JPS6354049B2 - - Google Patents
Info
- Publication number
- JPS6354049B2 JPS6354049B2 JP59126462A JP12646284A JPS6354049B2 JP S6354049 B2 JPS6354049 B2 JP S6354049B2 JP 59126462 A JP59126462 A JP 59126462A JP 12646284 A JP12646284 A JP 12646284A JP S6354049 B2 JPS6354049 B2 JP S6354049B2
- Authority
- JP
- Japan
- Prior art keywords
- steel
- rolled
- deep drawability
- cold
- temperature
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Heat Treatment Of Steel (AREA)
- Heat Treatment Of Sheet Steel (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP12646284A JPS616213A (ja) | 1984-06-21 | 1984-06-21 | 耐爪とび性および深絞り性に優れたホ−ロ−用冷延鋼板の製造法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP12646284A JPS616213A (ja) | 1984-06-21 | 1984-06-21 | 耐爪とび性および深絞り性に優れたホ−ロ−用冷延鋼板の製造法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS616213A JPS616213A (ja) | 1986-01-11 |
JPS6354049B2 true JPS6354049B2 (enrdf_load_stackoverflow) | 1988-10-26 |
Family
ID=14935812
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP12646284A Granted JPS616213A (ja) | 1984-06-21 | 1984-06-21 | 耐爪とび性および深絞り性に優れたホ−ロ−用冷延鋼板の製造法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS616213A (enrdf_load_stackoverflow) |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH07113138B2 (ja) * | 1988-07-29 | 1995-12-06 | 日本鋼管株式会社 | 耐泡性の優れたホーロー用冷延鋼板およびその製造方法 |
EP2145971A1 (en) * | 2008-07-07 | 2010-01-20 | ArcelorMittal France | Hot rolled steel and enamelled steel sheet free of fish scale defect |
Family Cites Families (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS53131919A (en) * | 1977-04-25 | 1978-11-17 | Nippon Steel Corp | Method of fabricating steel plate to be enameled using aluminum killed steel, having goods cratch resistance and cold moldability |
JPS5726340A (en) * | 1980-07-24 | 1982-02-12 | Matsushita Electric Ind Co Ltd | Bath room combined with drying room |
JPS6051537B2 (ja) * | 1981-06-29 | 1985-11-14 | 日本鋼管株式会社 | ホ−ロ−性に優れたアルミキルド冷延鋼板の製造法 |
-
1984
- 1984-06-21 JP JP12646284A patent/JPS616213A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS616213A (ja) | 1986-01-11 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US3239390A (en) | Method of producing non-ageing special low carbon iron sheets | |
WO1984001585A1 (en) | Process for manufacturing cold-rolled steel for deep drawing | |
JPS59140333A (ja) | 2次加工性と表面処理性の優れた深絞り用冷延鋼板の製造方法 | |
JP3309732B2 (ja) | 深絞り性の優れた直接1回掛けほうろう用冷延鋼板およびその製造方法 | |
JPS6354049B2 (enrdf_load_stackoverflow) | ||
JP3421911B2 (ja) | 焼成後強度が低下しにくいほうろう用冷延鋼板 | |
JP3352904B2 (ja) | 無方向性電磁鋼板の製造方法 | |
JP4023123B2 (ja) | ほうろう用鋼板とその製造方法 | |
JP3360624B2 (ja) | ほうろう用冷延鋼板とその製造方法 | |
JP3384265B2 (ja) | 耐爪とび性に優れたほうろう用冷延鋼板の製造方法 | |
JP3858127B2 (ja) | 耐爪とび性に優れたほうろう用冷延鋼板の製造方法 | |
JPH06279864A (ja) | ほうろう用アルミニウムキルド冷延鋼板の製造方法 | |
JP7648978B2 (ja) | 鋼板およびほうろう製品 | |
JPH01275736A (ja) | 加工性に優れた連続鋳造製ほうろう用鋼板およびその製造法 | |
WO1991001390A1 (fr) | Procede pour fabriquer une tole d'acier a emailler presentant un excellent pouvoir adhesif | |
JPH02282421A (ja) | 連続鋳造一連続焼鈍製非時効性ほうろう用鋼板の製造法 | |
JPH03166336A (ja) | 深絞り性の極めて優れたほうろう用鋼板 | |
JPH05179357A (ja) | フェライトステンレス冷延鋼板の製造方法 | |
JPS633945B2 (enrdf_load_stackoverflow) | ||
JPH03126814A (ja) | 高張力ほうろう用鋼板の製造方法 | |
JPS6051537B2 (ja) | ホ−ロ−性に優れたアルミキルド冷延鋼板の製造法 | |
JPS62151546A (ja) | 耐爪飛び性に優れ且つ焼成後の強度が高いホーロー用薄板向熱延鋼板およびその製造方法 | |
JPH02156043A (ja) | ほうろう用Alキルド鋼板およびその製造方法 | |
JPS6114212B2 (enrdf_load_stackoverflow) | ||
JPH06279865A (ja) | ほうろう用冷延鋼板の製造方法 |