WO2012132371A1 - レジストパターンの形成方法およびそれを用いたパターン化基板の製造方法 - Google Patents
レジストパターンの形成方法およびそれを用いたパターン化基板の製造方法 Download PDFInfo
- Publication number
- WO2012132371A1 WO2012132371A1 PCT/JP2012/002034 JP2012002034W WO2012132371A1 WO 2012132371 A1 WO2012132371 A1 WO 2012132371A1 JP 2012002034 W JP2012002034 W JP 2012002034W WO 2012132371 A1 WO2012132371 A1 WO 2012132371A1
- Authority
- WO
- WIPO (PCT)
- Prior art keywords
- resist
- pattern
- substrate
- resist pattern
- forming
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Ceased
Links
Images
Classifications
-
- G—PHYSICS
- G03—PHOTOGRAPHY; CINEMATOGRAPHY; ANALOGOUS TECHNIQUES USING WAVES OTHER THAN OPTICAL WAVES; ELECTROGRAPHY; HOLOGRAPHY
- G03F—PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR
- G03F7/00—Photomechanical, e.g. photolithographic, production of textured or patterned surfaces, e.g. printing surfaces; Materials therefor, e.g. comprising photoresists; Apparatus specially adapted therefor
- G03F7/20—Exposure; Apparatus therefor
-
- G—PHYSICS
- G03—PHOTOGRAPHY; CINEMATOGRAPHY; ANALOGOUS TECHNIQUES USING WAVES OTHER THAN OPTICAL WAVES; ELECTROGRAPHY; HOLOGRAPHY
- G03F—PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR
- G03F7/00—Photomechanical, e.g. photolithographic, production of textured or patterned surfaces, e.g. printing surfaces; Materials therefor, e.g. comprising photoresists; Apparatus specially adapted therefor
- G03F7/20—Exposure; Apparatus therefor
- G03F7/2022—Multi-step exposure, e.g. hybrid; backside exposure; blanket exposure, e.g. for image reversal; edge exposure, e.g. for edge bead removal; corrective exposure
- G03F7/203—Multi-step exposure, e.g. hybrid; backside exposure; blanket exposure, e.g. for image reversal; edge exposure, e.g. for edge bead removal; corrective exposure comprising an imagewise exposure to electromagnetic radiation or corpuscular radiation
-
- G—PHYSICS
- G03—PHOTOGRAPHY; CINEMATOGRAPHY; ANALOGOUS TECHNIQUES USING WAVES OTHER THAN OPTICAL WAVES; ELECTROGRAPHY; HOLOGRAPHY
- G03F—PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR
- G03F7/00—Photomechanical, e.g. photolithographic, production of textured or patterned surfaces, e.g. printing surfaces; Materials therefor, e.g. comprising photoresists; Apparatus specially adapted therefor
- G03F7/004—Photosensitive materials
- G03F7/039—Macromolecular compounds which are photodegradable, e.g. positive electron resists
- G03F7/0392—Macromolecular compounds which are photodegradable, e.g. positive electron resists the macromolecular compound being present in a chemically amplified positive photoresist composition
-
- G—PHYSICS
- G03—PHOTOGRAPHY; CINEMATOGRAPHY; ANALOGOUS TECHNIQUES USING WAVES OTHER THAN OPTICAL WAVES; ELECTROGRAPHY; HOLOGRAPHY
- G03F—PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR
- G03F7/00—Photomechanical, e.g. photolithographic, production of textured or patterned surfaces, e.g. printing surfaces; Materials therefor, e.g. comprising photoresists; Apparatus specially adapted therefor
- G03F7/20—Exposure; Apparatus therefor
- G03F7/2051—Exposure without an original mask, e.g. using a programmed deflection of a point source, by scanning, by drawing with a light beam, using an addressed light or corpuscular source
- G03F7/2059—Exposure without an original mask, e.g. using a programmed deflection of a point source, by scanning, by drawing with a light beam, using an addressed light or corpuscular source using a scanning corpuscular radiation beam, e.g. an electron beam
-
- G—PHYSICS
- G03—PHOTOGRAPHY; CINEMATOGRAPHY; ANALOGOUS TECHNIQUES USING WAVES OTHER THAN OPTICAL WAVES; ELECTROGRAPHY; HOLOGRAPHY
- G03F—PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR
- G03F7/00—Photomechanical, e.g. photolithographic, production of textured or patterned surfaces, e.g. printing surfaces; Materials therefor, e.g. comprising photoresists; Apparatus specially adapted therefor
- G03F7/26—Processing photosensitive materials; Apparatus therefor
- G03F7/30—Imagewise removal using liquid means
- G03F7/32—Liquid compositions therefor, e.g. developers
-
- G—PHYSICS
- G03—PHOTOGRAPHY; CINEMATOGRAPHY; ANALOGOUS TECHNIQUES USING WAVES OTHER THAN OPTICAL WAVES; ELECTROGRAPHY; HOLOGRAPHY
- G03F—PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR
- G03F7/00—Photomechanical, e.g. photolithographic, production of textured or patterned surfaces, e.g. printing surfaces; Materials therefor, e.g. comprising photoresists; Apparatus specially adapted therefor
- G03F7/26—Processing photosensitive materials; Apparatus therefor
- G03F7/30—Imagewise removal using liquid means
- G03F7/32—Liquid compositions therefor, e.g. developers
- G03F7/322—Aqueous alkaline compositions
-
- H—ELECTRICITY
- H10—SEMICONDUCTOR DEVICES; ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- H10P—GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10P76/00—Manufacture or treatment of masks on semiconductor bodies, e.g. by lithography or photolithography
- H10P76/20—Manufacture or treatment of masks on semiconductor bodies, e.g. by lithography or photolithography of masks comprising organic materials
- H10P76/204—Manufacture or treatment of masks on semiconductor bodies, e.g. by lithography or photolithography of masks comprising organic materials of organic photoresist masks
- H10P76/2041—Photolithographic processes
Definitions
- the present invention relates to a method of forming a resist pattern having a predetermined uneven pattern and a method of manufacturing a patterned substrate using the same.
- Nanoimprint is a pattern formation technology developed from the embossing technology. Specifically, the nanoimprint presses a mold (generally referred to as a mold, a stamper, or a template) on which a concavo-convex pattern is formed against a nanoimprint resist coated on a processing substrate to mechanically deform or flow the nanoimprint resist. Technology that precisely transfers fine patterns.
- Patent Document 1 As an example in which nanoimprinting is applied to formation of a circuit pattern of a semiconductor device, for example, Patent Document 1 can be mentioned.
- the range of the line width of the circuit pattern of the semiconductor device ranges from, for example, several tens of nm to several um.
- the concavo-convex pattern of the mold is manufactured by etching the surface of the substrate which is the basis of the mold, using as a mask the resist film on which the concavo-convex pattern corresponding to the circuit pattern is formed. Therefore, the range of the line width of the concavo-convex pattern formed in the resist film naturally becomes a wide range corresponding to the above range.
- Patent Document 1 in consideration of the above circumstances, the spot electron beam drawing apparatus in the first drawing area where the line width of the drawing pattern is 100 nm or less, and the variable shaped electron beam in the second drawing area where the line width is larger than 100 nm.
- the drawing apparatus discloses that a drawing pattern corresponding to a circuit pattern is drawn on a resist film. According to the method of Patent Document 1, the pattern of the first drawing area can be drawn with high accuracy, and the processing capability of the entire drawing process can be improved.
- the present invention has been made in view of the above problems, and in the formation of a resist pattern including a layout having a minimum line width of 100 nm or less, preventing deviation from the design of a drawing pattern due to a switching operation of a drawing apparatus. It is an object of the present invention to provide a method of forming a resist pattern that can be used.
- the present invention has an object to provide a method of manufacturing a patterned substrate capable of improving the processing accuracy of a concavo-convex pattern corresponding to the resist pattern in the manufacture of a patterned substrate which is etched using a resist pattern as a mask. It is said that.
- the formation method of the resist pattern concerning the present invention is: In a method of forming a resist pattern including a layout having a minimum line width of 100 nm or less, Form a resist film on the substrate, After the drawing pattern is drawn on the resist film by the variable-shaped electron beam, paddle development is performed on the resist film so that the film reduction rate of the resist non-dissolved portion of the resist film becomes 20% or less. is there.
- the "minimum line width” means the minimum line width in the pattern layout.
- Resist non-dissolving portion means, in the case of a positive resist, a portion of the resist film in a region which is not influenced by the electron beam for writing at all, and in the case of a negative resist, the portion of the electron beam for writing. The portion of the resist film in the affected area is meant.
- the “film reduction rate” means the ratio of the thickness difference after development at the same place to the thickness before development of the resist non-dissolved portion of the resist film.
- the developing time for paddle development is preferably 15 to 60 s.
- the dilution concentration of the developer for paddle development is preferably 20 to 90%.
- the temperature during paddle development is preferably 2 to 20 ° C.
- the developer for paddle development preferably does not contain an activator.
- the resist preferably contains a compound represented by the following structural formula (1) or a compound represented by the following structural formula (2).
- R 01 , R 02 and R 03 each independently represent, for example, a hydrogen atom, an alkyl group, a cycloalkyl group, a halogen atom, a cyano group or an alkoxycarbonyl group.
- Ar 1 represents, for example, an aromatic ring group.
- R 03 and Ar 1 may be an alkylene group, and the two may be combined with each other to form a 5- or 6-membered ring together with the —C—C— chain.
- Each of n Y's independently represents a hydrogen atom or a group capable of leaving by the action of an acid. However, at least one of Y represents a group capable of leaving by the action of an acid.
- n represents an integer of 1 to 4, preferably 1 to 2, and more preferably 1.
- A represents a hydrogen atom, an alkyl group, a cycloalkyl group, a halogen atom or a cyano group.
- R represents a halogen atom, an alkyl group, a cycloalkyl group, an aryl group, an alkenyl group, an aralkyl group, an alkoxy group, an alkylcarbonyloxy group or an alkylsulfonyloxy group, and when there are plural groups, they may be the same or different. You may combine with each other to form a ring.
- a represents an integer of 1 to 3;
- b represents an integer of 0 to (3-a).
- a resist pattern is formed on a substrate by the method described above, By etching the substrate using the resist film on which the resist pattern is formed as a mask, a concavo-convex pattern corresponding to the resist pattern is formed on the surface of the substrate.
- a resist film is formed on a substrate and a drawing pattern is drawn on the resist film with a variable shaping electron beam. Thereafter, paddle development is performed on the resist film so that the film reduction rate of the resist non-dissolved portion of the resist film becomes 20% or less.
- the inventors of the present invention have found that if the film reduction rate of the resist non-dissolved portion of the resist film is 20% or less, the resist film drawn by the electron beam in the foot region (a region where the intensity profile of the electron beam is tailed) It has been found that parts can be prevented from being completely removed by development.
- a resist pattern having a desired line width can be formed.
- a layout with a minimum line width of 100 nm or less is included. In the formation of the resist pattern, it is possible to prevent the deviation from the design of the drawing pattern due to the switching operation of the drawing apparatus.
- a resist pattern is formed on the substrate by the method described above, and the substrate is etched using the resist film on which the resist pattern is formed as a mask to form a resist pattern.
- a corresponding uneven pattern is formed on the surface of the substrate. Therefore, when drawing a resist film, it is possible to prevent a deviation from the design of the drawing pattern caused by the switching operation of the drawing apparatus.
- the manufacture of a patterned substrate which is etched using a resist pattern as a mask it becomes possible to improve the processing accuracy of the concavo-convex pattern corresponding to the resist pattern.
- FIG. 1 is a schematic cross-sectional view for explaining the relationship between the intensity profile of an electron beam and the writing of a resist film.
- a resist is applied on a substrate to form a resist film, and a drawing pattern including a layout with a minimum line width of 100 nm or less is drawn on the resist film by a variable shaped electron beam.
- the puddle development is carried out on the resist film so that the film reduction rate of the resist non-dissolved portion of the resist film is 20% or less.
- the substrate 3 is a substrate that is a base of a patterned substrate on the surface of which a concavo-convex pattern is formed.
- the substrate 3 is patterned by a method of manufacturing a patterned substrate described later to be a patterned substrate.
- the shape, structure, size, material, and the like of the substrate 3 are not particularly limited, and can be appropriately selected according to the purpose.
- the uneven pattern forming surface of the substrate 3 is a surface to which a resist is applied.
- the substrate 3 may be a 6 inch silicon wafer or a 6025 mask blank.
- the structure may be a single layer structure or a laminated structure.
- a material it can select suitably from what is well-known as a substrate material, For example, metal materials, such as silicon, nickel, aluminum, glass materials, such as quartz, resin, etc. are mentioned. These substrate materials may be used alone or in combination of two or more. There is no restriction
- the substrate 3 preferably has one or more mask layers on the surface to which the resist is applied.
- the substrate 3 is composed of a support substrate 3a and a mask layer 3b.
- the mask layer 3 b functions as a mask when the support substrate 3 a is etched as described later.
- the material of the mask layer 3b is selected from materials which reduce the etching selectivity of the mask layer 3b to the support substrate 3a.
- the material of the mask layer 3b is preferably a metal material such as chromium, tungsten, titanium, nickel, silver, platinum or gold, and a metal oxide material such as chromium oxide, tungsten oxide or titanium oxide.
- the mask layer 3 b preferably has at least one layer containing chromium and / or chromium oxide.
- the surface of the substrate 3 may be subjected to surface treatment with a silane coupling agent, HMDS (hexamethylzine lazan), or the like in order to enhance the adhesion to the resist.
- a silane coupling agent HMDS (hexamethylzine lazan), or the like in order to enhance the adhesion to the resist.
- the resist film 2 is made of a chemically amplified resist which becomes soluble in a developer by irradiation of an electron beam.
- the resist film 2 is formed, for example, by spin coating a resist solution on the substrate 3.
- the resist as described above is not particularly limited, but in particular, PRL 009 (trade name) manufactured by Fujifilm Electronics Materials Co., Ltd., a compound represented by the following structural formula (1) and the following structural formula (2) Resin containing the compound etc. which are represented can be used suitably.
- R 01 , R 02 and R 03 each independently represent, for example, a hydrogen atom, an alkyl group, a cycloalkyl group, a halogen atom, a cyano group or an alkoxycarbonyl group.
- Ar 1 represents, for example, an aromatic ring group.
- R 03 and Ar 1 may be an alkylene group, and the two may be combined with each other to form a 5- or 6-membered ring together with the —C—C— chain.
- Each of n Y's independently represents a hydrogen atom or a group capable of leaving by the action of an acid. However, at least one of Y represents a group capable of leaving by the action of an acid.
- n represents an integer of 1 to 4, preferably 1 to 2, and more preferably 1.
- A represents a hydrogen atom, an alkyl group, a cycloalkyl group, a halogen atom or a cyano group.
- R represents a halogen atom, an alkyl group, a cycloalkyl group, an aryl group, an alkenyl group, an aralkyl group, an alkoxy group, an alkylcarbonyloxy group or an alkylsulfonyloxy group, and when there are plural groups, they may be the same or different. You may combine with each other to form a ring.
- a represents an integer of 1 to 3;
- b represents an integer of 0 to (3-a).
- the drawing of the drawing pattern is performed using a variable-shaped electron beam drawing apparatus.
- the variable-shaped electron beam drawing apparatus changes the electron beam shape into a rectangle by transmitting an electron beam emitted from an electron gun (emitter) through a rectangular hole called a forming aperture, and synchronizes it with the movement of the xy stage. It is an apparatus which performs pattern irradiation by continuously irradiating a shaped electron beam. In the variable-shaped electron beam drawing apparatus, it is possible to adjust the electron beam irradiation range of various shapes by changing the transmission area of the hole of the forming aperture.
- variable-shaped electron beam drawing apparatus Since the variable-shaped electron beam drawing apparatus has a drawing processing capability that is about 100 times higher than that of the spot electron beam drawing apparatus, the drawing process is performed using only the variable-shaped electron beam drawing apparatus as a whole drawing process Processing capacity can be significantly improved.
- the resist film is drawn by an electron beam formed in accordance with the designed width of the line width at each point of the drawing pattern.
- a drawing apparatus called EBM-6000 manufactured by New Flare Technology Co., Ltd. can be used.
- the development of the resist is carried out by paddle development.
- the developer is supplied to the surface of the resist film on the substrate, and the entire surface of the resist film is covered with the developer using its surface tension, and then the supply of the developer is stopped and the substrate is
- This is a method of developing the resist film while keeping the substrate stationary or rotating the substrate at such a low speed that the developer does not scatter from the resist film.
- the developing solution is removed by rinsing with pure water or the like.
- the developer may be supplied a plurality of times.
- the first scan of the developer supply means is performed on the surface of the resist film so that the developer covers the entire surface of the resist film, and then the second scan is performed after a predetermined time has elapsed. You may do it.
- the number of scans is not particularly limited.
- a developing device called MaskTrack made by HamaTech can be used.
- the film reduction rate means the ratio of the thickness difference after development at the same place to the thickness before development of the resist non-dissolved portion of the resist film. That is, when the thickness before developing of the resist non-dissolved portion of the resist film is A, and the thickness after developing the resist non-dissolved portion at the same place is B, the film reduction ratio is (A ⁇ B) / A expressed.
- the film reduction rate is adjusted by appropriately adjusting the conditions in paddle development.
- the conditions for paddle development include, for example, development time (time for exposing resist to developer), concentration of developer, presence or absence of activator in developer, temperature of liquid during development, and supply means for supplying developer. It is the number of scans, etc.
- development time time for exposing resist to developer
- concentration of developer concentration of developer
- presence or absence of activator in developer concentration of developer
- temperature of liquid during development and supply means for supplying developer. It is the number of scans, etc.
- TMAH tetramethylammonium hydroxide
- NMD-3 a developing solution without an activating agent than an activating agent-containing developing solution NMD-W manufactured by Tokyo Ohka Kogyo Co., Ltd.
- the developing time is preferably 15 to 60 s
- the diluted concentration of the developer is preferably 20 to 90%
- the developer temperature during paddle development is 2 to 20 ° C. Is preferred.
- the number of scans of the supply means for supplying the developing solution is preferably once or twice because development is preferably performed while maintaining the developing solution in a static state as described later.
- variable shaped electron beam EB is formed into a rectangular shape by a forming aperture, but the intensity profile of the electron beam EB has a slight foot in the rectangular outer region (FIG. 1). Therefore, resist film 2 is drawn by electron beam EBa in the forming region Ra having a relatively uniform intensity profile and electron beam EBb in the foot region Rb. Since the width of the forming area Ra is normally designed to match the line width of the drawing pattern, the portion 2a of the resist film 2 drawn by the electron beam EBa of the forming area Ra is the desired line width of the drawing pattern. Therefore, in order to obtain a drawing pattern as designed using the variable shaped electron beam EB, it is important to develop so as to leave the portion 2b of the resist film 2 drawn by the electron beam EBb in the foot region Rb. .
- the inventor of the present invention has found that the film reduction rate of the resist non-dissolved portion 2c of the resist film 2 is effective as an index indicating the progress of development. Then, if development is performed so that the film reduction rate is 20% or less, it is confirmed that the portion 2b drawn by the electron beam EBb of the foot region Rb of the resist film 2 can be prevented from being completely removed by development. It was done. When paddle development is actually performed, the relationship between the film reduction rate and the development conditions is acquired using a resist film not drawn in advance.
- a resist pattern having a desired line width can be formed even when a drawing pattern including a layout having a minimum line width of 100 nm or less is drawn using variable shaped electron beams. it can.
- a layout with a minimum line width of 100 nm or less is included. In the formation of the resist pattern, it is possible to prevent the deviation from the design of the drawing pattern due to the switching operation of the drawing apparatus.
- variable shaped electron beam drawing apparatus having high processing capability of drawing processing performs drawing
- the processing capacity as the entire drawing processing is also compared to the method of Patent Document 1. It can be improved more.
- Method of manufacturing patterned substrate Next, an embodiment of the method for producing a patterned substrate of the present invention will be described.
- the patterned substrate is manufactured using the method for forming a resist pattern described above.
- a resist film on which a predetermined concavo-convex pattern is formed is formed on a substrate using the method for forming a resist pattern described above.
- the substrate is etched using the patterned resist film as a mask, and a concavo-convex pattern corresponding to the concavo-convex pattern formed on the resist film is formed on the substrate to form a pattern having a predetermined concavo-convex pattern on the surface Get the substrate.
- the patterned substrate is used as a mold for nanoimprinting itself or as a master for producing such a mold.
- the resist film 2 on which a predetermined concavo-convex pattern is formed is used as the mask layer 3b using the resist pattern forming method described above. Forming on the attached substrate 3. Next, dry etching is performed using the resist film 2 as a mask, and a concavo-convex pattern corresponding to the concavo-convex pattern formed in the resist film 2 is formed on the mask layer 3 b, and the mask layer 3 b is used as an etch stop layer to form a substrate 3. Further, dry etching is performed to form a concavo-convex pattern on the substrate 3 to obtain a patterned substrate having a predetermined concavo-convex pattern on the surface.
- the dry etching is not particularly limited as long as it can form a concavo-convex pattern on the substrate, and can be appropriately selected according to the purpose.
- RIE reactive ion etching
- ion milling ion milling
- sputter etching etc.
- RIE reactive ion etching
- ion milling ion milling
- a fluorine-based gas or a chlorine-based gas can be used as an etchant for RIE.
- the mold 1 obtained by the above-described manufacturing method is composed of a support 12 and a fine uneven pattern 13 formed on the surface of the support 12.
- the material of the support 12 may be, for example, metal materials such as silicon, nickel, aluminum, chromium, iron, tantalum and tungsten, and oxides, nitrides and carbides thereof. Specifically, silicon oxide, aluminum oxide, quartz glass, Pyrex (registered trademark) glass, soda glass, and the like can be given as the material of the support portion 12.
- the shape of the concavo-convex pattern 13 is not particularly limited, and is appropriately selected according to the application of the nanoimprint.
- a line & space pattern as shown in FIGS. 2A and 2B as a typical pattern.
- the length of the convex portion of the line & space pattern, the width W1 of the convex portion, the distance W2 between the convex portions, and the height (depth of the concave portion) H from the bottom of the concave portion are appropriately set.
- the width W1 of the projections is 10 to 100 nm, more preferably 20 to 70 nm
- the distance W2 between the projections is 10 to 500 nm, more preferably 20 to 100 nm
- the height H of the projections is 10 to It is 500 nm, more preferably 30 to 100 nm.
- the shape of the concavo-convex pattern 13 may be a shape in which dots having cross sections such as a rectangle, a circle, and an ellipse are arrayed.
- FIG. 3 is a graph showing the relationship between the developing conditions and the film reduction rate.
- the item "paddle development (4 times)" is that the development method is paddle development, the number of times of developer supply is four times, and the developer is TMAH 2.38% containing an activator, It is data in case the temperature of a developing solution is 23 ° C.
- the item “paddle development (twice)” is that the development method is paddle development, the number of times of developer supply is two, the developer is TMAH 2.38% containing an activator, and the temperature of the developer Is data at 23 ° C.
- the item “paddle development (one time)” is that the development method is paddle development, the number of times of developer supply is one, the developer is TMAH 2.38% containing an activator, and the temperature of the developer Is data at 23 ° C.
- the development method is paddle development, the number of times of developer supply is one, the developer is TMAH 2.38% without activator, and the temperature of the developer is 23 ° C.
- the developing method is paddle development, the number of times of supply of the developer is one, the developer is 2.38% of TMAH containing an activator, and the temperature of the developer is 10 ° C. It is data in a certain case.
- the development method is paddle development and the number of times of supply of the developer is one, and the developer is a rinse of the developer containing 2.38% TMAH and activator and pure water. It is data in the case of the dilution developing solution which mixed the solution by equal volume, and the temperature of a developing solution is 23 ° C.
- Example 1 A resist was applied on the substrate, a predetermined line & space pattern was drawn using a variable shaped electron beam (VSB), and then the resist film was developed. Then, it was examined to what extent resolution (minimum line width of a line & space pattern when a practically preferable pattern could be formed) could be obtained under the conditions.
- the resist is compound A represented by the above structural formula (1)
- the developing solution is TMAH 2.38% containing an activator
- the developing method is paddle development with a single supply of the developing solution
- the developing solution is The temperature is 23 ° C.
- the development time is 30 seconds.
- Example 2 The second embodiment is the same as the first embodiment except that the developing time is 15 seconds.
- Example 3 is the same as Example 2 except that the developer does not contain an activator.
- Example 4 is the same as Example 2 except that the temperature of the developer is 10 ° C.
- Example 5 is the same as Example 2 except that the concentration of TMAH in the developer is 1.19% and the development time is 30 seconds.
- Example 4 is the same as Example 1 except that the number of times of supply of the developer in paddle development is four and the development time is 60 seconds.
- Comparative Example 2 Comparative Example 1 is the same as Comparative Example 1 except that the developing method is spray development.
- Comparative Example 3 Comparative Example 2 is the same as Comparative Example 2 except that the resist is PRL 009 described above.
- Table 1 shows developing conditions and resolutions of the above-mentioned Examples 1 to 5 and Comparative Examples 1 to 3. As a result, under development conditions where the film reduction ratio of the resist non-dissolved portion of the resist film is 20% or less, it is possible to form a resist pattern including a layout with a minimum line width of 100 nm or less with only variable shaped electron beams It was confirmed that there is.
Landscapes
- Physics & Mathematics (AREA)
- General Physics & Mathematics (AREA)
- Spectroscopy & Molecular Physics (AREA)
- Electromagnetism (AREA)
- Health & Medical Sciences (AREA)
- Toxicology (AREA)
- Photosensitive Polymer And Photoresist Processing (AREA)
- Exposure And Positioning Against Photoresist Photosensitive Materials (AREA)
- Preparing Plates And Mask In Photomechanical Process (AREA)
- Exposure Of Semiconductors, Excluding Electron Or Ion Beam Exposure (AREA)
Priority Applications (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| KR1020137028208A KR20140018956A (ko) | 2011-03-30 | 2012-03-23 | 레지스트 패턴의 형성 방법 및 그것을 사용한 패턴화 기판의 제조 방법 |
| US14/040,171 US20140030656A1 (en) | 2011-03-30 | 2013-09-27 | Method for forming resist patterns and method for producing patterned substrates |
Applications Claiming Priority (2)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP2011-075219 | 2011-03-30 | ||
| JP2011075219A JP2012208396A (ja) | 2011-03-30 | 2011-03-30 | レジストパターンの形成方法およびそれを用いたパターン化基板の製造方法 |
Related Child Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| US14/040,171 Continuation US20140030656A1 (en) | 2011-03-30 | 2013-09-27 | Method for forming resist patterns and method for producing patterned substrates |
Publications (1)
| Publication Number | Publication Date |
|---|---|
| WO2012132371A1 true WO2012132371A1 (ja) | 2012-10-04 |
Family
ID=46930148
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| PCT/JP2012/002034 Ceased WO2012132371A1 (ja) | 2011-03-30 | 2012-03-23 | レジストパターンの形成方法およびそれを用いたパターン化基板の製造方法 |
Country Status (5)
| Country | Link |
|---|---|
| US (1) | US20140030656A1 (enExample) |
| JP (1) | JP2012208396A (enExample) |
| KR (1) | KR20140018956A (enExample) |
| TW (1) | TW201250777A (enExample) |
| WO (1) | WO2012132371A1 (enExample) |
Families Citing this family (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| CA2858277A1 (en) * | 2011-12-16 | 2013-06-20 | Heron Energy Pte Ltd | High speed turbine |
| US9921467B2 (en) * | 2015-11-30 | 2018-03-20 | Taiwan Semiconductor Manufacturing Company Ltd. | Mask blank and mask and fabrication method thereof |
Citations (14)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH05198495A (ja) * | 1991-06-04 | 1993-08-06 | Sony Corp | 現像方法及び現像装置 |
| JPH09190963A (ja) * | 1996-01-10 | 1997-07-22 | Canon Inc | マスク及びこれを用いたデバイス生産方法や露光装置 |
| JP2001056558A (ja) * | 1999-08-20 | 2001-02-27 | Tokyo Ohka Kogyo Co Ltd | 化学増幅型ポジ型レジスト組成物及びそれを用いたレジストパターン形成方法 |
| JP2004177929A (ja) * | 2002-09-30 | 2004-06-24 | Sumitomo Chem Co Ltd | 化学増幅型ポジ型レジスト組成物 |
| JP2004333549A (ja) * | 2003-04-30 | 2004-11-25 | Tokyo Ohka Kogyo Co Ltd | ポジ型レジスト組成物およびレジストパターン形成方法 |
| JP2005037414A (ja) * | 2003-05-16 | 2005-02-10 | Tokyo Ohka Kogyo Co Ltd | ネガ型ホトレジスト組成物 |
| JP2005114919A (ja) * | 2003-10-06 | 2005-04-28 | Tokyo Ohka Kogyo Co Ltd | レジスト積層体およびパターン形成方法 |
| JP2006285075A (ja) * | 2005-04-04 | 2006-10-19 | Shin Etsu Chem Co Ltd | レジスト材料並びにこれを用いたパターン形成方法 |
| JP2007055991A (ja) * | 2005-07-25 | 2007-03-08 | Tokyo Ohka Kogyo Co Ltd | 化合物およびその製造方法、低分子化合物、ポジ型レジスト組成物およびレジストパターン形成方法 |
| JP2008162970A (ja) * | 2006-12-28 | 2008-07-17 | Hitachi Ltd | 化合物、ネガ型レジスト組成物およびパターン形成方法 |
| JP2010134240A (ja) * | 2008-12-05 | 2010-06-17 | Jsr Corp | レジストパターン形成方法及びレジストパターン形成用現像液 |
| JP2010271501A (ja) * | 2009-05-20 | 2010-12-02 | Tokyo Ohka Kogyo Co Ltd | ポジ型レジスト組成物、レジストパターン形成方法、高分子化合物 |
| JP2011071170A (ja) * | 2009-09-24 | 2011-04-07 | Toppan Printing Co Ltd | パターン形成方法及びパターン形成装置 |
| JP2011124352A (ja) * | 2009-12-10 | 2011-06-23 | Tokyo Electron Ltd | 現像処理方法、プログラム及びコンピュータ記憶媒体 |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JP3848930B2 (ja) * | 2003-03-24 | 2006-11-22 | 東京エレクトロン株式会社 | 現像処理方法および現像処理装置 |
-
2011
- 2011-03-30 JP JP2011075219A patent/JP2012208396A/ja not_active Abandoned
-
2012
- 2012-03-23 WO PCT/JP2012/002034 patent/WO2012132371A1/ja not_active Ceased
- 2012-03-23 KR KR1020137028208A patent/KR20140018956A/ko not_active Ceased
- 2012-03-29 TW TW101110953A patent/TW201250777A/zh unknown
-
2013
- 2013-09-27 US US14/040,171 patent/US20140030656A1/en not_active Abandoned
Patent Citations (14)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH05198495A (ja) * | 1991-06-04 | 1993-08-06 | Sony Corp | 現像方法及び現像装置 |
| JPH09190963A (ja) * | 1996-01-10 | 1997-07-22 | Canon Inc | マスク及びこれを用いたデバイス生産方法や露光装置 |
| JP2001056558A (ja) * | 1999-08-20 | 2001-02-27 | Tokyo Ohka Kogyo Co Ltd | 化学増幅型ポジ型レジスト組成物及びそれを用いたレジストパターン形成方法 |
| JP2004177929A (ja) * | 2002-09-30 | 2004-06-24 | Sumitomo Chem Co Ltd | 化学増幅型ポジ型レジスト組成物 |
| JP2004333549A (ja) * | 2003-04-30 | 2004-11-25 | Tokyo Ohka Kogyo Co Ltd | ポジ型レジスト組成物およびレジストパターン形成方法 |
| JP2005037414A (ja) * | 2003-05-16 | 2005-02-10 | Tokyo Ohka Kogyo Co Ltd | ネガ型ホトレジスト組成物 |
| JP2005114919A (ja) * | 2003-10-06 | 2005-04-28 | Tokyo Ohka Kogyo Co Ltd | レジスト積層体およびパターン形成方法 |
| JP2006285075A (ja) * | 2005-04-04 | 2006-10-19 | Shin Etsu Chem Co Ltd | レジスト材料並びにこれを用いたパターン形成方法 |
| JP2007055991A (ja) * | 2005-07-25 | 2007-03-08 | Tokyo Ohka Kogyo Co Ltd | 化合物およびその製造方法、低分子化合物、ポジ型レジスト組成物およびレジストパターン形成方法 |
| JP2008162970A (ja) * | 2006-12-28 | 2008-07-17 | Hitachi Ltd | 化合物、ネガ型レジスト組成物およびパターン形成方法 |
| JP2010134240A (ja) * | 2008-12-05 | 2010-06-17 | Jsr Corp | レジストパターン形成方法及びレジストパターン形成用現像液 |
| JP2010271501A (ja) * | 2009-05-20 | 2010-12-02 | Tokyo Ohka Kogyo Co Ltd | ポジ型レジスト組成物、レジストパターン形成方法、高分子化合物 |
| JP2011071170A (ja) * | 2009-09-24 | 2011-04-07 | Toppan Printing Co Ltd | パターン形成方法及びパターン形成装置 |
| JP2011124352A (ja) * | 2009-12-10 | 2011-06-23 | Tokyo Electron Ltd | 現像処理方法、プログラム及びコンピュータ記憶媒体 |
Non-Patent Citations (2)
| Title |
|---|
| TAKERU OKADA ET AL.: "Enhanced resolution and groove-width simulation in cold development of ZEP520A", JOURNAL OF VACUUM SCIENCE AND TECHNOLOGY B, vol. 29, no. ISS.2, 28 March 2011 (2011-03-28), pages 021604-1- - 021604-5 * |
| TOSHIYUKI YOSHIMURA ET AL.: "Confirmation of acid-diffusion mechanism in negative-type chemical amplification resists", EXTENDED ABSTRACTS, JAPAN SOCIETY OF APPLIED PHYSICS AND RELATED SOCIETIES 1996 SPRING 2, March 1996 (1996-03-01), pages 564 * |
Also Published As
| Publication number | Publication date |
|---|---|
| TW201250777A (en) | 2012-12-16 |
| JP2012208396A (ja) | 2012-10-25 |
| KR20140018956A (ko) | 2014-02-13 |
| US20140030656A1 (en) | 2014-01-30 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US7851135B2 (en) | Method of forming an etching mask pattern from developed negative and positive photoresist layers | |
| JP5359430B2 (ja) | パターン形成方法、インプリントモールド及びフォトマスク | |
| CN106324998B (zh) | 光刻图形的形成方法 | |
| US20110171585A1 (en) | Photolithography Method | |
| US20100086877A1 (en) | Pattern forming method and pattern form | |
| KR101295414B1 (ko) | 다계조 포토마스크의 제조 방법 및 패턴 전사 방법 | |
| JP2009080421A (ja) | マスクブランク、及びインプリント用モールドの製造方法 | |
| TW201802573A (zh) | 具有多層遮光層的光罩 | |
| US8507184B2 (en) | Method of manufacturing semiconductor device | |
| JP5682202B2 (ja) | パターン形成方法、パターン形成体 | |
| JP2012208396A (ja) | レジストパターンの形成方法およびそれを用いたパターン化基板の製造方法 | |
| JP2013187387A (ja) | パターン形成方法 | |
| TW200811918A (en) | Method for forming resist pattern, semiconductor device and production method thereof | |
| JP2012023242A (ja) | パターン製造方法およびパターン形成体 | |
| US9651870B2 (en) | Method and tool of lithography | |
| JP5056538B2 (ja) | 真空紫外光によるパターン形成体の製造方法 | |
| JP2011167780A (ja) | パターン形成方法およびパターン形成体 | |
| JP2010076134A (ja) | ナノインプリントモールド | |
| JP2012190827A (ja) | インプリントモールド及びその作製方法、パターン形成体 | |
| JP2008286828A (ja) | パターン形成方法 | |
| JP2012190986A (ja) | ナノインプリント用のモールド | |
| JP5966808B2 (ja) | 半導体装置の製造方法 | |
| JP5466468B2 (ja) | ドライエッチング方法 | |
| JP5011774B2 (ja) | 転写マスクブランク及び転写マスク並びにパターン露光方法 | |
| KR20100013975A (ko) | 반사형 마스크, 그 제조방법 및 그를 이용한 반도체 소자의패턴 형성방법 |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| 121 | Ep: the epo has been informed by wipo that ep was designated in this application |
Ref document number: 12765276 Country of ref document: EP Kind code of ref document: A1 |
|
| NENP | Non-entry into the national phase |
Ref country code: DE |
|
| ENP | Entry into the national phase |
Ref document number: 20137028208 Country of ref document: KR Kind code of ref document: A |
|
| 122 | Ep: pct application non-entry in european phase |
Ref document number: 12765276 Country of ref document: EP Kind code of ref document: A1 |