JPS6081765A - ペ−スト式カドミウム陰極板の製造方法 - Google Patents
ペ−スト式カドミウム陰極板の製造方法Info
- Publication number
- JPS6081765A JPS6081765A JP58190444A JP19044483A JPS6081765A JP S6081765 A JPS6081765 A JP S6081765A JP 58190444 A JP58190444 A JP 58190444A JP 19044483 A JP19044483 A JP 19044483A JP S6081765 A JPS6081765 A JP S6081765A
- Authority
- JP
- Japan
- Prior art keywords
- electrode plate
- cadmium
- electrode
- active material
- carbon powder
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Classifications
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M4/24—Electrodes for alkaline accumulators
- H01M4/246—Cadmium electrodes
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M10/00—Secondary cells; Manufacture thereof
- H01M10/42—Methods or arrangements for servicing or maintenance of secondary cells or secondary half-cells
- H01M10/52—Removing gases inside the secondary cell, e.g. by absorption
- H01M10/526—Removing gases inside the secondary cell, e.g. by absorption by gas recombination on the electrode surface or by structuring the electrode surface to improve gas recombination
-
- H—ELECTRICITY
- H01—ELECTRIC ELEMENTS
- H01M—PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01M4/00—Electrodes
- H01M4/02—Electrodes composed of, or comprising, active material
- H01M2004/026—Electrodes composed of, or comprising, active material characterised by the polarity
- H01M2004/027—Negative electrodes
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y02—TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
- Y02E—REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02E60/00—Enabling technologies; Technologies with a potential or indirect contribution to GHG emissions mitigation
- Y02E60/10—Energy storage using batteries
Landscapes
- Chemical & Material Sciences (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Electrochemistry (AREA)
- General Chemical & Material Sciences (AREA)
- Battery Electrode And Active Subsutance (AREA)
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP58190444A JPS6081765A (ja) | 1983-10-12 | 1983-10-12 | ペ−スト式カドミウム陰極板の製造方法 |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JP58190444A JPS6081765A (ja) | 1983-10-12 | 1983-10-12 | ペ−スト式カドミウム陰極板の製造方法 |
Publications (2)
Publication Number | Publication Date |
---|---|
JPS6081765A true JPS6081765A (ja) | 1985-05-09 |
JPH0234434B2 JPH0234434B2 (fr) | 1990-08-03 |
Family
ID=16258232
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
JP58190444A Granted JPS6081765A (ja) | 1983-10-12 | 1983-10-12 | ペ−スト式カドミウム陰極板の製造方法 |
Country Status (1)
Country | Link |
---|---|
JP (1) | JPS6081765A (fr) |
Cited By (3)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS62136764A (ja) * | 1985-12-09 | 1987-06-19 | Matsushita Electric Ind Co Ltd | ペ−スト式カドミウム負極の製造法 |
JPS63138651A (ja) * | 1986-11-28 | 1988-06-10 | Matsushita Electric Ind Co Ltd | ペ−スト式カドミウム負極 |
JPS63158747A (ja) * | 1986-12-22 | 1988-07-01 | Matsushita Electric Ind Co Ltd | ペ−スト式カドミウム負極 |
Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS51150641A (en) * | 1975-06-20 | 1976-12-24 | Japan Storage Battery Co Ltd | Zinc plate for sealed alkaline battery |
JPS5636782A (en) * | 1979-09-04 | 1981-04-10 | Seiko Instr & Electronics Ltd | Print control system of dot printer |
-
1983
- 1983-10-12 JP JP58190444A patent/JPS6081765A/ja active Granted
Patent Citations (2)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS51150641A (en) * | 1975-06-20 | 1976-12-24 | Japan Storage Battery Co Ltd | Zinc plate for sealed alkaline battery |
JPS5636782A (en) * | 1979-09-04 | 1981-04-10 | Seiko Instr & Electronics Ltd | Print control system of dot printer |
Cited By (5)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
JPS62136764A (ja) * | 1985-12-09 | 1987-06-19 | Matsushita Electric Ind Co Ltd | ペ−スト式カドミウム負極の製造法 |
JPS63138651A (ja) * | 1986-11-28 | 1988-06-10 | Matsushita Electric Ind Co Ltd | ペ−スト式カドミウム負極 |
JPH0546662B2 (fr) * | 1986-11-28 | 1993-07-14 | Matsushita Electric Ind Co Ltd | |
JPS63158747A (ja) * | 1986-12-22 | 1988-07-01 | Matsushita Electric Ind Co Ltd | ペ−スト式カドミウム負極 |
JPH0555980B2 (fr) * | 1986-12-22 | 1993-08-18 | Matsushita Electric Ind Co Ltd |
Also Published As
Publication number | Publication date |
---|---|
JPH0234434B2 (fr) | 1990-08-03 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
JP2003249223A (ja) | リチウムイオン二次電池およびその製造方法 | |
JPS6081765A (ja) | ペ−スト式カドミウム陰極板の製造方法 | |
JPS61208755A (ja) | 密閉型アルカリ蓄電池用ペ−スト式カドミウム陰極板 | |
JPS6063875A (ja) | 密閉型アルカリ蓄電池用ペ−スト式カドミウム陰極板 | |
JPS63170851A (ja) | アルカリ蓄電池用カドミウム極 | |
JP2558759B2 (ja) | アルカリ蓄電池用カドミウム負極の製造法 | |
JP2773253B2 (ja) | アルカリ蓄電池用カドミウム負極の製造法 | |
JPH0837001A (ja) | 鉛蓄電池用正極板及びその製造方法 | |
JP3397216B2 (ja) | ニッケル極板とその製造方法およびこれを用いたアルカリ蓄電池 | |
JPH0775163B2 (ja) | 電池用カドミウム極の製造法 | |
JPH0582027B2 (fr) | ||
FI70490C (fi) | Elektroder foer blyackumulator samt foerfarande foer framstaellning av en elektrod | |
JP3018879B2 (ja) | ペースト式カドミウム負極の化成法 | |
JPH07320726A (ja) | 高分子固体電解質電池用負極材の製造方法 | |
JP2529308B2 (ja) | アルカリ蓄電池用カドミウム負極の製造法 | |
CN111435730A (zh) | 在以铅为基础的基材上形成铅碳化合物界面层的方法 | |
JPH0234433B2 (fr) | ||
JP3196234B2 (ja) | アルカリ蓄電池用カドミウム負極板とその製造方法 | |
JPH0439861A (ja) | ニッケル亜鉛蓄電池の製造法 | |
JPS62136764A (ja) | ペ−スト式カドミウム負極の製造法 | |
JPS6210860A (ja) | 酸化銀電池 | |
JPS63128557A (ja) | ニツケル−カドミウム電池 | |
JPS6211455B2 (fr) | ||
JPS62136763A (ja) | ペ−スト式カドミウム負極の製造法 | |
JPS60140656A (ja) | アルカリ蓄電池用カドミウム陰極板の製造法 |