DE1596151A1 - Verfahren zur Herstellung von Sauerstoffelektroden - Google Patents

Verfahren zur Herstellung von Sauerstoffelektroden

Info

Publication number
DE1596151A1
DE1596151A1 DE19651596151 DE1596151A DE1596151A1 DE 1596151 A1 DE1596151 A1 DE 1596151A1 DE 19651596151 DE19651596151 DE 19651596151 DE 1596151 A DE1596151 A DE 1596151A DE 1596151 A1 DE1596151 A1 DE 1596151A1
Authority
DE
Germany
Prior art keywords
salt
silver
production
plate
electrode
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
DE19651596151
Other languages
English (en)
Inventor
Smith Dexter William
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ZF International UK Ltd
Original Assignee
Lucas Industries Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Lucas Industries Ltd filed Critical Lucas Industries Ltd
Publication of DE1596151A1 publication Critical patent/DE1596151A1/de
Pending legal-status Critical Current

Description

Joseph Lucas (Industries) 1b96151
Limited
Great King Street
Birmingham / England 2J>. November 1965
Verfahren zur Herstellung von Sauerstoffelektroden
Eine übliche Silber-Sauerstoffelektrode für eine alkalische Brennstoffzelle kann dadurch leistungsfähiger gemacht werden, daß man ihr Katalysatoren zugibt, durch die die Zahl der verfügbaren freien Elektronen zunimmt; brauchbare Katalysatoren sind Legierungen von Silber mit Kadmium, Indium, Zinn oder Antimon. Es ist jedoch schwierig, solche Katalysatoren unmittelbar mit Silber zu mischen und dann eine poröse Struktur zu erzielen, da die Legierungen nur schwer in Pulverform hergestellt werden können.
Ziel der Erfindung ist, ein geeignetes Verfahren zur Herstellung einer Sauerstoffelektrode zu schaffen, die in alkalischen Brennstoffzellen, aber auch in Misch-Brennstoffzellen benutzt werden kann. Die Misch-Brennstoffzelle kann als eine Brennstoffzelle betrachtet werden, in der die Brennstoffelektrode durch eine Batterieplatte ersetzt ist oder als eine alkalische Batterie, in der eine der Batterieplatten durch eine Sauerstoff elektrode ersetzt ist.
Gemäß der Erfindung wird Silber mit dem Salz eines Metalles, das in Legierung mit Silber Katalysatorwirkung hat, gemischt, wobei das Salz von solcher Art ist, daß es unter Hitze zerfällt
^Jp 1 0 9 8 1 8 / 0 1 |7_
BAD
und das betreffende Metall entsteht, eine Platte aus der Mischung hergestellt und zum Zersetzen des Salzes erhitzt.
In einem Beispiel werden 5o-Volumen-# eines feinen Silberpulvers mit 5o-Volumen-# von Kadmiumformiat vermischt; die Mischung wird bis zum Durchgang durch ein Sieb von I9600 Maschen/cm (35o B.S. mesh) gemahlen. Die Verhältnisse sind so gewählt, daß die am Ende erhaltene Elektrode 25 - Jo % Porosität hat. Die Mischung wird dann bei I500 - 24oo kg/cmc (1o - 15 t.s.i.) zu einer Platte verpreßt.
Die Platte wird in strömendem trockenen Wasserstoff bis zu 3oo C aufgeheizt und für 1-3 Minuten bei dieser Temperatur gehalten. Unter diesen Bedingungen zerfällt das Kadmiumformiat und es bleibt eine poröse Silber-Kadmium-Elektrode zurück. Schließlich wird die Platte unter schnellem Aufheizen von 3oo auf 64o C in ruhender Wasserstoffatmosphäre gesintert, indem sie- 25 bis 35 Minuten bei dieser Temperatur gehalten und dann gekühlt wird.
Eine ähnliche Methode kann mit anderen zersetzbaren Salzen von Kadmium, Indium, Zinn oder Antimon oder mit Mischungen von Salzen des gleichen Metalles oder verschiedener Metalle angewandt werden.
Die Elektrode kann in Verbindung mit einer Wasserstoffelektrode in einer alkalischen Brennstoffzelle oder in Verbindung mit einer Batterieplatte in einer Misch-Brennstoffzelle verwendet werden, von der das bekannteste Beispiel die Zink-Luft-Batterie ist, die eine Zink-Batterieplatte und eine Sauerstoffelektrode verwendet.
Patentansprüche:
1098 18/0187

Claims (2)

1596T5T Patentansprüche:
1. Verfahren zur Herstellung einer Säuerstoffelektrode, dadur*di gekennzeichnet, daß Silber mit dem Salz eines Metalles gemischt wird, das in Legierung mit Silber Katalysatorwirkung hat, wobei das Salz von solcher Art ist, daß es unter Hitze zerfällt und das betreffende Metall entsteht, daß eine Platte aus der Mischung hergestellt und zum Zersetzen des Salzes erhitzt wird.
2. Verfahren nach Anspruch 1, dadurch gekennzeichnet, daß die Platte zum Zersetzen des Salzes in einer strömenden nicht oxydierenden Atmosphäre erhitzt und dann in einer ruhenden nicht oxydierenden Atmosphäre gesintert wird.
BAD ORiGIiNSAL 10 9 8 18/0187 λ
DE19651596151 1965-12-30 1965-11-25 Verfahren zur Herstellung von Sauerstoffelektroden Pending DE1596151A1 (de)