下完成,有机物质不易挥发,改善了生产作业环境,通过简单的工艺即可完成车顶篷的制作,且产品的性能指数可以得到充分的保障,产品的可靠性高。通过本发明生产工艺生产的车顶篷的合格率较高,较常规方法其产品合格率提高了20%,本发明生产效率高,较常规方法其产品的生产效率提高了30%,大大降低了生产成本,满足客户需求。
具体实施方式
为了本领域技术人员的理解,以下结合具体实施例对本发明做进一步详述。
实施例1
本实施例一种车顶篷的生产工艺,其步骤如下:
    步骤一,选用合格的车顶篷,在风速为12m/s、排风量为300m3/min的风房中对车顶篷外壳进行钻孔处理,本实施例按工程图纸出具的SOP要求进行钻孔。风房中风速的控制主要是吸收钻孔过程中产生的灰尘,以使得生产作业环境不受影响。
步骤二,对经步骤一处理后的车顶篷外壳进行清洗,以除去加工及运输过程中的油渍和污渍,然后将清洗好的车顶篷外壳进行风干处理,风干温度为40℃、相对湿度低于18%,风干时间为35min。
步骤三,将经步骤二的车顶篷置于喷胶房中,喷胶房中温度为20℃、相对湿度为18%,然后压缩空气并控制空气压力在55Kg/cm2之间,利用空气压力对车顶篷进行喷胶处理,车顶篷内侧胶水厚度控制为0.05mm。
步骤四,将密度为180g/m2的聚氨酯泡棉复合面料粘在车顶篷的内侧,然后进行热压成型,成型压力为6.2Mpa,成型时间为25s。
经上述步骤后,按工程图纸出具的SOP要求对车顶篷进行装配,最后包装出货。
实施例2
本实施例一种车顶篷的生产工艺,其步骤如下:
    步骤一,选用合格的车顶篷,在风速为15m/s、排风量为400m3/min的风房中对车顶篷外壳进行钻孔处理,本实施例按工程图纸出具的SOP要求进行钻孔。风房中风速的控制主要是吸收钻孔过程中产生的灰尘,以使得生产作业环境不受影响。
步骤二,对经步骤一处理后的车顶篷外壳进行清洗,以除去加工及运输过程中的油渍和污渍,然后将清洗好的车顶篷外壳进行风干处理,风干温度为42℃、相对湿度低于20%,风干时间为40min。
步骤三,将经步骤二的车顶篷置于喷胶房中,喷胶房中温度为22℃、相对湿度为20%,然后压缩空气并控制空气压力在60Kg/cm2之间,利用空气压力对车顶篷进行喷胶处理,车顶篷内侧胶水厚度控制为0.05mm。
步骤四,将棉花布粘在车顶篷的内侧,然后进行热压成型,成型压力为6.6Mpa,成型时间为27s。
经上述步骤后,按工程图纸出具的SOP要求对车顶篷进行装配,最后包装出货。
实施例3
本实施例一种车顶篷的生产工艺,其步骤如下:
    步骤一,选用合格的车顶篷,在风速为20m/s、排风量为500m3/min的风房中对车顶篷外壳进行钻孔处理,本实施例按工程图纸出具的SOP要求进行钻孔。风房中风速的控制主要是吸收钻孔过程中产生的灰尘,以使得生产作业环境不受影响。
步骤二,对经步骤一处理后的车顶篷外壳进行清洗,以除去加工及运输过程中的油渍和污渍,然后将清洗好的车顶篷外壳进行风干处理,风干温度为45℃、相对湿度低于25%,风干时间为45min。
步骤三,将经步骤二的车顶篷置于喷胶房中,喷胶房中温度为25℃、相对湿度为25%,然后压缩空气并控制空气压力在64Kg/cm2之间,利用空气压力对车顶篷进行喷胶处理,车顶篷内侧胶水厚度控制为0.08mm。
步骤四,将密度为190g/m2的聚氨酯泡棉复合面料粘在车顶篷的内侧,然后进行热压成型,成型压力为7.4Mpa,成型时间为30s。
经上述步骤后,按工程图纸出具的SOP要求对车顶篷进行装配,最后包装出货。
本发明在接近室温的环境下完成,有机物质不易挥发,改善了生产作业环境,通过简单的工艺即可完成车顶篷的制作,且产品的性能指数可以得到充分的保障,产品的可靠性高。通过本发明生产工艺生产的车顶篷的合格率较高,较常规方法其产品合格率提高了20%,本发明生产效率高,较常规方法其产品的生产效率提高了30%,大大降低了生产成本,满足客户需求。
上述实施例中提到的内容并非是对本发明的限定,在不脱离本发明的发明构思的前提下,任何显而易见的替换均在本发明的保护范围之内。

Claims (3)

1.一种车顶篷的生产工艺,其步骤如下:
     步骤一,在风速为12~20m/s、排风量为300~500m3/min的风房中对车顶篷外壳进行钻孔处理;
步骤二,对经步骤一处理后的车顶篷外壳进行清洗,以除去加工及运输过程中的油渍和污渍,然后将清洗好的车顶篷外壳进行风干处理,风干温度为40~45℃、相对湿度低于20%,风干时间为35~45min;
步骤三,将经步骤二的车顶篷置于喷胶房中,喷胶房中温度为20~25℃、相对湿度为18~25%,然后压缩空气并控制空气压力在55~64Kg/cm2之间,利用空气压力对车顶篷进行喷胶处理;
步骤四,将面料粘在车顶篷的内侧,然后进行热压成型,成型压力为6.2~7.4Mpa,成型时间为25~30s。
2.根据权利要求1所述的车顶篷的生产工艺,其特征在于:步骤三喷胶过程中,车顶篷内侧胶水厚度保持在0.05~0.08mm之间。
3.根据权利要求2所述的车顶篷的生产工艺,其特征在于:步骤四中所述面料为棉花布或密度为180~190g/m2的聚氨酯泡棉复合面料。
CN201310231724.2A 2013-06-13 2013-06-13 一种车顶篷的生产工艺 Active CN103303371B (zh)