JPS5982121A - ワ−ク打抜法 - Google Patents
ワ−ク打抜法Info
- Publication number
- JPS5982121A JPS5982121A JP19381882A JP19381882A JPS5982121A JP S5982121 A JPS5982121 A JP S5982121A JP 19381882 A JP19381882 A JP 19381882A JP 19381882 A JP19381882 A JP 19381882A JP S5982121 A JPS5982121 A JP S5982121A
- Authority
- JP
- Japan
- Prior art keywords
- punch
- work
- stage
- workpiece
- die
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
(57)【要約】本公報は電子出願前の出願データであるた
め要約のデータは記録されません。
め要約のデータは記録されません。
Description
【発明の詳細な説明】
本発明は、ワークのパリなし打抜法に関する。
従来、金属板から打抜を行なって、ワーク3aを求める
場合、第1図(a)と第1図(b)に示すように、抜は
側にパリ8が発生する。パリは実用上、後処理を必要と
する場合がほとんどで必シ、不経済である。
場合、第1図(a)と第1図(b)に示すように、抜は
側にパリ8が発生する。パリは実用上、後処理を必要と
する場合がほとんどで必シ、不経済である。
この発明は、上記の従来の1回打抜ワークのごとく、パ
ンチ摩耗が直接パリ発生につながる欠点を除去するため
、金型第1ステージを半抜とし・第1ステージパンチ、
ダイよりもクリアランスを大にした第2ステージで、送
り抜外し加工を行なうことにより、パリ少(パリ処理不
要)のワークを求めることを目的としたものである。
ンチ摩耗が直接パリ発生につながる欠点を除去するため
、金型第1ステージを半抜とし・第1ステージパンチ、
ダイよりもクリアランスを大にした第2ステージで、送
り抜外し加工を行なうことにより、パリ少(パリ処理不
要)のワークを求めることを目的としたものである。
以下、本発明を図面にもとづいて詳細に説明する。
第2図(第1ステージ)において、パンチ2aの被加工
材4を55%〜65%tの半抜きを行ない、ワーク3b
との間に破断が発生完了する条件を有するものである。
材4を55%〜65%tの半抜きを行ない、ワーク3b
との間に破断が発生完了する条件を有するものである。
第1ステージ(第2図)のパンチ2aは、被加工材4の
材質により55%〜65%tの範囲でパンチ突込み深さ
を任意に選び、杓抜の破断面発生時点で途中停止、ワー
ク3 bf抜落させない状態のtま、パンチ2aは上死
点に戻る。
材質により55%〜65%tの範囲でパンチ突込み深さ
を任意に選び、杓抜の破断面発生時点で途中停止、ワー
ク3 bf抜落させない状態のtま、パンチ2aは上死
点に戻る。
次に、破@面発生のみで波刃11工材から抜落されてい
ないワークを、ダイ上面の次のステージ(第3図(a)
と(b))で、第1ステージ(第2図)パンチとダイの
クリアランスより太きい、すなわち、パンチ2bはワー
クの太きさより小さ°く、ダイ1bはワークよυ大きい
クリアランスの第2パンチ2bにて外し抜きを引き続き
行なう。
ないワークを、ダイ上面の次のステージ(第3図(a)
と(b))で、第1ステージ(第2図)パンチとダイの
クリアランスより太きい、すなわち、パンチ2bはワー
クの太きさより小さ°く、ダイ1bはワークよυ大きい
クリアランスの第2パンチ2bにて外し抜きを引き続き
行なう。
第6図(a)と(b)に示すように、パンチ2bは、ワ
ークを完全に落下せしめるため、押し出し穴9を有した
ものである。
ークを完全に落下せしめるため、押し出し穴9を有した
ものである。
第2パンチ2 b T p 2ダイ1bは、ワーク寸法
より小さく、外周被抜部に触れない条件を有する。
より小さく、外周被抜部に触れない条件を有する。
ワーク3bは、破断面側に少量のパリが残る場合も考え
られるが、実用上はとんど支障のないワークを取り出せ
ることを目的としたものである。
られるが、実用上はとんど支障のないワークを取り出せ
ることを目的としたものである。
以上のごとく、本発明によれば、金型は2ステージを持
つ。
つ。
第1ステージパンチは、打抜に際して、途中抜破断面発
生状態のワークのまま、第2ステージに送る。
生状態のワークのまま、第2ステージに送る。
第2ステージの送り抜部パンチとダイは、第1ステージ
パンチ、ダイより、クリアランスを大餐〈取υ、外し抜
を行なう事で、パリなしワークが簡単に作られる効果を
有する。
パンチ、ダイより、クリアランスを大餐〈取υ、外し抜
を行なう事で、パリなしワークが簡単に作られる効果を
有する。
第11ン」(8)は、従来の打抜側面図第1図(b)は
、従来ワークの打抜完了側面図第2図は、本件の第1ス
テージ破断面発生(半抜き)状態側面図 第5図(a) Ifh、本件の第2ステージ外し状態側
面図 第3図(b)は、パンチからワーク葡離した状態側面図
である。 1a、1b・・・・・・グ イ 2a 2b・・・・・・パンチ 3a、3b・・・・・・ワーク 4・・・・・・被加工材 5・・・・・・ワークのダレ 6・・・・・・ワークのせん断面 7・・・・・・ワークの破断面 8・・・・・・ワークのパリ 9・・・・・・パンチからワーク外しの穴場上 出願人 株式会社 第二稍玉舎
、従来ワークの打抜完了側面図第2図は、本件の第1ス
テージ破断面発生(半抜き)状態側面図 第5図(a) Ifh、本件の第2ステージ外し状態側
面図 第3図(b)は、パンチからワーク葡離した状態側面図
である。 1a、1b・・・・・・グ イ 2a 2b・・・・・・パンチ 3a、3b・・・・・・ワーク 4・・・・・・被加工材 5・・・・・・ワークのダレ 6・・・・・・ワークのせん断面 7・・・・・・ワークの破断面 8・・・・・・ワークのパリ 9・・・・・・パンチからワーク外しの穴場上 出願人 株式会社 第二稍玉舎
Claims (1)
- 金属版材から、ワークを求める打抜方法で、第1拐抜の
際、パンチの深さをワーク厚みの55%〜65%の半抜
き状態にとどめて、パンチとダイの間に破断を生ぜしめ
た後、第2ステージの第1打抜パンチとダイよシも、ク
リアランスを大にしたパンチとダイにて、ワークの抜外
し加′工を行なうこと全特徴とするワーク打抜方法。