CN106048680A - 一种手机快充接口通电耐腐蚀的专用镀层 - Google Patents

一种手机快充接口通电耐腐蚀的专用镀层 Download PDF

Info

Publication number
CN106048680A
CN106048680A CN201610584598.2A CN201610584598A CN106048680A CN 106048680 A CN106048680 A CN 106048680A CN 201610584598 A CN201610584598 A CN 201610584598A CN 106048680 A CN106048680 A CN 106048680A
Authority
CN
China
Prior art keywords
mobile phone
layer
corrosion
alloy layer
micron
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201610584598.2A
Other languages
English (en)
Other versions
CN106048680B (zh
Inventor
吴仁杰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SILIKE (SHANGHAI) LOGISTICS CO., LTD.
Original Assignee
Dongguan Plater Hardware Plastic Products Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Dongguan Plater Hardware Plastic Products Co Ltd filed Critical Dongguan Plater Hardware Plastic Products Co Ltd
Priority to CN201610584598.2A priority Critical patent/CN106048680B/zh
Publication of CN106048680A publication Critical patent/CN106048680A/zh
Application granted granted Critical
Publication of CN106048680B publication Critical patent/CN106048680B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种手机快充接口通电耐腐蚀的专用镀层,包括手机快充接口的铜底材,在所述铜底材上依次电镀有第一镀铜层、第二镀镍钨合金层、第三镀钯层、第四镀银钨合金层、第五镀金层、第六镀铑钌合金层。所述第一镀铜层的厚度为0.5‑5.0微米,第二镀镍钨合金层的厚度为0.5‑5.0微米,第三镀钯层的厚度为0.025‑0.5微米,第四镀银钨合金层的厚度为0.5‑5.0微米,第五镀金层的厚度为0.025‑0.5微米,第六镀铑钌合金层的厚度为0.25‑5.0微米。本发明可使充电接口的镀层耐插拔次数增多,耐磨损,更抗腐蚀,延长镀层的使用寿命及提高充电效率。

Description

一种手机快充接口通电耐腐蚀的专用镀层
技术领域
本发明涉及手机的零配件,特别是一种手机快充接口通电耐腐蚀的专用镀层。
背景技术
现今智能手机屏幕大,耗电量大,充电量越来越频繁,一般的手机充电接口之镀层大多为铜上镀镍、镀金,此等工艺的缺点在于耐插拔次数少,使用寿命短。尤其现今的智能手机充电频繁,对电镀层的耐插拔,耐磨损及防腐蚀性能要求提高,因此如何用多层电镀镀层组合,以达到耐插拔,耐磨损,防腐蚀的效果即是急需克服的课题,因此,有必要研发一种新的手机快充接口通电耐腐蚀的专用镀层,以克服上述这些缺陷。
发明内容
为了克服现有技术的不足,本发明的目的在于提供一种镀层耐插拔次数增多、更耐磨损、更防腐蚀的、能延长镀层使用寿命、能提高充电效率的手机快充接口通电耐腐蚀的专用镀层。
本发明解决其技术问题所采用的技术方案是:一种手机快充接口通电耐腐蚀的专用镀层,包括手机快充接口的铜底材,在所述铜底材上依次电镀有第一镀铜层、第二镀镍钨合金层、第三镀钯层、第四镀银钨合金层、第五镀金层、第六镀铑钌合金层。
具体的,所述第一镀铜层的厚度为0.5-5.0微米,第二镀镍钨合金层的厚度为0.5-5.0微米,第三镀钯层的厚度为0.025-0.5微米,第四镀银钨合金层的厚度为0.5-5.0微米,第五镀金层的厚度为0.025-0.5微米,第六镀铑钌合金层的厚度为0.25-5.0微米。
本发明的另一种同样的构思的技术方案是,一种手机快充接口通电耐腐蚀的专用镀层,包括手机快充接口的铜底材,在所述铜底材上依次电镀有第一镀铜层、第二镀镍钨合金层、第三镀金层、第四镀银钨合金层、第五镀金层、第六镀铑钌合金层。
本发明的有益效果是:由于在所述铜底材上依次电镀有第一镀铜层、第二镀镍钨合金层、第三镀钯层、第四镀银钨合金层、第五镀金层、第六镀铑钌合金层,所述铜底材上依次镀铜、镀镍钨合金、镀钯、镀银钨合金、镀金、镀铑钌合金,所以本发明可使充电接口的镀层耐插拔次数增多,耐磨损,更抗腐蚀,延长镀层的使用寿命及提高充电效率。
附图说明
下面结合附图和实施方式对本发明作进一步说明。
图1是本发明的镀层结构示意图。
具体实施方式
参照图1,本发明一种手机快充接口通电耐腐蚀的专用镀层,包括手机快充接口的铜底材1,在所述铜底材上依次电镀有第一镀铜层2、第二镀镍钨合金层3、第三镀钯层4、第四镀银钨合金层5、第五镀金层6、第六镀铑钌合金层7。如图1所示,本发明所设一种手机快充接口通电耐腐蚀的专用镀层,主要是在手机快充接口的铜底材上经过必须的流程先行热脱、抛光、电脱、活化后,依次电镀第一层镀铜以填补铜底材表面的孔洞,第二层镀镍钨合金,镀镍钨合金的优点是耐腐蚀,且具有很强的耐磨性,第三层镀钯,镀钯主要是一种介质令镍钨合金与银钨合金结合性更好,第四层镀银钨合金,镀银钨合金的优点是耐腐蚀,具有很好的热稳定性,不含氰化物,第五层镀金,主要也是一种介质令银钨合金与铑钌合金结合性更好,第六层镀铑钌合金,镀铑钌合金的优点是耐腐蚀,耐磨,抗变色,由以上镀层的组合,提高了镀层的硬度,可使镀层耐磨损、耐腐蚀、抗变色,延长快充接口使用寿命,使产品的镀层耐插拔次数增多,提高镀层使用寿命及充电效率,达到更实用的目的。
具体的方案,所述第一镀铜层的厚度为0.5-5.0微米,第二镀镍钨合金层的厚度为0.5-5.0微米,第三镀钯层的厚度为0.025-0.5微米,第四镀银钨合金层的厚度为0.5-5.0微米,第五镀金层的厚度为0.025-0.5微米,第六镀铑钌合金层的厚度为0.25-5.0微米,在此厚度范围内可达到更好的结合和使用效果。
本发明的另一种同样的构思的技术方案是,一种手机快充接口通电耐腐蚀的专用镀层,包括手机快充接口的铜底材1,在所述铜底材上依次电镀有第一镀铜层2、第二镀镍钨合金层3、第三镀金层4、第四镀银钨合金层5、第五镀金层6、第六镀铑钌合金层7。即所述第三层镀钯层4可改为镀金层,同样可以达到相同的上下结合的效果,使产品的镀层耐插拔次数增多,提高镀层使用寿命及充电效率。
此外,本发明并不局限于上述实施方式,只要其以基本相同的手段达到本发明的技术效果,都应属于本发明的保护范围。

Claims (3)

1.一种手机快充接口通电耐腐蚀的专用镀层,其特征在于:包括手机快充接口的铜底材(1),在所述铜底材上依次电镀有第一镀铜层(2)、第二镀镍钨合金层(3)、第三镀钯层(4)、第四镀银钨合金层(5)、第五镀金层(6)、第六镀铑钌合金层(7)。
2.根据权利要求1所述的手机快充接口通电耐腐蚀的专用镀层,其特征在于:所述第一镀铜层的厚度为0.5-5.0微米,第二镀镍钨合金层的厚度为0.5-5.0微米,第三镀钯层的厚度为0.025-0.5微米,第四镀银钨合金层的厚度为0.5-5.0微米,第五镀金层的厚度为0.025-0.5微米,第六镀铑钌合金层的厚度为0.25-5.0微米。
3.一种手机快充接口通电耐腐蚀的专用镀层,其特征在于:包括手机快充接口的铜底材(1),在所述铜底材上依次电镀有第一镀铜层(2)、第二镀镍钨合金层(3)、第三镀金层(4)、第四镀银钨合金层(5)、第五镀金层(6)、第六镀铑钌合金层(7)。
CN201610584598.2A 2016-07-22 2016-07-22 一种手机快充接口通电耐腐蚀的专用镀层 Expired - Fee Related CN106048680B (zh)