DE509538C - Verfahren zur Herstellung von Lack - Google Patents
Verfahren zur Herstellung von LackInfo
- Publication number
- DE509538C DE509538C DEA51040D DEA0051040D DE509538C DE 509538 C DE509538 C DE 509538C DE A51040 D DEA51040 D DE A51040D DE A0051040 D DEA0051040 D DE A0051040D DE 509538 C DE509538 C DE 509538C
- Authority
- DE
- Germany
- Prior art keywords
- paint
- production
- parts
- ammonia
- proven
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Description
- Verfahren zur Herstellung von Lack Zusatz zum Patent 4.1o 6oo Vorliegende Erfindung stellt eine Verbesserung des durch Patent 4.io 6oo geschützten Verfahrens zur Herstellung von Lacken dar. Als emulgierender Zusatz wurde bisher entweder verdünntes Ammoniak oder gemäß Patent q.io 6oo bei erhöhter Temperatur Alkali oder Seife verwendet, wodurch bei einigen der verwendeten Öle eine Verseifung eintrat und diese Seife die Rolle der emulgierenden Beimengung übernahm. Es hat sich aber als nicht zweckmäßig erwiesen, größere Mengen Ammoniak als emulgierende Beimengung bei hoher Temperatur zu verwenden, da besondere Mittel vorgesehen werden mußten, um den unerwünschten Verlust " von Ammoniak zu verhindern. Das erwähnte Herstellungsverfahren hat sich als unzweckmäßig erwiesen, besonders wenn der Lack auf elektrolytischem Wege aufgetragen wird.
- Nach der Erfindung wird der auf elektrolytischem Wege aufgebrachte Überzug von Lack dadurch bedeutend verbessert, daß dem Lack gewisse Mengen von Ammoniak zugefügt werden. Zu diesem Zwecke stellt man den Lack zunächst nach dem bekannten Verfahren her, wobei man ein Alkali oder ein alkalisch reagierendes Salz zur Verseifung eines Teiles des Öles dem Lack zusetzt. Der Lack kann z. B. folgende Bestandteile in Gewichtsteilen enthalten: 3oo Teile Asphalt, 75 Teile Harz, i5o Teile gekochtes Holzöl, i 5o Teile gekochtes Leinöl. Dieser Mischung werden noch 7, 5 Teile kohlensaures Natrium hinzugefügt.
- Nach der Lösung des Lackes mit heißem Wasser und nach Abkühlung werden nun noch i bis io o,'o Ammoniak hinzugefügt; besonders gut bewährt sich ein Gehalt von 3,4% Ammoniak. Zum Schluß wird noch so viel Wasser beigegeben, bis die gewünschte Lösung erreicht ist.
Claims (1)
- PATENTANSPRUCH: Weiterausbildung des Patents q. i o 6oo, dadurch gekennzeichnet, daß als emulgierendes Mittel Ammoniak, zweckmäßig nach Abkühlung in vorzugsweise i bis io Gewichtsteilen, zugesetzt wird.