JPS6143394B2 - - Google Patents
Info
- Publication number
- JPS6143394B2 JPS6143394B2 JP58033843A JP3384383A JPS6143394B2 JP S6143394 B2 JPS6143394 B2 JP S6143394B2 JP 58033843 A JP58033843 A JP 58033843A JP 3384383 A JP3384383 A JP 3384383A JP S6143394 B2 JPS6143394 B2 JP S6143394B2
- Authority
- JP
- Japan
- Prior art keywords
- weight
- parts
- aqueous suspension
- particle size
- microspheres
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Compositions Of Macromolecular Compounds (AREA)
- Adhesives Or Adhesive Processes (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP3384383A JPS59159869A (ja) | 1983-03-03 | 1983-03-03 | 再剥離性粘着剤組成物およびその製造法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP3384383A JPS59159869A (ja) | 1983-03-03 | 1983-03-03 | 再剥離性粘着剤組成物およびその製造法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS59159869A JPS59159869A (ja) | 1984-09-10 |
| JPS6143394B2 true JPS6143394B2 (en:Method) | 1986-09-27 |
Family
ID=12397771
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP3384383A Granted JPS59159869A (ja) | 1983-03-03 | 1983-03-03 | 再剥離性粘着剤組成物およびその製造法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS59159869A (en:Method) |
Families Citing this family (3)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| JPS61152779A (ja) * | 1984-12-27 | 1986-07-11 | Toyo Ink Mfg Co Ltd | 再剥離型粘着剤組成物 |
| JPH0684490B2 (ja) * | 1985-05-15 | 1994-10-26 | ニチバン株式会社 | 再剥離性粘着剤組成物 |
| JPH0684491B2 (ja) * | 1985-05-15 | 1994-10-26 | ニチバン株式会社 | 再剥離性粘着剤組成物 |
Family Cites Families (1)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| US3857731A (en) * | 1973-04-06 | 1974-12-31 | Minnesota Mining & Mfg | Acrylate microsphere-surfaced sheet material |
-
1983
- 1983-03-03 JP JP3384383A patent/JPS59159869A/ja active Granted
Also Published As
| Publication number | Publication date |
|---|---|
| JPS59159869A (ja) | 1984-09-10 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| US4656218A (en) | Adhesive copolymer microspheres-containing aqueous suspension and method for producing the same | |
| US4645783A (en) | Adhesive copolymer microspheres-containing aqueous suspension and method for producing the same | |
| TW416963B (en) | Stabilized adhesive microspheres | |
| JP5346048B2 (ja) | 複合感圧接着性微小球 | |
| AU627607B2 (en) | Pressure-sensitive adhesive comprising hollow tacky microspheres and macromonomer-containing binder copolymer | |
| JP4130993B2 (ja) | 部分的に架橋された微小球 | |
| US4988567A (en) | Hollow acid-free acrylate polymeric microspheres having multiple small voids | |
| JPH04216888A (ja) | 中空多孔性アシッドフリーアクリレート系高分子量微小球 | |
| JP2004346333A (ja) | 粘着性微小球を含む再配置性感圧接着剤の膜を含むシート材料 | |
| JPH02194079A (ja) | 中空のアクリレートポリマー微小球およびその製造方法 | |
| JPH04227672A (ja) | 粘着性固体微小球とマクロモノマー含有バインダーコポリマーを含有する感圧接着剤 | |
| JPS61261382A (ja) | 再剥離性粘着剤組成物 | |
| JPH0339521B2 (en:Method) | ||
| JP2000281999A (ja) | 再剥離型感圧接着剤組成物 | |
| JP2610616B2 (ja) | 水分散型感圧性接着剤組成物 | |
| JPS6143394B2 (en:Method) | ||
| JPH0527669B2 (en:Method) | ||
| JPS6011569A (ja) | 再剥離性粘着剤組成物およびその製造法 | |
| JPS5822492B2 (ja) | 感圧接着剤 | |
| JPS63260973A (ja) | 微球状感圧性接着剤の製造方法 | |
| JPH0623364B2 (ja) | 水分散型感圧性接着剤組成物 | |
| JPH0352981A (ja) | 接着剤組成物 | |
| JPS6149350B2 (en:Method) | ||
| JPH0579272B2 (en:Method) | ||
| JP2582768B2 (ja) | 水分散型感圧性接着剤組成物の製造法 |