JPS61208755A - 密閉型アルカリ蓄電池用ペ−スト式カドミウム陰極板 - Google Patents
密閉型アルカリ蓄電池用ペ−スト式カドミウム陰極板Info
- Publication number
- JPS61208755A JPS61208755A JP60049763A JP4976385A JPS61208755A JP S61208755 A JPS61208755 A JP S61208755A JP 60049763 A JP60049763 A JP 60049763A JP 4976385 A JP4976385 A JP 4976385A JP S61208755 A JPS61208755 A JP S61208755A
- Authority
- JP
- Japan
- Prior art keywords
- active material
- material layer
- layer
- conductive
- cadmium
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M10/00—Secondary cells; Manufacture thereof
- H01M10/34—Gastight accumulators
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/24—Electrodes for alkaline accumulators
- H01M4/246—Cadmium electrodes
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M10/00—Secondary cells; Manufacture thereof
- H01M10/42—Methods or arrangements for servicing or maintenance of secondary cells or secondary half-cells
- H01M10/52—Removing gases inside the secondary cell, e.g. by absorption
- H01M10/526—Removing gases inside the secondary cell, e.g. by absorption by gas recombination on the electrode surface or by structuring the electrode surface to improve gas recombination
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M2004/026—Electrodes composed of, or comprising, active material characterised by the polarity
- H01M2004/027—Negative electrodes
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Secondary Cells (AREA)
- Engineering & Computer Science (AREA)
- Manufacturing & Machinery (AREA)
- Battery Electrode And Active Subsutance (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP60049763A JPS61208755A (ja) | 1985-03-13 | 1985-03-13 | 密閉型アルカリ蓄電池用ペ−スト式カドミウム陰極板 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP60049763A JPS61208755A (ja) | 1985-03-13 | 1985-03-13 | 密閉型アルカリ蓄電池用ペ−スト式カドミウム陰極板 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS61208755A true JPS61208755A (ja) | 1986-09-17 |
JPH0568828B2 JPH0568828B2 (enrdf_load_stackoverflow) | 1993-09-29 |
Family
ID=12840211
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP60049763A Granted JPS61208755A (ja) | 1985-03-13 | 1985-03-13 | 密閉型アルカリ蓄電池用ペ−スト式カドミウム陰極板 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS61208755A (enrdf_load_stackoverflow) |
Cited By (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6273566A (ja) * | 1985-09-26 | 1987-04-04 | Shin Kobe Electric Mach Co Ltd | 密閉形アルカリ蓄電池用陰極板の製造方法 |
JPS63158747A (ja) * | 1986-12-22 | 1988-07-01 | Matsushita Electric Ind Co Ltd | ペ−スト式カドミウム負極 |
JPS63202857A (ja) * | 1987-02-17 | 1988-08-22 | Sanyo Electric Co Ltd | アルカリ蓄電池用カドミウム電極 |
JPH03147257A (ja) * | 1989-10-31 | 1991-06-24 | Shin Kobe Electric Mach Co Ltd | 密閉形ニッケル‐カドミウム蓄電池用ペースト式陰極板 |
EP0645832A3 (de) * | 1993-08-11 | 1995-06-07 | Varta Batterie | Negative Elektrode für gasdichte alkalische Akkumulatoren, die eine Russ enthaltende Gasverzehrschicht besitzt. |
Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS569777A (en) * | 1979-07-04 | 1981-01-31 | Suwa Seikosha Kk | Liquid crystal display body |
JPS5713103A (en) * | 1980-06-23 | 1982-01-23 | Meidensha Electric Mfg Co Ltd | Wet type finely pulverizing method in manufacture of rare earth element magnet |
JPS5772264A (en) * | 1980-10-20 | 1982-05-06 | Matsushita Electric Ind Co Ltd | Cadmium electrode for alkaline battery and its manufacture |
-
1985
- 1985-03-13 JP JP60049763A patent/JPS61208755A/ja active Granted
Patent Citations (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS569777A (en) * | 1979-07-04 | 1981-01-31 | Suwa Seikosha Kk | Liquid crystal display body |
JPS5713103A (en) * | 1980-06-23 | 1982-01-23 | Meidensha Electric Mfg Co Ltd | Wet type finely pulverizing method in manufacture of rare earth element magnet |
JPS5772264A (en) * | 1980-10-20 | 1982-05-06 | Matsushita Electric Ind Co Ltd | Cadmium electrode for alkaline battery and its manufacture |
Cited By (6)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS6273566A (ja) * | 1985-09-26 | 1987-04-04 | Shin Kobe Electric Mach Co Ltd | 密閉形アルカリ蓄電池用陰極板の製造方法 |
JPS63158747A (ja) * | 1986-12-22 | 1988-07-01 | Matsushita Electric Ind Co Ltd | ペ−スト式カドミウム負極 |
JPS63202857A (ja) * | 1987-02-17 | 1988-08-22 | Sanyo Electric Co Ltd | アルカリ蓄電池用カドミウム電極 |
JPH03147257A (ja) * | 1989-10-31 | 1991-06-24 | Shin Kobe Electric Mach Co Ltd | 密閉形ニッケル‐カドミウム蓄電池用ペースト式陰極板 |
EP0645832A3 (de) * | 1993-08-11 | 1995-06-07 | Varta Batterie | Negative Elektrode für gasdichte alkalische Akkumulatoren, die eine Russ enthaltende Gasverzehrschicht besitzt. |
CN1065665C (zh) * | 1993-08-11 | 2001-05-09 | 瓦尔达电池股份公司 | 具有含有碳黑耗气层的密封碱性蓄电池负极 |
Also Published As
Publication number | Publication date |
---|---|
JPH0568828B2 (enrdf_load_stackoverflow) | 1993-09-29 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US3785868A (en) | Zinc electrode | |
JP3246345B2 (ja) | アルカリ蓄電池用ニッケル正極とこれを用いたニッケル・水素蓄電池 | |
JP3923157B2 (ja) | アルカリ蓄電池 | |
JP2001338645A (ja) | アルカリ蓄電池用ペースト型正極およびニッケル水素蓄電池 | |
JPH117948A (ja) | ニッケル−水素電池用陰極およびその製造方法 | |
JPS61208755A (ja) | 密閉型アルカリ蓄電池用ペ−スト式カドミウム陰極板 | |
JP3198891B2 (ja) | アルカリ蓄電池用正極 | |
JPS5931177B2 (ja) | アルカリ蓄電池用亜鉛極 | |
JPS624828B2 (enrdf_load_stackoverflow) | ||
JP3461923B2 (ja) | 電池用負極材料およびその製造方法、それを利用した負極体並びに二次電池 | |
JPH0536392A (ja) | ニツケル水素二次電池モジユール | |
JPH04109556A (ja) | 密閉型二次電池 | |
JPH0642374B2 (ja) | 金属−水素アルカリ蓄電池 | |
JP3287386B2 (ja) | アルカリ蓄電池用ニッケル電極 | |
JPH0234433B2 (enrdf_load_stackoverflow) | ||
JP2734149B2 (ja) | ペースト式カドミウム負極の製造法 | |
JPH09245827A (ja) | アルカリ蓄電池の製造法 | |
JPS59114767A (ja) | 水素電極の製造方法 | |
JP2564176B2 (ja) | 密閉型アルカリ二次電池用カドミウム負極板およびその負極板を用いた密閉型アルカリ二次電池 | |
JP2840270B2 (ja) | アルカリ蓄電池用ペースト式カドミウム電極及びその製造方法 | |
JPS62252072A (ja) | アルカリ蓄電池用負極の製造法 | |
JPH06124706A (ja) | 密閉形ニッケル−亜鉛蓄電池 | |
JPH03159064A (ja) | ニッケルカドミウム蓄電池 | |
JPS63164162A (ja) | アルカリ蓄電池用カドミウム負極 | |
JPS6084768A (ja) | アルカリ亜鉛蓄電池 |