JPS619950A - 溶融金属の連続鋳造方法 - Google Patents

溶融金属の連続鋳造方法

Info

Publication number
JPS619950A
JPS619950A JP13177084A JP13177084A JPS619950A JP S619950 A JPS619950 A JP S619950A JP 13177084 A JP13177084 A JP 13177084A JP 13177084 A JP13177084 A JP 13177084A JP S619950 A JPS619950 A JP S619950A
Authority
JP
Japan
Prior art keywords
slag
tundish
molten metal
continuous casting
molten
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP13177084A
Other languages
English (en)
Japanese (ja)
Other versions
JPH052418B2 (enrdf_load_stackoverflow
Inventor
Kazuyoshi Nakai
中井 一吉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JFE Steel Corp
Original Assignee
Kawasaki Steel Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Kawasaki Steel Corp filed Critical Kawasaki Steel Corp
Priority to JP13177084A priority Critical patent/JPS619950A/ja
Publication of JPS619950A publication Critical patent/JPS619950A/ja
Publication of JPH052418B2 publication Critical patent/JPH052418B2/ja
Granted legal-status Critical Current

Links

Classifications

    • BPERFORMING OPERATIONS; TRANSPORTING
    • B22CASTING; POWDER METALLURGY
    • B22DCASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
    • B22D43/00Mechanical cleaning, e.g. skimming of molten metals
    • B22D43/005Removing slag from a molten metal surface
    • B22D43/008Removing slag from a molten metal surface by suction

Landscapes

  • Engineering & Computer Science (AREA)
  • Mechanical Engineering (AREA)
  • Continuous Casting (AREA)
JP13177084A 1984-06-26 1984-06-26 溶融金属の連続鋳造方法 Granted JPS619950A (ja)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP13177084A JPS619950A (ja) 1984-06-26 1984-06-26 溶融金属の連続鋳造方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP13177084A JPS619950A (ja) 1984-06-26 1984-06-26 溶融金属の連続鋳造方法

Publications (2)

Publication Number Publication Date
JPS619950A true JPS619950A (ja) 1986-01-17
JPH052418B2 JPH052418B2 (enrdf_load_stackoverflow) 1993-01-12

Family

ID=15065752

Family Applications (1)

Application Number Title Priority Date Filing Date
JP13177084A Granted JPS619950A (ja) 1984-06-26 1984-06-26 溶融金属の連続鋳造方法

Country Status (1)

Country Link
JP (1) JPS619950A (enrdf_load_stackoverflow)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS61140354A (ja) * 1984-12-12 1986-06-27 Sumitomo Metal Ind Ltd 異鋼種の連続鋳造方法

Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS58116960A (ja) * 1981-12-30 1983-07-12 Nippon Steel Corp 溶融金属容器

Patent Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS58116960A (ja) * 1981-12-30 1983-07-12 Nippon Steel Corp 溶融金属容器

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPS61140354A (ja) * 1984-12-12 1986-06-27 Sumitomo Metal Ind Ltd 異鋼種の連続鋳造方法

Also Published As

Publication number Publication date
JPH052418B2 (enrdf_load_stackoverflow) 1993-01-12

Similar Documents

Publication Publication Date Title
JPS619950A (ja) 溶融金属の連続鋳造方法
JPH0620621B2 (ja) タンデイツシユの再使用方法および再使用用装置
JP2786814B2 (ja) 鋼の連続鋳造におけるタンディッシュの再使用方法
JPH0675756B2 (ja) スライディングノズルの開孔方法
JP2755891B2 (ja) 溶融金属容器の内張り不定形耐火物の補修方法
JPS63174764A (ja) 連続鋳造における鋳込み開始時の溶鋼酸化防止方法
JPS61189848A (ja) 連続鋳造方法
JP4600095B2 (ja) タンディッシュの熱間再使用方法
JP4189313B2 (ja) 熱間回転タンディッシュを用いた溶鋼の連続鋳造方法
JPH01237061A (ja) 連続鋳造用タンディッシュの再使用方法
JPH0119990B2 (enrdf_load_stackoverflow)
JP3642015B2 (ja) ステンレス鋼の連続鋳造方法
JPH0475750A (ja) 複層鋳片の連続鋳造方法及び装置
JPH01127159A (ja) 異鋼種の連続連続鋳造方法
JPH01228654A (ja) 連続鋳造におけるタンデイツシユの再使用方法
JPH07227652A (ja) タンディシュ熱間回転時の操業方法
JPH01122641A (ja) 連続鋳造用タンディッシュの再使用方法
JPH0455770B2 (enrdf_load_stackoverflow)
JP2710093B2 (ja) タンディッシュの連続使用方法
JPS61179807A (ja) 混銑車用溶滓受容器の取扱い装置
JPS63137553A (ja) ロングノズル浸漬スタ−ト方法
JPH11347693A (ja) ベルトホイール式連続鋳造用注湯装置および前記注湯装置を用いた連続鋳造方法
JPH01107949A (ja) タンデイツシユ無補修再使用方法
JPH11320043A (ja) 連続鋳造設備及び連続鋳造方法
JP2003326341A (ja) タンディッシュの連続使用方法