JPS6315899B2 - - Google Patents
Info
- Publication number
- JPS6315899B2 JPS6315899B2 JP12797180A JP12797180A JPS6315899B2 JP S6315899 B2 JPS6315899 B2 JP S6315899B2 JP 12797180 A JP12797180 A JP 12797180A JP 12797180 A JP12797180 A JP 12797180A JP S6315899 B2 JPS6315899 B2 JP S6315899B2
- Authority
- JP
- Japan
- Prior art keywords
- film
- temperature
- inert gas
- deep
- furnace
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Blow-Moulding Or Thermoforming Of Plastics Or The Like (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP12797180A JPS5753316A (en) | 1980-09-17 | 1980-09-17 | Deep drawing method of biaxially stretched polyester film |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP12797180A JPS5753316A (en) | 1980-09-17 | 1980-09-17 | Deep drawing method of biaxially stretched polyester film |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS5753316A JPS5753316A (en) | 1982-03-30 |
| JPS6315899B2 true JPS6315899B2 (enrdf_load_stackoverflow) | 1988-04-06 |
Family
ID=14973212
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP12797180A Granted JPS5753316A (en) | 1980-09-17 | 1980-09-17 | Deep drawing method of biaxially stretched polyester film |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS5753316A (enrdf_load_stackoverflow) |
Families Citing this family (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH0737173B2 (ja) * | 1985-06-19 | 1995-04-26 | 大日本印刷株式会社 | 部分金属薄膜層を有する転写シ−トの製造方法 |
| JPH01220317A (ja) * | 1988-02-29 | 1989-09-04 | Fuji Rubber Kk | 耐熱性樹脂ドームばね |
| JP4270640B2 (ja) * | 1999-03-31 | 2009-06-03 | 大日本印刷株式会社 | パウチフィルムへの膨らみ部の形成方法、及びその形成方法による膨らみ部を備えたパウチ |
-
1980
- 1980-09-17 JP JP12797180A patent/JPS5753316A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS5753316A (en) | 1982-03-30 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPH10286874A (ja) | 耐熱容器の成形方法 | |
| JPS5894419A (ja) | 樹脂シ−トの連続プレス成形法 | |
| JPS6315899B2 (enrdf_load_stackoverflow) | ||
| TWI630179B (zh) | Method for producing glass molded body and device for manufacturing glass molded body | |
| JPH05192990A (ja) | ポリエステル成型品の製造方法とその装置 | |
| JPS6020173B2 (ja) | ポリエチレンテレフタレ−ト製耐熱容器の製造方法 | |
| JP4019308B2 (ja) | 2軸延伸ブロー成形方法 | |
| JPH03199030A (ja) | 熱可塑性樹脂シートの熱成形方法及び装置 | |
| JPH0485019A (ja) | 結晶性ポリエチレンテレフタレートシートの成形方法 | |
| EP0089201A2 (en) | Reheating of preforms with radio frequency energy | |
| EP0730949A2 (en) | Methods of winding, annealing and unwinding a polymer film web, an annealing apparatus and a photographic film support prepared using said method or apparatus | |
| JP2592670B2 (ja) | ポリエステルボトルの製造法 | |
| JPH0462028A (ja) | 高延伸ブロー成形容器の製造方法 | |
| JPH06179239A (ja) | ポリエチレンテレフタレートシートの成形方法及びその成形金型 | |
| JPH02276626A (ja) | 熱成形品の熱処理方法及び装置 | |
| JP2871783B2 (ja) | 複合材の成形方法および成形装置 | |
| JP2006062353A (ja) | フランジ部の加熱処理方法、フランジ部の加熱処理装置及びフランジ付き樹脂製容器の製造方法 | |
| JPS5837886B2 (ja) | プラスチック薄肉成形品の製造方法 | |
| JPH04265729A (ja) | ポリカーボネート樹脂シートの熱成形方法 | |
| JP3529175B2 (ja) | 熱可塑性ポリエステル樹脂発泡成形品の製造方法 | |
| JPH0462027A (ja) | 高延伸ブロー成形容器の製造方法 | |
| JPH0446902Y2 (enrdf_load_stackoverflow) | ||
| JPH06218805A (ja) | 発泡ポリプロピレンシートの成形方法 | |
| JPH10315311A (ja) | キャリアテープの製造方法 | |
| JPH0376626A (ja) | ポリエステルシートの熱成形方法 |