JP2011137123A5 - - Google Patents

Download PDF

Info

Publication number
JP2011137123A5
JP2011137123A5 JP2010000191A JP2010000191A JP2011137123A5 JP 2011137123 A5 JP2011137123 A5 JP 2011137123A5 JP 2010000191 A JP2010000191 A JP 2010000191A JP 2010000191 A JP2010000191 A JP 2010000191A JP 2011137123 A5 JP2011137123 A5 JP 2011137123A5
Authority
JP
Japan
Prior art keywords
curing
polymerizable monomer
hydrocarbon group
carbon
carbon atoms
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP2010000191A
Other languages
English (en)
Other versions
JP2011137123A (ja
JP5591543B2 (ja
Filing date
Publication date
Application filed filed Critical
Priority claimed from JP2010000191A external-priority patent/JP5591543B2/ja
Priority to JP2010000191A priority Critical patent/JP5591543B2/ja
Priority to PCT/JP2010/055960 priority patent/WO2010114077A1/ja
Priority to EP10758848.5A priority patent/EP2415751B1/en
Priority to CN201080015370.2A priority patent/CN102365260B/zh
Priority to US13/260,110 priority patent/US8796492B2/en
Priority to KR1020117025161A priority patent/KR101383511B1/ko
Publication of JP2011137123A publication Critical patent/JP2011137123A/ja
Publication of JP2011137123A5 publication Critical patent/JP2011137123A5/ja
Publication of JP5591543B2 publication Critical patent/JP5591543B2/ja
Application granted granted Critical
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Claims (3)

  1. 下記式(1);
    Figure 2011137123
    (式中、Rは、水素原子、若しくは、炭素数3以上の鎖状飽和炭化水素基、炭素数3以上の鎖状不飽和炭化水素基、炭素数3以上の脂環式炭化水素基、炭素数6以上の芳香族炭化水素基、又は、これらの炭化水素基を構成する少なくとも1つの炭素−炭素結合に酸素原子が挿入した構造の基を表し、該炭化水素の水素原子は、ハロゲン原子で置換されていてもよい。)で表されるラジカル重合性単量体であって、
    1333Pa条件下での沸点が95℃以上であることを特徴とするラジカル重合性単量体。
  2. 請求項1に記載のラジカル重合性単量体を硬化させる方法であって、
    該硬化方法は、加熱及び/又は活性エネルギー線の照射により硬化させる工程を含むことを特徴とするラジカル重合性単量体の硬化方法。
  3. 請求項に記載の硬化方法によりラジカル重合性単量体を硬化させて得られることを特徴とする硬化物。
JP2010000191A 2009-03-31 2010-01-04 反応性希釈剤 Active JP5591543B2 (ja)