JPH0419299B2 - - Google Patents
Info
- Publication number
- JPH0419299B2 JPH0419299B2 JP60038672A JP3867285A JPH0419299B2 JP H0419299 B2 JPH0419299 B2 JP H0419299B2 JP 60038672 A JP60038672 A JP 60038672A JP 3867285 A JP3867285 A JP 3867285A JP H0419299 B2 JPH0419299 B2 JP H0419299B2
- Authority
- JP
- Japan
- Prior art keywords
- zinc
- plating
- bath
- hot
- layer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Landscapes
- Coating With Molten Metal (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP3867285A JPS61201767A (ja) | 1985-03-01 | 1985-03-01 | 二段めつき方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP3867285A JPS61201767A (ja) | 1985-03-01 | 1985-03-01 | 二段めつき方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS61201767A JPS61201767A (ja) | 1986-09-06 |
JPH0419299B2 true JPH0419299B2 (en, 2012) | 1992-03-30 |
Family
ID=12531759
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP3867285A Granted JPS61201767A (ja) | 1985-03-01 | 1985-03-01 | 二段めつき方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS61201767A (en, 2012) |
Families Citing this family (13)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS63134653A (ja) * | 1986-11-22 | 1988-06-07 | Nippon Steel Corp | 耐食性および加工性にすぐれた合金めつき鋼材の製造法 |
JPH01263255A (ja) * | 1988-04-14 | 1989-10-19 | Nippon Aen Kogyo Kk | 高付着溶融アルミニウム−亜鉛合金めっき方法 |
JPH0753901B2 (ja) * | 1989-12-07 | 1995-06-07 | 株式会社興和工業所 | 溶融亜鉛メッキ方法 |
US5849408A (en) * | 1993-12-27 | 1998-12-15 | Nippon Mining & Metals Co., Ltd. | Hot-dip zinc plating product |
JP2839130B2 (ja) * | 1993-12-27 | 1998-12-16 | 日鉱金属株式会社 | 溶融亜鉛合金めっき方法 |
JP3080014B2 (ja) * | 1996-11-11 | 2000-08-21 | 住友金属工業株式会社 | 溶融めっき方法 |
JP3425520B2 (ja) * | 1997-12-25 | 2003-07-14 | 日鉱金属株式会社 | 鉄鋼材料の溶融亜鉛二段めっき法 |
SG90041A1 (en) * | 1999-03-22 | 2002-07-23 | Fu Tsai Tsai | Hot dipping 5 weight % a1-zn alloy coating on steel |
DE10003680C2 (de) * | 2000-01-28 | 2003-04-10 | Thyssenkrupp Stahl Ag | Verfahren zum Herstellen eines mit einer Zinkbeschichtung versehenen Stahlbandes und zinkbeschichtetes Stahlband |
JP5909818B2 (ja) * | 2007-04-27 | 2016-04-27 | 盛貽熱浸▲辛▼企業股▲分▼有限公司 | 鉛フリー熔融亜鉛めっき方法及びその完成品 |
JP2009280897A (ja) * | 2008-05-23 | 2009-12-03 | Kowa Industry Co Ltd | 溶融高純度亜鉛めっき法 |
JP6870453B2 (ja) * | 2017-04-18 | 2021-05-12 | 日本製鉄株式会社 | 溶融亜鉛めっき鋼管 |
US12320005B2 (en) * | 2022-02-21 | 2025-06-03 | Nippon Steel Corporation | Hot-dip plated steel material |
Family Cites Families (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5230233A (en) * | 1975-09-02 | 1977-03-07 | Nippon Kokan Kk | Melttplating method of aluminummzing alloy |
JPS5735672A (en) * | 1980-08-11 | 1982-02-26 | Nippon Mining Co Ltd | Galvanizing method providing high corrosion resistance |
-
1985
- 1985-03-01 JP JP3867285A patent/JPS61201767A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS61201767A (ja) | 1986-09-06 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JP2777571B2 (ja) | アルミニウム−亜鉛−シリコン合金めっき被覆物及びその製造方法 | |
JPH0419299B2 (en, 2012) | ||
JP3476408B2 (ja) | 溶融Zn−Mg−Al系合金めっき鋼線およびその製造方法 | |
JPH07207421A (ja) | 亜鉛合金めっき方法 | |
JP2783452B2 (ja) | 合金化溶融亜鉛めっき鋼板の製造方法 | |
JPS6138259B2 (en, 2012) | ||
JPH03281788A (ja) | Zn―Al合金めっき鋼線の製造方法 | |
JPS63157847A (ja) | 合金化亜鉛メツキ鋼板の製造方法 | |
JPS63143269A (ja) | 耐食性および加工性にすぐれた合金めつき鋼材の製造法 | |
JPS63134653A (ja) | 耐食性および加工性にすぐれた合金めつき鋼材の製造法 | |
JP3009269B2 (ja) | 溶融亜鉛合金めっき被覆物 | |
JPS63297577A (ja) | 物性的に強化された鋼材表面構造並びにその製造方法 | |
JPS636620B2 (en, 2012) | ||
JP2747554B2 (ja) | アルミニウム・亜鉛合金めっき鋼板及びその製造方法 | |
JPH0368749A (ja) | 亜鉛系溶融めっき鋼板の製造方法 | |
JPH08269662A (ja) | 亜鉛−錫合金めっき鋼板の製造法 | |
JP3077950B2 (ja) | 溶融亜鉛合金めっき被覆物の製造方法 | |
JPS6227536A (ja) | 溶融亜鉛めつき用亜鉛合金及びその使用方法 | |
JP2541380B2 (ja) | 電着塗装性に優れた、複数の鉄−亜鉛合金めっき層を有する鉄−亜鉛合金めっき鋼板の製造方法 | |
JPH03260043A (ja) | 耐黒変性に優れた溶融亜鉛めっき鋼板およびその製造方法 | |
JPH04224666A (ja) | めっき密着性及び耐食性に優れた溶融亜鉛めっきステンレス鋼帯の製造方法 | |
KR0136176B1 (ko) | 내식성 및 광택성이 우수한 제로스팽글 용융아연 도금강판 제조방법 | |
JPH04246158A (ja) | 表面性状および耐食性に優れた合金めっき鋼線の製造方法 | |
JPH0368748A (ja) | 合金化溶融めっき鋼板およびその製造方法 | |
JPS62290894A (ja) | 合金めつき鋼板 |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
EXPY | Cancellation because of completion of term |