DE1019669B - Konverterboeden fuer Blaskonverter fuer die Stahlherstellung - Google Patents
Konverterboeden fuer Blaskonverter fuer die StahlherstellungInfo
- Publication number
- DE1019669B DE1019669B DEW19470A DEW0019470A DE1019669B DE 1019669 B DE1019669 B DE 1019669B DE W19470 A DEW19470 A DE W19470A DE W0019470 A DEW0019470 A DE W0019470A DE 1019669 B DE1019669 B DE 1019669B
- Authority
- DE
- Germany
- Prior art keywords
- converter
- floors
- steel production
- blow
- converters
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Description
- Konverterböden für Blaskonverter für die Stahlherstellung Konverterböden werden allgemein aus gebranntem, grob gemahlenem Dolomit mit Teerzusatz hergestellt. Die fertiggeformten Böden werden dann bei mäßiger Temperatur, die 750 bis 800° C nicht übersteigen soll, in reduzierend gehaltenen Verbrennungsgasen gebrannt. Der fertige Boden ist eine mäßig porige, harte Masse aus Dolomit und Kohlenstoff, wobei der letztere hauptsächlich das Bindemittel bildet. Der Konverterboden muß im Einsatz, d. h. während des Blasens des Konverters, dem chemischen Angriff des Eisens in Gegenwart von Sauerstoff bei sehr hoher Temperatur, etwa 1700° C, gut widerstehen. Die Abnutzung ist aber bei großen Konvertern doch so erheblich, daß die Böden im Mittel nach fünfzig bis sechzig Chargen verbraucht sind.
- Die vorliegende Erfindung betrifft nun einen Konverterboden für Blaskonverter aus Teerdolomitmasse, dessen Haltbarkeit dadurch gesteigert wird, daß der Blasboden im fertiggebrannten Zustand einen Gehalt an kohlensaurem Kalk aufweist. Während seiner Herstellung beträgt der Zusatz an kohlensaurem Kalk 1 bis 10% der Dolomitmasse. Beim Brennen der Böden liegen die Temperaturen unterhalb von 800° C, so daß also hier die Kohlensäure noch nicht entweicht. Wenn aber die Temperaturen während des Blasens durch die sehr hohen Temperaturen des Stahles im Konverter allmählich auch im Boden ansteigen, entwickelt sich C O_ Gas. Dieses durchdringt die Poren und verwehrt dem Sauerstoff des Blaswindes, der durch die Düsenrohre des Bodens gepreßt wird, den Eintritt in die Bodenmasse. Dadurch wird die vorzeitige Verbrennung des Kohlenstoffes im Dolomit verhindert, und der Boden bleibt bis zum beginnenden Schlacken- oder Eisenangriff dichter.
- Versuche mit solchen erfindungsgemäßen Böden haben ergeben, daß diese eine rund 10% höhere Haltbarkeit aufweisen.
Claims (2)
- PATENTANSPRÜCHE: 1. Aus Teerdolomitmasse hergestellter Blasboden für Stahlwerkskonverter, dadurch gekennzeichnet, daß der Blasboden im fertiggebrannten Zustand einen Gehalt an kohlensaurem Kalk aufweist.
- 2. Konverterboden nach Anspruch 1, dadurch gekennzeichnet, daß während seiner Herstellung der Zusatz an kohlensaurem Kalk 1 bis 10% der Dolomitmasse beträgt.