TW594462B - Method of manufacturing a touch screen panel - Google Patents
Method of manufacturing a touch screen panel Download PDFInfo
- Publication number
- TW594462B TW594462B TW091111840A TW91111840A TW594462B TW 594462 B TW594462 B TW 594462B TW 091111840 A TW091111840 A TW 091111840A TW 91111840 A TW91111840 A TW 91111840A TW 594462 B TW594462 B TW 594462B
- Authority
- TW
- Taiwan
- Prior art keywords
- coating
- patent application
- panel
- protective coating
- scope
- Prior art date
Description
594462 A7 _____B7 五、發明説明(1 ) 發明範疇 本發明係有關一種製造觸摸式螢幕面板之方法,其中於 邊緣電極以及導線線路之前沉積透明硬質塗層材料,讓硬 質塗層位於邊緣電極下方,俾免除當透明硬質塗層材料沉 積於邊緣電極及導線線路上方時,於面板邊緣呈現色彩變 化問題。 發明背景 觸摸式面板今日已經普遍用作為輸入及顯示介面用於 例如自動櫃員機、賭場的賭博機、現鈔收銀機等。觸摸式 螢幕面板通常包含一絕緣(例如玻璃)基板以及一設置於絕 緣基板上的電阻層。然後導電邊緣電極圖案形成於電阻層 邊緣。導電電極形成跨電阻層之X及γ方向的正交電場。手 才θ或光筆的接觸區接觸面板上的主動區,造成產生信號, 该#號表示手指或光筆所在位置相對於基板之X及γ座 標。藉此方式,藉導線或佈線線路連接至觸摸式面板的相 關觸摸式面板電路可確定觸摸發生於基板的何處。典型 地’電腦程式於觸摸式螢幕面板下方之監視器產生選項給 使用者(例如「『是』則按此處,『否』則按此處」),當觸 摸式面板由使用者使用時,導電邊緣電極圖案輔助偵測選 擇何種選項。 於先前技藝’電阻層(例如錫銻氧化物)濺鍍於玻璃基板 上。然後導電邊緣電極及導線線路使用厚膜糊沉積於電阻 層上環繞面板周邊。然後二氧化矽透明硬質塗層施用於面 板於導電邊緣電極及導線軌線上方俾於使用時保護面板。 -4 - 本紙張尺度適财g國家標準(CNS)罐格(咖χ 297公爱)
裝 訂
594462 A7 B7
五、發明説明(2 ) 但因邊緣電極以及導線線路的厚度,造成硬質塗層不平 坦,反而於面板邊緣升高,造成美感缺陷,面板邊緣存在 有色彩變化。此種無法接受的色彩變化於液體硬質塗層材 料築壩於邊緣電桎及線路周圍且流乾時,造成藉濕化學方 法施用結合二氧化矽透明硬質塗層之電容式觸摸式螢幕面 板的重大良率問題。 此外’厚膜材料的裂開及孤立造成功能不良,於構成電 容式觸摸式螢幕製造上的重大良率問題。此項問題係由於 邊緣電極及線路之厚膜與二氧化矽透明硬質塗層間之化學 交互作用所引起,以及經由於二氧化矽硬質塗層網路密化 期間機械應力加諸厚膜所引起。 它方面’若於邊緣電極及線路之前,沉積二氧化碎透明 硬質塗層材料’讓硬質塗層位於邊緣電極及線路下方俾消 除色彩變化問題’硬質塗層材料可避免邊緣電極及線路與 電阻塗層間建立矯正電連接。 發明概要 本發明之一目的係提供一種製造觸摸式螢幕面板之新穎 方法。 本發明之又一目的係提供可免除面板邊緣之色彩變化方 法。 本發明之又一目的係提供此種方法,其可減少或消除觸 摸式螢幕面板因邊緣電極及線路之厚膜裂開或孤立而造成 功能故障問題。 本發明之又一目的係提供一種可提供電容式觸摸式面板 -5 - 本紙張尺度適用中國國家標準(CNS) A4規格(210X 297公釐)
裝 訂
594462 A7
製造良率之方法。 :發:之又一目的係提供—種方法其免除二氧㈣塗層 藝相關之不良交互作用影響土:飞如此減少先前技 覆蓋於邊緣電極及料上方β 1技藝:氧切塗層係 ,本發明之又—目的係提供此種觸摸式勞幕面板其帶有更 %全密化之二氧化矽硬質塗層。 本發明係基於經由於邊緣電極圖案沉積於觸摸式勞幕面 板前’均句施用絕緣保護塗層,以及經由添加碳酸麵或甲 酸鋼组成物至邊料極及線路㈣之㈣銀/麵料糊,因 此當面板被燒製時,邊緣電極#穿^護塗層,如此盘面板 上保護性塗層下方之電阻塗層妥為建立電接觸,可克服施 用絕緣保護塗層至觸摸式螢幕面板之邊緣電缺線路上方 關聯的色彩變化及其它問題。 本發明之一特徵為一種製造觸摸式螢幕面板之方法,其 中一電阻塗層施用於一絕緣基板一面上,一絕緣保護塗層 施用於電阻塗層,一包括多數邊緣電極之導電邊緣電極圖 案沉積於保護塗層上,以及面板經燒製直到邊緣電極蝕穿 保護塗層且與電阻塗層作電接觸為止。 較好邊緣電極材料包括導電糊混合添加劑。絕緣保護塗 層可為一氧化碎,添加劑包括化學化合物,且於升高溫度 時轉化成熔融鹼金屬氫氧化物而溶解保護性塗層之二氧化 碎。典型地化合物係選自鈉碳酸鹽及/或鈉甲酸鹽組成的組 群。通常導電糊為銀/玻璃料組成物。添加劑典型係占導電 -6 - 本紙張尺奴&關家標準(CNS) A樣格(210X297公釐)
裝 訂
槔 594462 A7 ____B7 _ 五、發明説明(4~Γ 糊之1-25%重量比。 施用導電塗層之步驟包括濺鍍、蒸鍍、化學氣相沉積、 網印或襯墊印刷等方法。施用絕緣保護塗層之步騾係包括 /¾:塗、凹凸面塗覆、濺鍍、蒸鍍、化學氣相沉積、網印或 襯墊印刷。 一具體實施例中,絕緣保護塗層係於導電邊緣電極圖案 沉積其上之前硬化。燒製包括讓面板透過波長2 5至6 〇微 米之紅外線接觸升高溫度。 較佳具體實施例中,線路也沉積於保護塗層上,面板燒 製直到線路圖案蝕穿保護塗層而與電阻塗層做電接觸為 止。如此線路圖案材料包括導電糊混合添加劑。當絕緣保 護塗層包括一氧化硬時,添加劑包括化合物,該化合物於 升南溫度轉成鹼金屬氫氧化物而溶解保護塗層的二氧化 石夕〇 該方法進一步包括將線路圖案置於面板上,線路與邊緣 電極間提供電隔離。提供電隔離之方法包括結合電介質層 於線路圖案與保護塗層間。經由結合電介質層於邊緣電極 與線路間可提供電隔離。另外,經由未添加添加劑至線路 材料,且不會姓穿保護塗層,如此與邊緣電極做電隔離。 本發明之特點為一種製造一觸摸式螢幕面板之方法,該 方法包含:施用一電阻塗層至一絕緣基板一面上,施用一 絕緣保護塗層至電阻塗層,混合導電糊與添加劑,沉積混 合物成包括多數邊緣電極之導電邊緣電極圖案 塗層上,以及燒製面板,直到邊緣電極蚀穿保護 本紙張尺度適用中國國家標準(CNS) A4規格(210X 297公釐) 594462 A7 B7 五、發明説明( 電阻塗層做電接觸為止。絕緣保護塗層通常包括二氧化 石夕,添加劑包括料化合物,該化合物於升高溫錢變成 熔融鹼金屬氮氧化物而溶解保護塗層的二氧化矽。化學化 合物可選自鈉碳酸鹽類及/或鈉甲酸鹽類組成的組群。導電 糊可為銀/玻璃料組成物。添加劑典型係占導電糊之 重量比。 較佳具體實施例中,該方法進—步包括沉積線路圖案於 保護塗層上,以及燒製面板直到線路圖案蝕穿保護塗層而 與電阻塗層做電接觸為止。線路圖案材料包括導電糊二入 添加劑。絕緣導電塗層包括二氧化矽,添加劑包:化;: 裝 合物,該化合物於升高溫度轉成熔融鹼金屬氫氧化物:其 溶解保護塗層之二氧化碎。 ’、 、該方法進-步包括料路圖案與邊緣電極間提供電隔離 訂 〈步驟…具體實施例中,使用雷射來㈣保護材料以及 邊緣電極與線路間的電阻材料。 本發明也有一特徵在於一種觸摸式螢幕面板,其包含一 絕緣基板;一於絕緣基板表面上之電阻塗層;二塗· 線 層上之保護塗層;以及-包括多數邊緣電極之導電邊緣電 極圖案於該保護塗層上,且延伸至電崎層且 做電接觸。 玉增 、面板也包括線路圖案於保護塗層上。電介質材料係 於線路圖案與保護塗層間。另外,電介質材料可設 電邊緣電極圖案上方,然後線路圖案設置於電介質材料上。 星_式之簡要銳明
-8 - 594462 A7 ______B7___·___ 五、發明説明(7 ) 隨後形成於面板1〇周邊,如網印厚膜導電銀/玻璃料糊(例 如杜邦7713或費洛(Fen:o)3350)所示。各種邊緣電極圖案包 括美國專利第4,198,539 ; 4,293,734 ;或4,371,746號,也包括 美國專利申請案第09/169,391號,各案皆以引用方式併入此 處。其它沉積邊緣電極及線路圖案之方法以及隔離邊緣電 極與線路圖案之方法以及隔離毗鄰線路彼此之方法揭示於 美國專利申請案第〇9/775,253及09/773,979號,以引用方式併 入此處/。 於先前技藝,圖2透明二氧化矽硬質塗層30係藉浸塗、 噴塗或其它塗覆技術施用於面板上。但由於如36及38顯示 之邊緣電極厚度,硬質塗層非平面,於面板邊緣升高。如 36及38所示升高的干擾圖樣導致無法接受的色彩變化構成 藉濕化學方法施用攙混二氧化矽透明硬質塗層之電容式觸 摸式面板的重大議題。此等色彩變化係由於厚膜邊緣電極 以及線路圖案附近之二氧化矽透明硬質塗層厚度變化之 故。此種變化係由於施用於觸摸式螢幕周邊的厚膜圖案周 圍的液體塗覆液築高以及流掉所引起,結果導致塗覆表面 局部區域比平均沉積厚度更厚。厚度的變化表現為無法接 受的色謂,造成美感缺陷。此外,二氧化碎硬質塗層密化 期間’邊緣電極以及線路材料與二氧化矽透明硬質塗層間 的化學交互作用,結果導致邊緣電極及線路之厚膜材料的 裂開與孤立,造成功能故障。於二氧化矽硬質塗層材料密 化期間,厚膜材料上的機械應力也導致邊緣電極及/或線路 圖案材料出現裂開以及孤立型功能故障。 -10- 本紙張尺度適用中國國家標準(CNS) A4規格(210 X 297公釐) 594462 A7 _____B7_ 五、發明説明(8 ) 本發明中,因圖3硬質塗層30係於邊緣電極16及線路18 及24之前沉積,讓硬質塗層位於邊緣電極及線路下方,故 可消除色彩變化。如此,硬質塗層3 0為平面,即使於面板 邊緣各處皆平坦光滑,原因在於硬質塗層3 0係直接沉積於 電阻塗層32上之故。但邊緣電極及線路並未視需要而與電 阻塗層32直接電接觸俾產生跨電阻層32的電場。此項問題 於本發明係經由混合添加劑與用於邊緣電極及線路之導電 糊而克服,導電糊當接觸升高溫度時局部溶解保護性塗層 的二氧化矽。如此,當面板被燒製時,邊緣電極16及線路 18及24「燒穿」硬質塗層30(圖4)且與電阻塗層32建立電接 觸及物理接觸。為了電隔離邊緣電極與線路丨8及24、以及 電隔離任二毗鄰線路,可使用雷射燒蝕技術來去除邊緣電 極與線路間以及任二毗鄰線路間的電阻塗層。參考美國專 利申請案第09/773,979號,申請日2001年2月,以引用方 式併入此處。另外,線路材料未經添加劑改性,因此線路 未蝕穿硬質塗層材料,如此提供邊緣電極與線路間以及任 二毗鄰線路間的電隔離。於選擇性步驟中,保護性邊界層 40(圖5)沉積於硬質塗層30之邊緣電極及線路上方,及 可添加多種耐刮及抗黴菌組成物。參考美國專利申請安第 09/^,404 ; 09/233,3〇5及G9/626,272號,以引用方式:=此 "全部具體實施例中,經由於邊緣電極圖案及線路沉積之 前,均勻施用絕緣保護塗層於觸摸式螢幕面板,以及經由 添加碳酸氫鈉或甲酸鈉組成物至邊緣電極及線路材料2銀 -11 -
594462 A7 B7 五、發明説明(9 ) /玻璃料糊,讓面板燒製時,邊緣電極可蝕穿保護塗層,如 此於面板上的電阻塗層建立電接觸,可克服施用絕緣保護 塗層至觸摸式螢幕面板於邊緣電極及線路上方時造成的色 彩變化及其它問題。燒穿方法經由於二氧化碎塗覆過程完 成後施用邊緣電極圖案及線路,如此去除邊緣電極及線路 之築高缺陷,燒穿方法可免除先前技藝相關之無法接受的 色彩變化問題。又經由使用燒穿方法,邊緣電極及線路之 厚膜材料未由二氧化碎塗層覆蓋,因厚膜材料與二氧化珍 透明硬質塗層間之化學交互作用引發的不良交互作用影響 減至最低。又於二氧化矽硬質塗層網路密化期間,加諸厚 膜材料上的機械應力減至最低。 較佳具體實施例中,厚膜導電糊例如但非限於費洛335〇 或杜邦7713,混合1-25%重量比範圍之碳酸氫鈉或甲酸鈉添 加劑。發現2-5%添加劑重量比為最理想。使用燒穿過程, 此種添加劑允許厚膜導電糊與下方電阻塗層達成可接受的 電接觸。處理期間,前方電阻塗層或甚至玻璃基板兩面上 首先塗覆以透明硬質塗層材料,以及視需要地使用紅外線 擴大加熱硬化。參考共同審查中之申請案第〇9/626,272號, 申請日2000年7月25日,以引用方式併入此處。如前述製備 之厚膜導電糊隨後施用於基板,再度使用紅外線擴大加熱 硬化。最後,線路連接至觸摸式螢幕面板。經由燒製二氧 化矽硬質塗層兩次,由於二氧化矽結構之進一步硬化而達 成更為耐用的硬質塗層。 如此,本發明之目的係攙混一或多種化學化合物於厚膜 -12 - 本紙張尺度適用中國國家標準(CNS) Α4規格(210X297公釐) 裝 訂
A7
糊配方,該添加劑將於厚㈣燒製期間轉變絲融驗金屬 氳氣化物。於升高溫度時,此等 " 此寺溶融鹼金屬氫氧化物如氫 乳化納或錢㈣可溶解:氧切,隔開厚膜糊與透明塗 層的塗層必須接觸厚膜糊俾便讓觸摸式螢幕發揮功能。攙 屍驗金屬,氧化物於厚膜糊之最直接方法係呈氫氧化物添 加。但此等材料具有高度腐#性,處理上危險,造成於室 溫時發生非期望的反應。聽此種非期望之反應例,發現 添加氫氧㈣至厚膜糊,導致材料絲加至糊之後數小時 時間以内硬化,造成厚膜糊無法用於網印。此外,鹼金屬 氫氧化物之吸濕性極高,吸收大氣的水份,隨後以無法控 制的方式改變厚膜糊組成。 如此,較好使用鹼金屬氫氧化物之前驅物替代來調配厚 膜糊,該化學前驅物於儲存及網印期間之溫度相對不具反 應性,但於厚膜糊燒製期間之溫度,典型為5〇〇<5c溫度轉成 所需驗金屬氫氧化鋼。目前最滿意之經過試驗的前驅物為 碳酸氫納。此種物質於室溫無害,且相對非吸濕性。但此 種物質加熱時,首先於50°C熔化,然後於約i〇〇°c喪失二氧 化碳轉成碳酸鈉。碳酸鈉又於約4〇〇艽喪失二氧化碳,於全 然乾燥環境下轉成氧化鈉,或經由進一步於大氣水或厚膜 糊有機組成份燃燒水反應轉成氫氧化鈉。於此溫度,氫氧 化鈉熔化且有高度反應性,而達成二氧化矽層之溶解。 除了碳酸氫鈉外,顯然碳酸鈉也可達成相同結果,但碳 酸鈉比碳酸氫鈉更具有吸濕性,因此於細分粉末形式下更 難以處理。同理,預期添加碳酸鈉,碳酸鈉於50(TC以下之 -13 -本紙張尺度適用中國國家標準(CNS) A4規格(210 X 297公釐) 五、發明説明(11 ) 因此本發明也涵蓋 溫度分解,也達成二氧化矽層的溶解 此等化合物用於此項目的。 除了無機聽合物外,也可使用 :物作為前驅物,來於升高溫度形成氫氧 氣 二更==金屬化合物傾向於比厚膜糊尖=溫 於更小量水,如同典型燒製烘箱環境 丄1 產生龄金屬氫氧化物。例如發現添加甲酸 箱子.切可產生如同添加碳酸氯納的相同結果。同理, 加乙氧⑽、異丙氧化m化納、草酸麵、酒 ’内或確實任一種單純由鈉、4、氫及氧組成的化合物 °產生期望效果,只要該化合物可於低於鳩。c之溫度分解 即:。由於此等化合物之吸濕性質,此等化合物比較同系 列中的其它化合物更難以調配成厚膜糊,但使用任一種化 :物溶解二氧切或其它材料製造的硬質塗層也 發明之範圍。 同理,使用前述之平行鉀化合物包括碳酸氫鉀、碳酸 鉀^硝酸鉀或有機金屬鉀化合物如乙氧化鉀、異丙氧化鉀、 甲氧化鉀草酸鉀或酒石酸鉀或鈉/鉀混合碳酸鹽或混合有 機金屬如鉀鈉酒石酸鹽用於局部溶解硬質塗層(例如二氧 化矽)也涵蓋於本發明之範圍,原因在於該等金屬也預期於 500 C以下义溫度分解而形成熔融鹼金屬氫氧化物(氫氧化 鉀)。 典型地,電阻塗層32(圖3)係藉濺鍍、蒸鍍、化學氣相沉 積凹凸面塗覆、網印或襯墊印刷施用。保護性硬質塗層 594462 A7 ___B7 I、發明説明(12 ) " —— 30可藉浸塗、凹凸面塗覆、濺鍍、蒸鍍、化學氣相沉^ 網印或襯墊印刷施用。燒製期間,若面板接受紅外線解^, 則以波長2.5至6.0微米為佳。參考美國專利申倚安# 09/626,272號,申請日2000年7月25日,以引用方:衣矛 力八併入此 處。 線路圖案之線路須與邊緣電極圖案之邊緣電極電隔離。 本發明中有數種不同方式來達成電隔離。 一具體實施例中,使用雷射30(圖6)來燒蝕線路24與邊緣 電極16間的硬質塗層30及電阻塗層32材料。參考美國專利 申請案第09/773,979號。 另一具體實施例中,並未添加任何添加劑至線路材料, 未蝕穿硬質塗層,如圖7所示。 又另一具體實施例中,電介質層52(圖8)沉積於線路24 與硬質塗層30間,防止線路24被蝕穿硬質塗層3〇 ,提供線 路24與邊緣電極16間的電隔離。 又另一具體實施例中,電介質層52(圖9)沉積於位於電介 夤層52上的邊緣電極16及線路24上方。本具體實施例可有 利地節省面板邊緣空間,提供面板頂面的較大主動區。 任一具體實施例中,線路及電介質層可藉網印沉積,或 裝飾片可如專利申請案第〇9/775,253及09/773,979號之揭示 使用。 雖然本發明之特定結構係於某些圖式顯示而未於其它圖 式顯示’但為求方便,各特色可組合根據本發明之任何或 全部其它特色。用於此處「包括」、「包含」、「具有」及「帶 -15 - 本紙張尺度適财S g家標準(CNS) Α樣格(21Gχ 297公董)
Claims (1)
- 594462 A8 B8 C8 D8 1. 申請專利範圍 •種製造-觸摸式螢幕面板之方法,該方法包含: 施用一電阻塗層至一絕緣基板的一面上;。 施用一絕緣保護塗層至該電阻塗層; 保包括多數邊緣電極之導電邊緣電極圖案於 保瘦塗層上;以及 燒製該面板直到邊緣電極蝕穿 層作電接觸為止。 層且與電阻塗 2. 如申請專利範圍第巧之方法,其中邊緣電 導電糊混合添加劑。 " 3. 如申請專利範_2項之方法,其中絕緣保護性塗戶包 2二乳切,添加劑包括化學化合物,該化學化合物於 高溫時轉成㈣驗金屬氫氧化物,其溶解 的 二氧化矽。 曰 4·如申請專利範圍第3項之方法,其中該化學化合物係選 自鈉碳酸鹽及/或鈉甲酸鹽組成的組群。 5·如申請專利範圍第2項之方法,其中該導電糊為銀/玻璃 料組成物。 6·如申請專利範圍第2項之方法,其中該添加劑係占導電 糊之1-25%重量比。 7·如申請專利範圍第丨項之方法,其中施用電阻塗層之方 法包括選自濺鍍、蒸鍍、化學氣相沉積、凹凸面胃塗覆、 浸潰塗覆、網印及襯墊印刷組成的組群中之任一種方 8.如申請專利範圍第丨項之方法,其中該施用絕緣保護性 -17 本纸張尺度適用中國國家標準(CNS) Α4規格(210 X 297公釐) 裝 訂 594462 ABCD 六、申請專利範圍 塗層之步驟為一種選自浸塗、凹凸面塗覆、濺鍍、蒸鍍、 化學氣相沉積、網印及襯墊印刷組成的組群之方法。 9·如申請專利範圍第1項之方法,進一步包含於導電邊緣 電極圖案沉積於絕緣保護性塗層之前硬化該絕緣保護 性塗層。 10·如申請專利範圍第1項之方法,其中之燒製包括讓面板 接觸升高溫度。 11.如申請專利範圍第1〇項之方法,其中之燒製進一步包括 讓面板接觸紅外線。 I2·如申請專利範圍第Π項之方法,其中該紅外線輻射具有 2.5至6.0微米之波長。 B•如申請專利範圍第1項之方法,進一步包括沉積線路圖 案於保護性塗層上,以及燒製面板直到線路圖案蝕穿保 護性塗層且與電阻塗層做電接觸為止。 14.如申請專利範圍第13項之方法,其中線路圖案材料包括 導電糊混合添加劑。 15·如申請專利範圍第14項之方法,其中絕緣保護性塗層包 括二氧化矽,添加劑包括化學化合物,該化學化合:於 高溫時轉成鹼金屬氫氧化物,其溶解保護性塗層之二於 化矽。 "—虱 16·如申請專利範圍第13項之方法,進一步包括提供電隔離 於線路圖案與邊緣電極間之步驟。 Π.如申請專利範圍第16項之方法’其中提供電隔離之步驟 包括使用雷射來轴刻邊緣電極與綠路間之保護性材^ -18 - 本纸張尺度適用中國國家標準(CNS) A4規格(210 X 297公釐) ^4462 A8 B8 C8及電阻材料之步驟。 18·如申凊專利範圍第1項之方法,進一 案於面板上。 步包括設置線路圖 19·如申請專利範圍第1 8項之方法 於線路與邊緣電極之間。 ,進一步包括提供電隔離 2〇·=申請專利範圍第19項之方法,其中提供電隔離包括結 a層電介質層於線路圖案與保護性塗層之間。 21·如申請專利範圍第19項之方法,其中提供電隔離包括結 合一層電介質層於邊緣電極與線路之間。 m 22·如申請專利範圍第19項之方法,其中提供電隔離包括未 添加添加劑至線路材料,故不會蝕穿保護性塗層。 23· —種製造一觸摸式螢幕面板之方法,該方法包含:裴 施用一電阻塗層至一絕緣基板之一面上; 施用一絕緣保護塗層至電阻塗層; 混合導電糊與添加劑; 將混合物成包括多數邊緣電極之導電邊緣電極圖案 形式沈積於保護塗層上;以及 燒製面板’直到邊緣電極钱穿保護塗層而與電阻塗層 做電接觸為止。 24·如申凊專利範圍第2 3項之方法,其中該絕緣保護性塗層 包括二氧化石夕,而該添加劑包括化學化合物,該化學化 合物於高溫時轉成熔融鹼金屬氫氧化物該鹼金屬氫氧 化物溶解該保護性塗層的二氧化碎。 25·如申請專利範圍第24項之方法,其中該化學化合物係選 -19 - 本纸張尺度適用中國國家標準(CNS) Α4規格(210 X 297公釐) 訂 •線 594462 A8 B8 C8 D8 六、申請專利範圍 自鈉碳酸鹽及/或鈉甲酸鹽組成的組群。 26·如申請專利範圍第23項之方法,其中該導電糊為銀/玻 璃料組成物。 27·如申請專利範圍第23項之方法,其中該添加劑係占導電 糊之1-25%重量比。 28·如申睛專利範圍第23項之方法,進一步包括沉積線路圖 案於保護性塗層上,以及燒製面板直到線路圖案蝕穿保 護性塗層且與電阻塗層做電接觸為止。 29·如申叫專利範圍第2 8項之方法,其中線路圖案材料包括 導電糊混合添加劑。 3〇·如申請專利範圍第29項之方法,其中絕緣保護性塗層包 括二氧化矽,添加劑包括化學化合物,該化學化合:於 高溫時轉成鹼金屬氫氧化物而溶解保護性塗層之二j 化矽。 3 —虱 31.如申請專利範圍第28項之方法,進一 延步包括提供電隔離 於線路圖案與邊緣電極間之步驟。 32·如申請專利範圍心項之方法,其中提供電隔離之_ 包括使用雷射來姓刻邊緣電極與線路間之保: 及電阻材料之步驟。 進一步包括設置線路圖 進—步包括提供電隔離 其中提供電隔離包括結 33·如申請專利範圍第23項之方法 案於面板上。 34.如申請專利範圍第33項之方法 於線路與邊緣電極間。 35.如申清專利範圍第34項之方法 • 20 - 594462 A8 B8 C8合一層電介質層於線路圖案與保護性塗層間。 36·如申請專利範圍第34項之方法,其中提供電隔離包括結 合一層電介質層於邊緣電極與線路間。 37·如申請專利範圍第34項之方法,其中提供電隔離包括未 添加添加劑至線路材料,故不會蝕穿保護性塗層。 38· —種觸摸式螢幕面板,其包含: 一絕緣基板; 一在絕緣基板表面上之電阻塗層; 一在電阻塗層上之保護塗層;以及 一包括多數邊緣電極之導電邊緣電極圖案於該保護 塗層上’且延伸至電阻塗層且與電阻塗層做電接觸。 39. 如申叫專利範圍第3 8項之面板,其中邊緣電極材料包含 導電糊混合添加劑。 40. 如申凊專利範圍第39項之面板,其中絕緣保護性塗層包 括二氧化矽,添加劑包括化學化合物,該化學化合物於 高溫時轉成熔融鹼金屬氫氧化物,其溶解保護性塗層的 二氧化矽。 41·如申請專利範圍第4〇項之面板,其中該化學化合物係選 自鋼碳酸鹽及/或鈉曱酸鹽組成的組群。 42·如申請專利範圍第39項之面板,其中該導電糊為銀/玻 璃料組成物。 43, 如申清專利範圍第39項之面板,其中該添加劑占導電糊 之1-25%重量比。 44. 如申請專利範圍第38項之面板,其中該電阻塗層係藉由 -21 - 本紙張尺度適用中國國家標準(CNS) A4規格(210 X 297公釐)裝 訂594462 A8 B8 C8 _ D8 申請專利範圍 ~~ ~ 選自賤鍍、蒸鍍、化學氣相沉積、凹凸面塗覆、浸塗、 網印及襯墊印刷組成的組群之方法施用。 45·如申請專利範圍第3 8項之面板,其中該絕緣保護性塗層 係經由一種選自浸塗、凹凸面塗覆、滅鍵、蒸鏡、化學 氣相沉積、網印及襯墊印刷組成的組群之方法施用。 46·如申請專利範圍第38項之面板,其中該絕緣保護性塗層 係於導電性邊緣電極圖案沉積於其上之前硬化。 47. 如申請專利範圍第3 8項之面板,進一步包括沉積於保護 性塗層上之線路圖案,其钱穿保護性塗層,以及與電阻 塗層做電接觸。 48. 如申請專利範圍第47項之面板,其中該線路圖案材料包 括導電糊 >昆合添加劑。 49. 如申請專利範圍第4 8項之面板,其中該絕緣保護性塗層 包括一氧化;?夕,而添加劑包括一種化學化合物,該化學 化合物於高溫時轉變成熔融鹼金屬氫氧化物,其溶解保 護性塗層之二氧化珍。 50·如申請專利範圍第38項之面板,進一步包括線路圖 保護性塗層上。 ; 51. 如申請專利範圍第50項之面板,進一步包括電隔離於線 路圖案與邊緣電極間。 52. 如申請專利範圍第5丨項之面板,進一步包括電介質材料 於線路圖案與保護性塗層間。 53·如申請專利範圍第5丨項之面板,進一步包括電介質材料 於電介質材料上的導電性邊緣電極圖案及線路圖案上 方0 -22 - 本紙張尺度適财s s家標準(CNS) A4規格_ x 297公爱)~ :------- 594462 第091111840號專利申請案 -;—— 中文說明書替換頁阳年u月〕 Α7 身亟'由後文較佳具體實施例之詳細說明及附圖,熟諳技藝人 士將了解其它目的、特色及優點,附圖中: 圖1為典型觸摸式螢幕面板之示意頂視圖; 圖2為圖1所示面板沿線2-2所取之示意剖面圖;圖3為本發明之觸摸式螢幕面板於燒製前之示意剖面 153 · 圖, 圖4為根據本發明製造之觸摸式螢幕面板於燒製後之示 思、剖面圖; 圖5為根據本發明製造之另一觸摸式螢幕面板之示意剖 面圖;之 圖6為根據本發明製造之觸摸式螢幕面板之剖面圖,其 中使用雷射來電隔離線路與邊緣電極; 圖7為根據本發明之觸摸式螢幕之示意剖面圖,其中線 路材料不含添加劑,如此線路不會蝕穿硬質塗層而提供線 路與邊緣電極間的電隔離; 圖8為根據本發明之觸摸式螢幕之示意剖面圖,其中電 介質層設置於線路與邊緣電極間俾提供電隔離;以及 圖9為根據本發明之觸摸式螢幕之示意剖面圖,其中線 路係位於邊緣電極上方且藉添加電介質層而與邊緣電極做 電隔離。 毽-倖具體實施例夕揭士 如前又背景乙節說明,圖i典型觸摸式螢幕面板1〇包括 衾巴緣玻璃基板12於其表面14塗覆有電阻層32,圖2(例如錫 銻氧化物)。導電邊緣電極圖案16及線路18、2〇、21及24594462 第091111840號專利申請案 中文說明書替換頁(92年12月)五、發明説明(13 ) 有」等詞需做廣泛全面性的解譯,而非囿限於任何實體互 連結構。此外本案揭示之任何具體實施例皆非唯一可能的 具體實施例。 熟諳技藝人士將了解其它具體實施例且該等具體實施例 係屬於如下申請專利範圍。 元件符號對照表 10 觸摸式螢幕面板 12 絕緣玻璃基板 14 表面 16 邊緣電極圖案 18,20,21,24 線路 30 硬質塗層 32 電阻塗層 36 邊緣電極 38 邊緣電極 40 保護性邊界層 52 電介質層 -16 - 本紙張尺度適用中國國家標準(CNS) A4規格(210 X 297公釐)