JPS63125694A - 溶接缶用表面処理鋼板の製造方法 - Google Patents
溶接缶用表面処理鋼板の製造方法Info
- Publication number
- JPS63125694A JPS63125694A JP27170986A JP27170986A JPS63125694A JP S63125694 A JPS63125694 A JP S63125694A JP 27170986 A JP27170986 A JP 27170986A JP 27170986 A JP27170986 A JP 27170986A JP S63125694 A JPS63125694 A JP S63125694A
- Authority
- JP
- Japan
- Prior art keywords
- plating
- alloy
- bath
- steel sheet
- amount
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Electroplating Methods And Accessories (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP27170986A JPS63125694A (ja) | 1986-11-17 | 1986-11-17 | 溶接缶用表面処理鋼板の製造方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP27170986A JPS63125694A (ja) | 1986-11-17 | 1986-11-17 | 溶接缶用表面処理鋼板の製造方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS63125694A true JPS63125694A (ja) | 1988-05-28 |
| JPH0210879B2 JPH0210879B2 (enEXAMPLES) | 1990-03-09 |
Family
ID=17503748
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP27170986A Granted JPS63125694A (ja) | 1986-11-17 | 1986-11-17 | 溶接缶用表面処理鋼板の製造方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS63125694A (enEXAMPLES) |
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH04116192A (ja) * | 1990-09-05 | 1992-04-16 | Nkk Corp | 耐食性および溶接性に優れた無塗装缶用表面処理鋼板およびその製造方法 |
| JP2007177311A (ja) * | 2005-12-28 | 2007-07-12 | Fujitsu Ltd | めっき皮膜及びその形成方法並びに電子部品 |
| JP2012046827A (ja) * | 2011-11-18 | 2012-03-08 | Fujitsu Ltd | めっき皮膜及びその形成方法並びに電子部品 |
-
1986
- 1986-11-17 JP JP27170986A patent/JPS63125694A/ja active Granted
Cited By (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPH04116192A (ja) * | 1990-09-05 | 1992-04-16 | Nkk Corp | 耐食性および溶接性に優れた無塗装缶用表面処理鋼板およびその製造方法 |
| JP2007177311A (ja) * | 2005-12-28 | 2007-07-12 | Fujitsu Ltd | めっき皮膜及びその形成方法並びに電子部品 |
| JP2012046827A (ja) * | 2011-11-18 | 2012-03-08 | Fujitsu Ltd | めっき皮膜及びその形成方法並びに電子部品 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0210879B2 (enEXAMPLES) | 1990-03-09 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| JPS5825758B2 (ja) | 溶接塗装缶用鋼板 | |
| JPS5930798B2 (ja) | 溶接缶容器用鋼板とその製造法 | |
| JPS6046199B2 (ja) | 耐錆性の高い溶接缶用表面処理鋼板の製造方法 | |
| JPS61223197A (ja) | 表面処理鋼板 | |
| JPS63125694A (ja) | 溶接缶用表面処理鋼板の製造方法 | |
| JPS62103390A (ja) | 製缶用薄Snメツキ鋼板及びその製造方法 | |
| JPS62297491A (ja) | 容器用電解クロムメツキ鋼板の製造法 | |
| JPH0140118B2 (enEXAMPLES) | ||
| JPH02274866A (ja) | 耐食性に優れたCr―Ni拡散処理鋼板の製造法 | |
| JPH0826477B2 (ja) | 塗料密着性に優れたSn系多層めっき鋼板の製造法 | |
| JPS6029477A (ja) | 溶接性と塗装性能にすぐれた缶容器用鋼板の製造法 | |
| JPS63186860A (ja) | 耐錆性、溶接性に優れた表面処理鋼板の製造方法 | |
| JPS61195989A (ja) | 耐食性及び溶接性に優れた表面処理鋼板の製造方法 | |
| JPS6240396A (ja) | 溶接性、耐食性に優れた缶用表面処理鋼板 | |
| JP3224457B2 (ja) | 高速シーム溶接性、耐食性、耐熱性および塗料密着性に優れた溶接缶用素材 | |
| JPS6393894A (ja) | 外面塗料密着性に優れた缶用鋼板 | |
| JP2000080499A (ja) | ニッケル系めっき鋼板の化学処理法 | |
| JPS60262975A (ja) | 溶接性に優れた表面処理鋼板及びその製造方法 | |
| JPH041074B2 (enEXAMPLES) | ||
| JPS61250177A (ja) | 製缶用表面処理鋼板 | |
| JPS6396294A (ja) | 溶接性、耐食性に優れた缶用鋼板の製造方法 | |
| JP3434927B2 (ja) | 塗装外観に優れた溶接缶用鋼板の製造方法 | |
| JP2737813B2 (ja) | 塗料密着性とシーム溶接性に優れた錫めっき鋼板 | |
| JP2000008194A (ja) | 錫系めっき鋼板の化学処理法 | |
| JPS6310238B2 (enEXAMPLES) |
Legal Events
| Date | Code | Title | Description |
|---|---|---|---|
| R250 | Receipt of annual fees |
Free format text: JAPANESE INTERMEDIATE CODE: R250 |
|
| LAPS | Cancellation because of no payment of annual fees |