CN101892331A - 一种皮革表面仿古处理方法 - Google Patents

一种皮革表面仿古处理方法 Download PDF

Info

Publication number
CN101892331A
CN101892331A CN2010102367958A CN201010236795A CN101892331A CN 101892331 A CN101892331 A CN 101892331A CN 2010102367958 A CN2010102367958 A CN 2010102367958A CN 201010236795 A CN201010236795 A CN 201010236795A CN 101892331 A CN101892331 A CN 101892331A
Authority
CN
China
Prior art keywords
animal skin
skin blank
leather surface
blank
mixing oil
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2010102367958A
Other languages
English (en)
Inventor
廖顺南
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2010102367958A priority Critical patent/CN101892331A/zh
Publication of CN101892331A publication Critical patent/CN101892331A/zh
Pending legal-status Critical Current

Abstract

本发明涉及一种皮革表面仿古处理方法,包括采用混合油对皮革表面进行处理,混合油包括虫胶、松香、酒精,重量配比为5~25∶5~15∶100,优选虫胶、松香、酒精的重量配比为20∶5∶100。处理步骤,a、先把动物皮胚表层打磨至毛绒状;b、展开动物皮胚喷涂混合油——风干;c、移到烘干房中,在42~47℃温度下烘烤2~3小时;d、常温环境,对动物皮胚上效果底色;e、移到烘干房中烘干;f、将动物皮胚裂纹处理;g、采用混合颜料对动物皮胚上效果色,然后再均匀喷涂一层混合油;h、移到烘干房中烘烤干;i、将动物皮胚拉出裂纹,并打磨、抛光;k、移到烘干房中,在30~40℃温度下烘烤5~7小时;j、产品冷却后,涂皮革保护蜡,制成成品。

Description

一种皮革表面仿古处理方法
技术领域
本发明属于皮革表面处理技术领域,具体涉及一种皮革表面仿古处理方法。
背景技术
随着时尚潮流的变化发展,类似古董之类的旧风格产品越来越受到人们的青睐,然而这类产品毕竟非常有限,难以获得,于是催生了“复古”、“仿古”类家具、服装、工艺品等产品的产生。而作为此类产品的重要原材料一直受到生产工艺的制约,比如仿古皮革,如果处理不好,即破坏皮革强度,也影响视觉效果。
发明内容
本发明的目的在于提供一种皮革表面仿古处理方法,处理后的皮革可以应用于“复古”、“仿古”类家具、服装、工艺品等产品上。
本发明的目的是这样实现的:一种皮革表面仿古处理方法,其特征在于:采用混合油对皮革表面进行处理,所述的混合油包括虫胶、松香、酒精,重量配比为10~20∶5~15∶100。
所述混合油中,虫胶、松香、酒精的重量配比为15∶10∶100。
所述皮革表面处理包括以下步骤:
a、先把动物皮胚表层打磨至毛绒状以增加混合油的附着力;
b、展开动物皮胚,在打磨过的表面均匀喷涂一次混合油,风干15~20分钟后再喷涂一次混合油,放置15~20分钟;
c、移到烘干房中,在42~47℃温度下烘烤2~3小时;
d、动物皮胚移至常温环境,采用混合颜料给动物皮胚上效果底色,然后再均匀喷涂一层混合油;
e、移到烘干房中,在42~47℃温度下烘烤2~3小时;
f、将动物皮胚搓揉出裂纹,使动物皮胚恢复柔软性,采用浓度在95%以上的酒精对动物皮胚进行搓洗,封闭裂纹;
g、采用混合颜料对步骤f得到的动物皮胚上效果色,然后再均匀喷涂一层混合油;
h、移到烘干房中,在42~47℃温度下烘烤2~3小时;
i、将动物皮胚拉出裂纹,并用沙纸和海绵砂布打磨、抛光;
k、移到烘干房中,在30~40℃温度下烘烤5~7小时;
j、产品冷却后,涂皮革保护腊,制成成品。
所述动物皮胚为猪皮皮胚或牛皮皮胚。
所述混合颜料包括黑色精、红棕色精、混合油、酒精,其重量配比为:45~60∶40~55∶1000∶5000~6000。
所述混合颜料包括黑色精、红棕色精、混合油、酒精,其重量配比为:53∶48∶1000∶5500。
本发明的积极效果:采用上述皮革表面仿古处理方法,制作的皮革无论在视觉还是触觉方面都能达到仿古效果,从而可以广泛应用于“复古”、“仿古”类家具、服装、工艺品等产品上。
具体实施方式
本发明所述皮革表面仿古处理方法,采用混合油对皮革表面进行处理,混合油主要由虫胶、松香和酒精组成,重量配比为5~25∶5~15∶100,较理想的重量配比为20∶5∶100。具体的处理步骤包括:
a、先把动物皮胚表层打磨至毛绒状以增加混合油的附着力,较常用的皮革主要是猪皮皮胚和牛皮皮胚;
b、展开动物皮胚,在打磨过的表面均匀喷涂一次混合油,风干15~20分钟后再喷涂一次混合油,放置15~20分钟;
c、移到烘干房中,在42~47℃温度下烘烤2~3小时;
d、动物皮胚移至常温环境,采用混合颜料给动物皮胚上效果底色,然后再均匀喷涂一层混合油;
e、移到烘干房中,在42~47℃温度下烘烤2~3小时;
f、将动物皮胚搓揉出裂纹,使动物皮胚恢复柔软性,采用浓度在95%以上的酒精对动物皮胚进行搓洗,封闭裂纹;
g、采用混合颜料对步骤f得到的动物皮胚上效果色,然后再均匀喷涂一层混合油;
h、移到烘干房中,在42~47℃温度下烘烤2~3小时;
i、将动物皮胚拉出裂纹,并用沙纸和海绵砂布打磨、抛光;
k、移到烘干房中,在30~40℃温度下烘烤5~7小时;
j、产品冷却后,涂皮革保护腊,制成成品。
上述步骤中采用的混合颜料包括黑色精、红棕色精、混合油、酒精,其重量配比为:45~60∶40~55∶1000∶5000~6000,优选为53∶48∶1000∶5500。

Claims (6)

1.一种皮革表面仿古处理方法,其特征在于:采用混合油对皮革表面进行处理,所述的混合油包括虫胶、松香、酒精,重量配比为5~25∶5~15∶100。
2.根据权利要求1所述的皮革表面仿古处理方法,其特征在于:所述混合油中,虫胶、松香、酒精的重量配比为20∶5∶100。
3.根据权利要求1或2所述的皮革表面仿古处理方法,其特征在于:所述皮革表面处理包括以下步骤:
a、先把动物皮胚表层打磨至毛绒状以增加混合油的附着力;
b、展开动物皮胚,在打磨过的表面均匀喷涂一次混合油,风干15~20分钟后再喷涂一次混合油,放置15~20分钟;
c、移到烘干房中,在42~47℃温度下烘烤2~3小时;
d、动物皮胚移至常温环境,采用混合颜料给动物皮胚上效果底色,然后再均匀喷涂一层混合油;
e、移到烘干房中,在42~47℃温度下烘烤2~3小时;
f、将动物皮胚搓揉出裂纹,使动物皮胚恢复柔软性,采用浓度在95%以上的酒精对动物皮胚进行搓洗,封闭裂纹;
g、采用混合颜料对步骤f得到的动物皮胚上效果色,然后再均匀喷涂一层混合油;
h、移到烘干房中,在42~47℃温度下烘烤2~3小时;
i、将动物皮胚拉出裂纹,并用沙纸和海绵砂布打磨、抛光;
k、移到烘干房中,在30~40℃温度下烘烤5~7小时;
j、产品冷却后,涂皮革保护腊,制成成品。
4.根据权利要求3所述的皮革表面仿古处理方法,其特征在于:所述动物皮胚为猪皮皮胚或牛皮皮胚。
5.根据权利要求3所述的皮革表面仿古处理方法,其特征在于:所述混合颜料包括黑色精、红棕色精、混合油、酒精,其重量配比为:45~60∶40~55∶1000∶5000~6000。
6.根据权利要求5所述的皮革表面仿古处理方法,其特征在于:所述混合颜料包括黑色精、红棕色精、混合油、酒精,其重量配比为:53∶48∶1000∶5500。
CN2010102367958A 2010-07-24 2010-07-24 一种皮革表面仿古处理方法 Pending CN101892331A (zh)