JPH0334481B2 - - Google Patents
Info
- Publication number
- JPH0334481B2 JPH0334481B2 JP13118483A JP13118483A JPH0334481B2 JP H0334481 B2 JPH0334481 B2 JP H0334481B2 JP 13118483 A JP13118483 A JP 13118483A JP 13118483 A JP13118483 A JP 13118483A JP H0334481 B2 JPH0334481 B2 JP H0334481B2
- Authority
- JP
- Japan
- Prior art keywords
- latex
- weight
- particle size
- parts
- rubber
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Processes Of Treating Macromolecular Substances (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP13118483A JPS6023425A (ja) | 1983-07-19 | 1983-07-19 | ゴム弾性体ラテツクスの粒径肥大方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP13118483A JPS6023425A (ja) | 1983-07-19 | 1983-07-19 | ゴム弾性体ラテツクスの粒径肥大方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS6023425A JPS6023425A (ja) | 1985-02-06 |
| JPH0334481B2 true JPH0334481B2 (enExample) | 1991-05-22 |
Family
ID=15051978
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP13118483A Granted JPS6023425A (ja) | 1983-07-19 | 1983-07-19 | ゴム弾性体ラテツクスの粒径肥大方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS6023425A (enExample) |
Families Citing this family (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP5731261B2 (ja) * | 2011-04-06 | 2015-06-10 | 株式会社日本触媒 | 微粒子の製造方法 |
-
1983
- 1983-07-19 JP JP13118483A patent/JPS6023425A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS6023425A (ja) | 1985-02-06 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JP2515264B2 (ja) | ラテックスの凝集方法、得られた凝集ラテックスおよび熱可塑性母材を改質して耐衝撃性をもたせるための該ラテックスの応用 | |
| EP0823450B1 (en) | Composite and moldings produced therefrom | |
| JP4817403B2 (ja) | 肥大化ラテックスの製造方法 | |
| JP3274978B2 (ja) | ポリブタジエンゴムラテックス用凝集剤の製造方法 | |
| JPH035405B2 (enExample) | ||
| JPS62106915A (ja) | ポリ塩化ビニル用透明性、衝撃性改善剤 | |
| EP1598372B1 (en) | Polymer particle composition and process for producing the same | |
| CN100386347C (zh) | 生产具有改进粉料性能的粉状线性聚合物的方法 | |
| JP3607708B2 (ja) | 耐候性樹脂組成物及びその製造方法 | |
| JP2003119396A (ja) | 耐衝撃性の優れた熱可塑性樹脂組成物 | |
| JP2608219B2 (ja) | 耐衝撃性及び光沢性熱可塑性樹脂の製造方法 | |
| JPH0334481B2 (enExample) | ||
| KR100513658B1 (ko) | 열안정성 및 분체 특성이 뛰어난 열가소성 수지 조성물 및그 제조방법 | |
| JPH11502258A (ja) | 高衝撃強度を有する熱可塑性樹脂の製造方法 | |
| JP2634691B2 (ja) | 塩化ビニル系樹脂組成物 | |
| KR100198733B1 (ko) | 폴리부타디엔 고무 라텍스의 제조 방법 | |
| KR930006082B1 (ko) | 열가소성 수지 조성물의 제조방법 | |
| KR100188529B1 (ko) | 저온내충격성 및 광택도가 우수한 열가소성 수지조성물의제조방법 | |
| KR940010341B1 (ko) | 고무라텍스의 제조방법 | |
| KR0182712B1 (ko) | 고무 라텍스를 응집하기 위한 응집제 및 그 제조방법 | |
| JPH054964B2 (enExample) | ||
| JP3315545B2 (ja) | 乳化重合による重合体の製造方法 | |
| KR100215388B1 (ko) | 내충격성및표면광택이우수한그라프트중합체의제조방법 | |
| KR950010553B1 (ko) | 내충격성 내후성 저광택 열가소성 수지의 제조방법 | |
| JPS5917728B2 (ja) | 耐衝撃性樹脂の製造方法 |