JPH01229622A - 高硬度、耐汚染性および防眩性に優れた塗装鋼板およびその製造方法 - Google Patents

高硬度、耐汚染性および防眩性に優れた塗装鋼板およびその製造方法

Info

Publication number
JPH01229622A
JPH01229622A JP5596388A JP5596388A JPH01229622A JP H01229622 A JPH01229622 A JP H01229622A JP 5596388 A JP5596388 A JP 5596388A JP 5596388 A JP5596388 A JP 5596388A JP H01229622 A JPH01229622 A JP H01229622A
Authority
JP
Japan
Prior art keywords
meth
acrylate
weight
parts
acid
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP5596388A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0445342B2 (enrdf_load_stackoverflow
Inventor
Nagaharu Ueno
上野 長治
Joji Oka
岡 襄二
Koji Ota
孝二 大田
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nippon Steel Corp
Original Assignee
Nippon Steel Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Nippon Steel Corp filed Critical Nippon Steel Corp
Priority to JP5596388A priority Critical patent/JPH01229622A/ja
Publication of JPH01229622A publication Critical patent/JPH01229622A/ja
Publication of JPH0445342B2 publication Critical patent/JPH0445342B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Application Of Or Painting With Fluid Materials (AREA)
  • Laminated Bodies (AREA)
  • Paints Or Removers (AREA)
JP5596388A 1988-03-11 1988-03-11 高硬度、耐汚染性および防眩性に優れた塗装鋼板およびその製造方法 Granted JPH01229622A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP5596388A JPH01229622A (ja) 1988-03-11 1988-03-11 高硬度、耐汚染性および防眩性に優れた塗装鋼板およびその製造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP5596388A JPH01229622A (ja) 1988-03-11 1988-03-11 高硬度、耐汚染性および防眩性に優れた塗装鋼板およびその製造方法

Publications (2)

Publication Number Publication Date
JPH01229622A true JPH01229622A (ja) 1989-09-13
JPH0445342B2 JPH0445342B2 (enrdf_load_stackoverflow) 1992-07-24

Family

ID=13013738

Family Applications (1)

Application Number Title Priority Date Filing Date
JP5596388A Granted JPH01229622A (ja) 1988-03-11 1988-03-11 高硬度、耐汚染性および防眩性に優れた塗装鋼板およびその製造方法

Country Status (1)

Country Link
JP (1) JPH01229622A (enrdf_load_stackoverflow)

Cited By (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2001181574A (ja) * 1999-12-24 2001-07-03 Kansai Paint Co Ltd 塗料組成物及びこの組成物を用いた塗装金属板
JP2002256220A (ja) * 2001-02-28 2002-09-11 Mitsubishi Rayon Co Ltd 被覆用硬化性組成物、多層硬化塗膜、被覆物品、自動車用外板、および活性エネルギー線硬化性組成物
JP2003206418A (ja) * 2002-01-15 2003-07-22 Toppan Printing Co Ltd 活性エネルギー線硬化ハードコート樹脂組成物およびハードコート層を含む積層体
US6746986B1 (en) 2000-04-24 2004-06-08 Nisshin Steel Co., Ltd. Painted metal sheet for printing with a sublimation dye
JP2008081719A (ja) * 2006-08-30 2008-04-10 Kansai Paint Co Ltd 上塗塗料組成物
JP2010181898A (ja) * 2010-03-10 2010-08-19 Dainippon Printing Co Ltd 高精細化デイスプレイ用防眩フィルムの製造方法
CN104070748A (zh) * 2014-05-22 2014-10-01 东莞市纳利光学材料有限公司 磨砂保护膜及其制备方法
JP2014188842A (ja) * 2013-03-27 2014-10-06 Dainippon Printing Co Ltd 化粧シート及びこれを用いた化粧板

Cited By (10)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2001181574A (ja) * 1999-12-24 2001-07-03 Kansai Paint Co Ltd 塗料組成物及びこの組成物を用いた塗装金属板
US6746986B1 (en) 2000-04-24 2004-06-08 Nisshin Steel Co., Ltd. Painted metal sheet for printing with a sublimation dye
US6987081B2 (en) 2000-04-24 2006-01-17 Nisshin Steel Co., Ltd. Painted metal sheet for printing with a sublimation dye
JP2002256220A (ja) * 2001-02-28 2002-09-11 Mitsubishi Rayon Co Ltd 被覆用硬化性組成物、多層硬化塗膜、被覆物品、自動車用外板、および活性エネルギー線硬化性組成物
JP2003206418A (ja) * 2002-01-15 2003-07-22 Toppan Printing Co Ltd 活性エネルギー線硬化ハードコート樹脂組成物およびハードコート層を含む積層体
JP2008081719A (ja) * 2006-08-30 2008-04-10 Kansai Paint Co Ltd 上塗塗料組成物
JP2010181898A (ja) * 2010-03-10 2010-08-19 Dainippon Printing Co Ltd 高精細化デイスプレイ用防眩フィルムの製造方法
JP2014188842A (ja) * 2013-03-27 2014-10-06 Dainippon Printing Co Ltd 化粧シート及びこれを用いた化粧板
CN104070748A (zh) * 2014-05-22 2014-10-01 东莞市纳利光学材料有限公司 磨砂保护膜及其制备方法
CN104070748B (zh) * 2014-05-22 2016-05-11 东莞市纳利光学材料有限公司 磨砂保护膜及其制备方法

Also Published As

Publication number Publication date
JPH0445342B2 (enrdf_load_stackoverflow) 1992-07-24

Similar Documents

Publication Publication Date Title
EP2178654B1 (en) Process of powder coating aluminium substrates
WO2001083627A1 (fr) Composition de revetement a base d'eau durcissable aux rayons d'energie actinique, matiere metallique enduite du film durci de la composition, procede de production, et procede de liaison de la matiere metallique enduite
JPS60106830A (ja) 硬化性組成物
TW201510041A (zh) 水性樹脂組合物、使用其之積層體及圖像顯示裝置
JP2683845B2 (ja) 上塗り塗膜形成方法
JPH01229622A (ja) 高硬度、耐汚染性および防眩性に優れた塗装鋼板およびその製造方法
JPH05309324A (ja) 優れた引っ掻抵抗性および耐衝撃性を有する塗装した鋼板
EP2703447A1 (en) Aqueous composite resin composition and article
JPS6040169A (ja) 塗装金属板の製造方法および塗料組成物
JPH08259644A (ja) 活性エネルギー線硬化型樹脂組成物
JPH0431422A (ja) 活性エネルギー線硬化型樹脂組成物
ES2750610T3 (es) Composiciones filmógenas aptas para curado y método de mitigación de la acumulación de suciedad en un sustrato
JPH07157521A (ja) 活性エネルギー線硬化型樹脂組成物、その硬化物及び硬化物の製造方法
JPS6040170A (ja) 塗装金属板の製造方法および塗料組成物
JP3996636B2 (ja) 耐摩耗傷性コーティング組成物
JP4429199B2 (ja) 複層塗膜形成方法およびこれに用いる塗料
JP3869579B2 (ja) 金属板用水性塗料組成物、および表面処理方法
JPS62152841A (ja) 自動車車体の積層塗膜
JP3723883B2 (ja) 複層塗膜形成法
JPH02242863A (ja) 塗装金属板及びその製造方法及び塗料組成物
JP3894633B2 (ja) 樹脂組成物及びその硬化物
JPS6118583B2 (enrdf_load_stackoverflow)
JPH09136981A (ja) エマルション被覆材組成物
JP2003300010A (ja) 自動車塗膜の補修方法及び基材
JPS60186524A (ja) 自動車用中塗り塗料組成物

Legal Events

Date Code Title Description
FPAY Renewal fee payment (event date is renewal date of database)

Free format text: PAYMENT UNTIL: 20070724

Year of fee payment: 15

FPAY Renewal fee payment (event date is renewal date of database)

Free format text: PAYMENT UNTIL: 20080724

Year of fee payment: 16

EXPY Cancellation because of completion of term
FPAY Renewal fee payment (event date is renewal date of database)

Free format text: PAYMENT UNTIL: 20080724

Year of fee payment: 16