JPS6117895B2 - - Google Patents
Info
- Publication number
- JPS6117895B2 JPS6117895B2 JP14822582A JP14822582A JPS6117895B2 JP S6117895 B2 JPS6117895 B2 JP S6117895B2 JP 14822582 A JP14822582 A JP 14822582A JP 14822582 A JP14822582 A JP 14822582A JP S6117895 B2 JPS6117895 B2 JP S6117895B2
- Authority
- JP
- Japan
- Prior art keywords
- components
- sulfide
- lubricating
- alloy
- hard
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired
Links
Landscapes
- Powder Metallurgy (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP14822582A JPS5938350A (ja) | 1982-08-26 | 1982-08-26 | 摩擦部材および摺動部材用焼結Al合金 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP14822582A JPS5938350A (ja) | 1982-08-26 | 1982-08-26 | 摩擦部材および摺動部材用焼結Al合金 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS5938350A JPS5938350A (ja) | 1984-03-02 |
JPS6117895B2 true JPS6117895B2 (en, 2012) | 1986-05-09 |
Family
ID=15448070
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP14822582A Granted JPS5938350A (ja) | 1982-08-26 | 1982-08-26 | 摩擦部材および摺動部材用焼結Al合金 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS5938350A (en, 2012) |
Families Citing this family (8)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS616243A (ja) * | 1984-06-19 | 1986-01-11 | Mitsubishi Metal Corp | 耐摩耗性のすぐれたAl焼結合金製摺動部材 |
JPS61152874A (ja) * | 1984-12-24 | 1986-07-11 | 東レ株式会社 | 機能性薬剤がドツト状に付与された繊維シ−ト |
US4902576A (en) * | 1985-10-17 | 1990-02-20 | Kabushiki Kaisha Toyoto Chuo Kenkyusho | High temperature sliding element and method for preventing high temperature sliding wear |
JPH0714386Y2 (ja) * | 1989-05-23 | 1995-04-05 | セーレン電子株式会社 | インクジェット方式の捺染装置 |
AUPN273695A0 (en) * | 1995-05-02 | 1995-05-25 | University Of Queensland, The | Aluminium alloy powder blends and sintered aluminium alloys |
JPH10103373A (ja) * | 1996-08-06 | 1998-04-21 | Toyota Motor Corp | 湿式摩擦接触装置 |
JP4871713B2 (ja) * | 2006-12-07 | 2012-02-08 | 王子インターパック株式会社 | 段ボール製梱包材用連結部材 |
CN113564406A (zh) * | 2021-06-23 | 2021-10-29 | 中铁隆昌铁路器材有限公司 | 一种高熔点合金增强铜基粉末冶金摩擦材料及其制备方法 |
-
1982
- 1982-08-26 JP JP14822582A patent/JPS5938350A/ja active Granted
Also Published As
Publication number | Publication date |
---|---|
JPS5938350A (ja) | 1984-03-02 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
EP0202035B1 (en) | Wear-resistant, sintered iron alloy and process for producing the same | |
US5498483A (en) | Wear-resistant sintered ferrous alloy for valve seat | |
JPS6117895B2 (en, 2012) | ||
JPS6038461B2 (ja) | 耐摩性に優れた焼結合金 | |
JP3682556B2 (ja) | 耐熱・耐摩耗性焼結ステンレス鋼 | |
JPS5881954A (ja) | 耐摩耗性および自己潤滑性にすぐれた高強度鉄基焼結合金 | |
JPS6154856B2 (en, 2012) | ||
JP2556114B2 (ja) | 耐摩耗性のすぐれた高強度高靭性Cu基焼結合金 | |
JPS5941432A (ja) | 摺動部材用焼結Al合金 | |
JPS626737B2 (en, 2012) | ||
JP2606335B2 (ja) | 耐摩耗性のすぐれた高強度高靭性Cu基焼結合金 | |
JPS6154855B2 (en, 2012) | ||
JPS62127454A (ja) | 耐摩耗性複合焼結材 | |
JPH01212737A (ja) | 耐摩耗性鉄系焼結合金 | |
JP2705376B2 (ja) | 高強度高靭性を有するFe基焼結合金製バルブシート | |
JP3257196B2 (ja) | 強度および耐摩耗性に優れた摺動部材用鉄基焼結合金 | |
JPH0543998A (ja) | 相手攻撃性のきわめて低い金属充填Fe基焼結合金製バルブシート | |
KR0118773B1 (ko) | 밸브시이트용 철계 소결합금 | |
JP2697171B2 (ja) | 高温で耐摩耗性にすぐれた銅基焼結合金 | |
JPS6140027B2 (en, 2012) | ||
RU2006511C1 (ru) | Порошковый материал на основе меди | |
JPS5937735B2 (ja) | 耐摩耗性焼結合金 | |
JP2556113B2 (ja) | 耐摩耗性のすぐれた高強度高靭性Cu基焼結合金 | |
JP2606327B2 (ja) | 耐摩耗性のすぐれた高強度高靭性Cu基焼結合金 | |
JPS62133043A (ja) | Cu含浸Fe系焼結材料 |