JPS6236323B2 - - Google Patents

Info

Publication number
JPS6236323B2
JPS6236323B2 JP1122282A JP1122282A JPS6236323B2 JP S6236323 B2 JPS6236323 B2 JP S6236323B2 JP 1122282 A JP1122282 A JP 1122282A JP 1122282 A JP1122282 A JP 1122282A JP S6236323 B2 JPS6236323 B2 JP S6236323B2
Authority
JP
Japan
Prior art keywords
nanbo
oriented
ultra
ceramic
melt
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired
Application number
JP1122282A
Other languages
English (en)
Japanese (ja)
Other versions
JPS58165208A (ja
Inventor
Yasuyoshi Torii
Tadashi Sekya
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
National Institute of Advanced Industrial Science and Technology
Original Assignee
Agency of Industrial Science and Technology
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Agency of Industrial Science and Technology filed Critical Agency of Industrial Science and Technology
Priority to JP57011222A priority Critical patent/JPS58165208A/ja
Publication of JPS58165208A publication Critical patent/JPS58165208A/ja
Publication of JPS6236323B2 publication Critical patent/JPS6236323B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Inorganic Insulating Materials (AREA)
JP57011222A 1982-01-27 1982-01-27 配向性ニオブ酸ナトリウム膜の製造法 Granted JPS58165208A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP57011222A JPS58165208A (ja) 1982-01-27 1982-01-27 配向性ニオブ酸ナトリウム膜の製造法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP57011222A JPS58165208A (ja) 1982-01-27 1982-01-27 配向性ニオブ酸ナトリウム膜の製造法

Publications (2)

Publication Number Publication Date
JPS58165208A JPS58165208A (ja) 1983-09-30
JPS6236323B2 true JPS6236323B2 (enExample) 1987-08-06

Family

ID=11771929

Family Applications (1)

Application Number Title Priority Date Filing Date
JP57011222A Granted JPS58165208A (ja) 1982-01-27 1982-01-27 配向性ニオブ酸ナトリウム膜の製造法

Country Status (1)

Country Link
JP (1) JPS58165208A (enExample)

Families Citing this family (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
DE60224748T2 (de) * 2001-04-23 2009-02-05 Kabushiki Kaisha Toyota Chuo Kenkyusho Kornorientierte Keramik und Verfahren zu ihrer Herstellung, sowie anisotrop geformtes Pulver und Verfahren zu seiner Herstellung

Also Published As

Publication number Publication date
JPS58165208A (ja) 1983-09-30

Similar Documents

Publication Publication Date Title
Ye et al. Structure and properties of hot-pressed lead-free (Ba0. 85Ca0. 15)(Zr0. 1Ti0. 9) O3 piezoelectric ceramics
KR850000596B1 (ko) 철, 붕소, 규소의 3원 비결정성 합금
JP3391307B2 (ja) 圧電セラミックスの製造方法
JP3985144B2 (ja) 酸化物イオン伝導性結晶体の製造方法
JP2003267796A (ja) ペロブスカイト構造を有する酸化物及びその製造方法
CN111533457A (zh) 一种铁电性能连续、可调谐的Bi2GeO5铁电微晶玻璃及其制备方法
CN110508919B (zh) 一种梯度铝硅电子封装材料的制备方法
JPS58161924A (ja) 結晶配向性ニオブ酸ランタンの透明薄帯製造法
JPS6235993B2 (enExample)
JPS58165208A (ja) 配向性ニオブ酸ナトリウム膜の製造法
Deshpande et al. Synthesis and characterization of lithium niobate ceramics with glass additions
Hussin et al. Structural and electrical properties of Bi0. 5Na0. 5TiO3 templates produced by topochemical microcrystal conversion method
JPS582289A (ja) 単結晶体の製造方法
JPS593091A (ja) 酸化物単結晶の製造方法
CN113233772B (zh) 一种调控玻璃网络结构实现高介电常数及高击穿性能的玻璃陶瓷及其制备方法
JP2610033B2 (ja) 酸化物系超電導成形体の製造方法
JPH0336798B2 (enExample)
Rizak et al. Electric properties of lithium tetraborate in vitreous and crystalline states
JPH03257018A (ja) 酸化物高温超電導体の前駆体およびその製造方法
JPH0346710A (ja) 超電導線の製造方法
JPS6479011A (ja) フレーク状酸化物超電導体及びその製造方法
JPH01176608A (ja) 酸化物超電導線条体の製造方法
JP2795450B2 (ja) 磁気ヘッド用非晶質磁性合金
JPS6084712A (ja) チタン酸鉛焦電体素子の製造方法
JPH01103999A (ja) 強誘電体単結晶の単一分域化方法