JPH0250803B2 - - Google Patents
Info
- Publication number
- JPH0250803B2 JPH0250803B2 JP56186216A JP18621681A JPH0250803B2 JP H0250803 B2 JPH0250803 B2 JP H0250803B2 JP 56186216 A JP56186216 A JP 56186216A JP 18621681 A JP18621681 A JP 18621681A JP H0250803 B2 JPH0250803 B2 JP H0250803B2
- Authority
- JP
- Japan
- Prior art keywords
- metal
- coating
- layer
- sprayed
- rolled
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Lifetime
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C4/00—Coating by spraying the coating material in the molten state, e.g. by flame, plasma or electric discharge
- C23C4/18—After-treatment
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Mechanical Engineering (AREA)
- Plasma & Fusion (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Materials Engineering (AREA)
- Physics & Mathematics (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Heat Treatment Of Sheet Steel (AREA)
- Metal Rolling (AREA)
- Coating By Spraying Or Casting (AREA)
- Heat Treatment Of Steel (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP18621681A JPS5887223A (ja) | 1981-11-20 | 1981-11-20 | 金属被覆鋼板の製造方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP18621681A JPS5887223A (ja) | 1981-11-20 | 1981-11-20 | 金属被覆鋼板の製造方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5887223A JPS5887223A (ja) | 1983-05-25 |
JPH0250803B2 true JPH0250803B2 (en, 2012) | 1990-11-05 |
Family
ID=16184397
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP18621681A Granted JPS5887223A (ja) | 1981-11-20 | 1981-11-20 | 金属被覆鋼板の製造方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5887223A (en, 2012) |
Families Citing this family (4)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS591003A (ja) * | 1982-06-28 | 1984-01-06 | Kawasaki Steel Corp | 耐食性、耐海水性および防汚性に優れる被覆鋼板の製造方法 |
JPS594903A (ja) * | 1982-06-29 | 1984-01-11 | Kawasaki Steel Corp | 自溶性合金被覆鋼板の製造方法 |
CN105369182B (zh) * | 2015-10-26 | 2018-02-09 | 昆明理工大学 | 一种制备钛铝合金薄板的方法 |
CN111389911A (zh) * | 2020-03-24 | 2020-07-10 | 首钢集团有限公司 | 一种薄宽规格高强度低合金耐磨钢板的生产方法 |
Family Cites Families (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS542612A (en) * | 1977-06-08 | 1979-01-10 | Hitachi Ltd | Fault-protective circuit of signal transmitter |
JPS6016509B2 (ja) * | 1978-08-29 | 1985-04-25 | 古河電気工業株式会社 | 導電用高力銅合金 |
-
1981
- 1981-11-20 JP JP18621681A patent/JPS5887223A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS5887223A (ja) | 1983-05-25 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
US6427904B1 (en) | Bonding of dissimilar metals | |
EP0640390B1 (en) | Catalytic converters - metal foil material for use therein, and a method of making the material | |
TWI357444B (en) | Zirconium-cladded steel plates, and elements of ch | |
JPS63236545A (ja) | 触媒担体及びその製造法 | |
CN102356177A (zh) | 防止熔损用被覆部件 | |
KR100543578B1 (ko) | 상이한 금속들의 결합 | |
KR102819975B1 (ko) | 부식방지 코팅이 구비된 강판 제품으로부터 판금 부품을 제조하는 방법 | |
US5121535A (en) | Method for production of thin sections of reactive metals | |
EP0119036B1 (en) | Metal-coating a metallic substrate | |
JPH0250803B2 (en, 2012) | ||
JP3403460B2 (ja) | 非酸化物系セラミック溶射皮膜を有する炭素材料の製造方法 | |
US5127146A (en) | Method for production of thin sections of reactive metals | |
JPH0250805B2 (en, 2012) | ||
JPH0353055A (ja) | 表面にセラミックスを溶射した金属ロール | |
JPH0250804B2 (en, 2012) | ||
EP0081847B1 (en) | Enameling process | |
JP3379917B2 (ja) | Al含有皮膜被覆部材とその製造方法 | |
JPH0516212Y2 (en, 2012) | ||
JPH04274890A (ja) | 亜鉛−アルミ二層表面処理鋼板の製造方法 | |
JPS5896862A (ja) | 複合被覆鋼板の製造方法 | |
JP2761963B2 (ja) | 加工性に優れたアルミニウムクラッド鋼板の製造方法 | |
JPH01317688A (ja) | 複合被覆鋼板の製造方法 | |
JPH024950A (ja) | 耐食性および耐摩耗性に優れた表面処理鋼板の製造方法 | |
JPS61186107A (ja) | 高耐食性表面被覆鋼板の製造方法 | |
JP3256360B2 (ja) | Ni合金クラッドステンレス鋼板 |