JP2011222531A - 電極表面被膜形成剤 - Google Patents
電極表面被膜形成剤 Download PDFInfo
- Publication number
- JP2011222531A JP2011222531A JP2011159838A JP2011159838A JP2011222531A JP 2011222531 A JP2011222531 A JP 2011222531A JP 2011159838 A JP2011159838 A JP 2011159838A JP 2011159838 A JP2011159838 A JP 2011159838A JP 2011222531 A JP2011222531 A JP 2011222531A
- Authority
- JP
- Japan
- Prior art keywords
- atom
- group
- forming agent
- battery
- lithium
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
Description
項1. 式(I):
項2. 式(II):
で表される少なくとも1種の化合物を含む電極表面被膜形成剤。
項3. 式(III):
で表される少なくとも1種の化合物を含む電極表面被膜形成剤。
項4. 式(I)の部分構造もしくは式(IIa)〜(IIIa)の部分構造をその側鎖に1個以上有する含フッ素繰り返し単位を構成要素とする含フッ素ポリマーからなる電極表面被膜形成剤。
項5. 上記式(I)、(II)および(IIa)においてX1およびX2がともにフッ素原子である項1、2または4記載の電極表面被膜形成剤。
項6. 上記式(I)、(II)および(IIa)においてX1、X2の一方がフッ素原子で、もう一方がトリフルオロメチル基である項1、2または4記載の電極表面被膜形成剤。
項7. 電池作成時または/かつ電池使用時に、電極材料表面に保護膜として作用することを特徴とする項1〜6のいずれかに記載の電極表面被膜形成剤。
項8. 電極がリチウム、リチウムインターカレート化合物またはリチウム合金からなる負極である項7記載の電極表面被膜形成剤。
項9. 項1〜6のいずれかに記載の化合物の少なくとも1種を電解液に添加することを特徴とする電池製造方法。
項10. 項1〜6のいずれかに記載の化合物の少なくとも1種を用いて電池の製造前にあるいは製造過程で負極を処理することを特徴とする電池製造方法。
項11. 負極がリチウム金属、リチウムインターカレート化合物またはリチウム合金である項8または9記載の電池製造方法。
該含フッ素ポリマーは、式(I)、(IIa)、(IIIa)の部分構造を有する繰り返し単位のみからなっていても良いが、該部分構造を有しない繰り返し単位を含んでいても良い。このような式(I)、(IIa)、(IIIa)の部分構造を有しない繰り返し単位としては、−(CF2CF2)−,−(CF2CF(CF3))−,−(CH2CH2)−,−(CH2CH(CH3))−,−(CF2O)−、−(OCF2CF(CF3))−、−(CF2CF2O)−、−(CH2CF2CF2O)−、−(CF2CF2CF2O)−などが例示される。
実施例1
DSC測定はパーキンエルマー製のDSC7を用いた。また、測定用の試料は、チタン製耐圧密閉容器に1M LiPF6/EC+DMC=1:1(vol%)電解液5 μl、ニトリル化合物5 μlをリチウム金属1.3 mgと混合し調整した。昇温速度は5℃/minで行い、発熱反応ピーク温度を測定した。図1は、本発明の化合物との比較例であるジメチルジフルオロマロネートを用いて測定した結果である。また、種々のニトリル化合物を用いて測定した結果を図2〜10に示す。
Claims (7)
- 電池作成時または/かつ電池使用時に、電極材料表面に保護膜として作用することを特徴とする請求項1又は2のいずれかに記載の電極表面被膜形成剤。
- 電極がリチウム金属、リチウムインターカレート化合物またはリチウム合金からなる負極である請求項3記載の電極表面被膜形成剤。
- 請求項1又は2のいずれかに記載の化合物の少なくとも1種を電解液に添加することを特徴とする電池製造方法。
- 請求項1又は2のいずれかに記載の化合物の少なくとも1種を用いて電池の製造前にあるいは製造過程で負極を処理することを特徴とする電池製造方法。
- 負極がリチウム金属、リチウムインターカレート化合物またはリチウム合金である請求項5または6記載の電池製造方法。