JPH0580131B2 - - Google Patents
Info
- Publication number
- JPH0580131B2 JPH0580131B2 JP63107656A JP10765688A JPH0580131B2 JP H0580131 B2 JPH0580131 B2 JP H0580131B2 JP 63107656 A JP63107656 A JP 63107656A JP 10765688 A JP10765688 A JP 10765688A JP H0580131 B2 JPH0580131 B2 JP H0580131B2
- Authority
- JP
- Japan
- Prior art keywords
- substrate
- substrates
- atmosphere
- bonding
- heating chamber
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Local Oxidation Of Silicon (AREA)
- Recrystallisation Techniques (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP63107656A JPH01278752A (ja) | 1988-05-02 | 1988-05-02 | 半導体基板接合方法および接合装置 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP63107656A JPH01278752A (ja) | 1988-05-02 | 1988-05-02 | 半導体基板接合方法および接合装置 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPH01278752A JPH01278752A (ja) | 1989-11-09 |
| JPH0580131B2 true JPH0580131B2 (enExample) | 1993-11-08 |
Family
ID=14464705
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP63107656A Granted JPH01278752A (ja) | 1988-05-02 | 1988-05-02 | 半導体基板接合方法および接合装置 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPH01278752A (enExample) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP5055671B2 (ja) * | 2001-07-26 | 2012-10-24 | 信越半導体株式会社 | Soi基板の製造方法 |
-
1988
- 1988-05-02 JP JP63107656A patent/JPH01278752A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPH01278752A (ja) | 1989-11-09 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPH04119626A (ja) | 接合ウェーハの製造方法 | |
| EP0603849B1 (en) | Method for producing a semiconducteur substrate by using a bonding process | |
| JP2006210898A (ja) | Soiウエーハの製造方法及びsoiウェーハ | |
| JPS60121715A (ja) | 半導体ウエハの接合方法 | |
| US8076219B2 (en) | Reduction of watermarks in HF treatments of semiconducting substrates | |
| JPS62122148A (ja) | 半導体基板 | |
| JPH07235651A (ja) | 半導体基板およびその作製方法 | |
| KR100253583B1 (ko) | 접합형 에스. 오. 아이 웨이퍼 제조방법 | |
| JPH01278752A (ja) | 半導体基板接合方法および接合装置 | |
| RU2382437C1 (ru) | Способ изготовления структуры кремний-на-изоляторе | |
| JPS63129633A (ja) | 半導体表面処理方法 | |
| JPH03181115A (ja) | 半導体基板の製造方法 | |
| JP2595935B2 (ja) | 表面清浄化方法 | |
| JPS60236210A (ja) | 半導体ウエハの接合方法 | |
| JPH0669087A (ja) | シリコン基板の形成方法 | |
| JPS61182216A (ja) | 半導体基板の接合方法 | |
| JPH0479209A (ja) | Soi基板の製造方法 | |
| JPH0963910A (ja) | 張り合わせウェーハおよびその製造方法 | |
| CN120727560B (zh) | 可降低退火热应力的含锑化铟异质晶圆制备方法及产品 | |
| JPH0580132B2 (enExample) | ||
| JPS6169135A (ja) | 半導体装置の製造方法 | |
| JPH03173131A (ja) | 半導体装置の製造方法 | |
| JPH0497533A (ja) | 半導体基板 | |
| JP3191346B2 (ja) | 貼り合わせ基板の製造方法 | |
| KR0136201B1 (ko) | 내부결함이 없는 접합 웨이퍼 제조방법 |