JPS6245885B2 - - Google Patents
Info
- Publication number
- JPS6245885B2 JPS6245885B2 JP57024845A JP2484582A JPS6245885B2 JP S6245885 B2 JPS6245885 B2 JP S6245885B2 JP 57024845 A JP57024845 A JP 57024845A JP 2484582 A JP2484582 A JP 2484582A JP S6245885 B2 JPS6245885 B2 JP S6245885B2
- Authority
- JP
- Japan
- Prior art keywords
- weight
- water
- copolymer
- slurry
- dispersion
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Processes Of Treating Macromolecular Substances (AREA)
- Compositions Of Macromolecular Compounds (AREA)
- Paints Or Removers (AREA)
- Adhesives Or Adhesive Processes (AREA)
- Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2484582A JPS58141231A (ja) | 1982-02-17 | 1982-02-17 | スラリ−状水分散体の製造方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP2484582A JPS58141231A (ja) | 1982-02-17 | 1982-02-17 | スラリ−状水分散体の製造方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS58141231A JPS58141231A (ja) | 1983-08-22 |
JPS6245885B2 true JPS6245885B2 (enrdf_load_stackoverflow) | 1987-09-29 |
Family
ID=12149548
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP2484582A Granted JPS58141231A (ja) | 1982-02-17 | 1982-02-17 | スラリ−状水分散体の製造方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS58141231A (enrdf_load_stackoverflow) |
Families Citing this family (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
DE4404411A1 (de) * | 1994-02-11 | 1995-08-17 | Basf Ag | Dispersionsfußbodenkleber |
JP4366708B2 (ja) * | 2002-05-20 | 2009-11-18 | 日東電工株式会社 | 再剥離用水分散型感圧性接着剤 |
Family Cites Families (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS5717945A (en) * | 1980-07-04 | 1982-01-29 | Nippon Seimitsu Kogyo Kk | Shutter device of camera equipped with discrimination function of battery capacity |
-
1982
- 1982-02-17 JP JP2484582A patent/JPS58141231A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS58141231A (ja) | 1983-08-22 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JPS5823801A (ja) | 懸濁重合法 | |
JPS6346106B2 (enrdf_load_stackoverflow) | ||
JPS59117505A (ja) | 微細なポリビニルアセタ−ル,その製造方法およびその用途 | |
US4665142A (en) | Emulsion polymers free from emulsifiers and protective colloids, a process for their preparation and their use | |
JP3162367B2 (ja) | 保護コロイド系再分散性アクリル樹脂エマルジョン粉末およびその製造方法 | |
JPH07507350A (ja) | 表面処理した吸収剤ポリマー | |
WO2000020463A9 (en) | Use of derivatives of polyaspartic acid as emulsifiers and stabilizers in aqueous free radical emulsion polymerization | |
JPH11508959A (ja) | カルボキシル化されたブタジエン含有コポリマーをベースとする再分散性粉末 | |
JPS6245885B2 (enrdf_load_stackoverflow) | ||
JP6874154B2 (ja) | 塩化ビニル系樹脂ラテックス組成物およびその製造方法 | |
WO1997003128A1 (fr) | Composition de polymere carboxylee | |
CA2334796A1 (en) | New protective colloids in latices with improved film formation at low temperatures | |
JPS6150482B2 (enrdf_load_stackoverflow) | ||
JP3426358B2 (ja) | ポリビニルアルコール系樹脂微粒子の製造法 | |
JPS6031852B2 (ja) | ヒドロゾルの製造方法 | |
JPS59179676A (ja) | 感圧性接着テ−プの製造方法 | |
JPS60199086A (ja) | エアゾ−ル型感圧性接着剤組成物 | |
JPH044323B2 (enrdf_load_stackoverflow) | ||
US2558396A (en) | Method of preparing finely divided plasticized polymerized materials and products thereof | |
JPH0586403B2 (enrdf_load_stackoverflow) | ||
JPS58164632A (ja) | ヒドロゾルの製造方法 | |
JPH0155673B2 (enrdf_load_stackoverflow) | ||
JPS59184241A (ja) | ヒドロゾルの製造方法 | |
JP2023529276A (ja) | アルキルフェノールを含まない反応性非イオン性界面活性剤、アルキルフェノールを含まない反応性非イオン性界面活性剤を得るための方法、乳化重合により得られるラテックス、高い耐水性を有する水性コーティング組成物、及び水性コーティング組成物の使用 | |
JPS58164669A (ja) | 感圧性接着テ−プの製造方法 |