JPH0432160B2 - - Google Patents
Info
- Publication number
- JPH0432160B2 JPH0432160B2 JP63219244A JP21924488A JPH0432160B2 JP H0432160 B2 JPH0432160 B2 JP H0432160B2 JP 63219244 A JP63219244 A JP 63219244A JP 21924488 A JP21924488 A JP 21924488A JP H0432160 B2 JPH0432160 B2 JP H0432160B2
- Authority
- JP
- Japan
- Prior art keywords
- tin
- plating
- anode
- plating solution
- metal
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Electroplating Methods And Accessories (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP21924488A JPH0270087A (ja) | 1988-09-01 | 1988-09-01 | 錫めっき方法および装置 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP21924488A JPH0270087A (ja) | 1988-09-01 | 1988-09-01 | 錫めっき方法および装置 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPH0270087A JPH0270087A (ja) | 1990-03-08 |
JPH0432160B2 true JPH0432160B2 (enrdf_load_stackoverflow) | 1992-05-28 |
Family
ID=16732479
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP21924488A Granted JPH0270087A (ja) | 1988-09-01 | 1988-09-01 | 錫めっき方法および装置 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPH0270087A (enrdf_load_stackoverflow) |
Families Citing this family (10)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPH0826480B2 (ja) * | 1989-03-28 | 1996-03-13 | 日本エレクトロプレイテイング・エンジニヤース株式会社 | メッキ装置及びメッキ金属の補給方法 |
JPH05302199A (ja) * | 1992-04-24 | 1993-11-16 | Bridgestone Bekaert Steel Code Kk | 不溶性陽極を用いた銅めっき法における銅めっき浴の組成制御方法 |
KR100683268B1 (ko) | 1998-09-08 | 2007-02-15 | 가부시키가이샤 에바라 세이사꾸쇼 | 기판도금장치 |
US6793794B2 (en) | 2000-05-05 | 2004-09-21 | Ebara Corporation | Substrate plating apparatus and method |
IT1318545B1 (it) * | 2000-05-31 | 2003-08-27 | De Nora Elettrodi Spa | Cella di elettrolisi per il ripristino della concentrazione di ionimetallici in processi di elettrodeposizione. |
KR20010074263A (ko) * | 2001-05-03 | 2001-08-04 | 이수재 | 구리이온공급장치 |
AT413037B (de) * | 2003-07-25 | 2005-10-15 | Andritz Ag Maschf | Vorrichtung zum elektrolytischen beschichten eines metallischen gegenstandes mit zinn oder einer zinnlegierung |
DE10342291A1 (de) * | 2003-09-12 | 2005-04-14 | Dr.-Ing. Max Schlötter GmbH & Co KG | Verfahren zur elektrolytischen Abscheidung von Zinnlegierungen mit elektropositiveren Metallen |
US9303329B2 (en) | 2013-11-11 | 2016-04-05 | Tel Nexx, Inc. | Electrochemical deposition apparatus with remote catholyte fluid management |
JP7707911B2 (ja) * | 2021-12-28 | 2025-07-15 | トヨタ自動車株式会社 | 成膜装置及び成膜方法 |
Family Cites Families (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
BE787143A (fr) * | 1971-08-04 | 1973-02-05 | Creusot Loire | Procede de soufflage par tuyeres immergees dans un bain metallique |
JPS5232332A (en) * | 1975-09-05 | 1977-03-11 | Konishiroku Photo Ind Co Ltd | Transfer paper transport device in the electrophotographic copying mac hine |
JPS60121299A (ja) * | 1983-12-01 | 1985-06-28 | Tokuyama Soda Co Ltd | ニッケルメッキ方法 |
-
1988
- 1988-09-01 JP JP21924488A patent/JPH0270087A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPH0270087A (ja) | 1990-03-08 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JP3131648B2 (ja) | 非シアン化浴を用いる銅メッキ方法 | |
JPH0432160B2 (enrdf_load_stackoverflow) | ||
JPH10121297A (ja) | 不溶性陽極を用いた電気銅めっき装置及びそれを使用する銅めっき方法 | |
JP2009270188A (ja) | 高純度水酸化リチウムの製造方法 | |
TWI390083B (zh) | An electrolytic electrode and a method for producing a quaternary ammonium aqueous ammonium hydroxide solution using the electrolytic electrode | |
KR20120011584A (ko) | 3가크롬도금액 및 이를 이용한 도금방법 | |
CN103898553B (zh) | 一种电积和精炼同步进行生产金属钙的方法 | |
JP2559935B2 (ja) | 不溶性陽極を用いた錫又は錫ー鉛合金電気めっきの方法及び装置 | |
US4159926A (en) | Nickel plating | |
JPH10511743A (ja) | メッキ設備 | |
JPH05302199A (ja) | 不溶性陽極を用いた銅めっき法における銅めっき浴の組成制御方法 | |
US3855089A (en) | Process for the electrolytic refining of heavy metals | |
JP2009203487A (ja) | 隔膜電解による金属電解採取方法 | |
JPS6141799A (ja) | 電気錫メツキ浴への錫イオン補給法 | |
CN101545112B (zh) | 电解二氧化锰的电解方法 | |
JPS5983785A (ja) | 高濃度硫酸コバルト水溶液の製造方法 | |
ES306422A1 (es) | Procedimiento de refinado electrolitico de una aleaciën de niquel | |
US3706639A (en) | Rejuvenated chromium plating medium containing chromic compound | |
Murase et al. | Measurement of pH in the vicinity of a cathode during the chloride electrowinning of nickel | |
JP2014031533A (ja) | めっき方法 | |
JP3002265B2 (ja) | 高純度金属クロムの製造方法 | |
JPS63307291A (ja) | 高純度銅の製造方法 | |
US3715290A (en) | Method and apparatus for preparation of aluminium coagulating agent | |
JPS60128271A (ja) | 金属銅及び塩素の製造方法 | |
JP2010007133A (ja) | 金属インジウム製造方法及び装置 |