JPS60222176A - 粗悪素地に対する塗装方法 - Google Patents
粗悪素地に対する塗装方法Info
- Publication number
- JPS60222176A JPS60222176A JP4741685A JP4741685A JPS60222176A JP S60222176 A JPS60222176 A JP S60222176A JP 4741685 A JP4741685 A JP 4741685A JP 4741685 A JP4741685 A JP 4741685A JP S60222176 A JPS60222176 A JP S60222176A
- Authority
- JP
- Japan
- Prior art keywords
- oil
- rust
- paint
- painting
- component
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Links
Landscapes
- Application Of Or Painting With Fluid Materials (AREA)
Priority Applications (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP4741685A JPS60222176A (ja) | 1985-03-12 | 1985-03-12 | 粗悪素地に対する塗装方法 |
Applications Claiming Priority (1)
| Application Number | Priority Date | Filing Date | Title |
|---|---|---|---|
| JP4741685A JPS60222176A (ja) | 1985-03-12 | 1985-03-12 | 粗悪素地に対する塗装方法 |
Publications (2)
| Publication Number | Publication Date |
|---|---|
| JPS60222176A true JPS60222176A (ja) | 1985-11-06 |
| JPH0252550B2 JPH0252550B2 (enExample) | 1990-11-13 |
Family
ID=12774543
Family Applications (1)
| Application Number | Title | Priority Date | Filing Date |
|---|---|---|---|
| JP4741685A Granted JPS60222176A (ja) | 1985-03-12 | 1985-03-12 | 粗悪素地に対する塗装方法 |
Country Status (1)
| Country | Link |
|---|---|
| JP (1) | JPS60222176A (enExample) |
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| KR20010002974A (ko) * | 1999-06-18 | 2001-01-15 | 김영 | 철근의 부식방지 및 접착력 향상을 위한 피막 도포방법 |
| CN114405728A (zh) * | 2021-12-08 | 2022-04-29 | 中圳特种钢材(江苏)有限公司 | 螺纹钢防腐涂层喷涂装置、系统及方法 |
-
1985
- 1985-03-12 JP JP4741685A patent/JPS60222176A/ja active Granted
Cited By (2)
| Publication number | Priority date | Publication date | Assignee | Title |
|---|---|---|---|---|
| KR20010002974A (ko) * | 1999-06-18 | 2001-01-15 | 김영 | 철근의 부식방지 및 접착력 향상을 위한 피막 도포방법 |
| CN114405728A (zh) * | 2021-12-08 | 2022-04-29 | 中圳特种钢材(江苏)有限公司 | 螺纹钢防腐涂层喷涂装置、系统及方法 |
Also Published As
| Publication number | Publication date |
|---|---|
| JPH0252550B2 (enExample) | 1990-11-13 |
Similar Documents
| Publication | Publication Date | Title |
|---|---|---|
| KR960704985A (ko) | 점착이 잘되고 부식을 방지하는 래커층을 만드는 간단한 방법 및 그 기초 부분품(simplified process for producing an anticorrosive paint with a good adhesiveness and workpieces thus obtained) | |
| CN105149195A (zh) | 一种新型钢结构油漆施工工艺 | |
| CN104151918A (zh) | 一种中性环保脱漆剂 | |
| US3438799A (en) | Method for the surface treatment of metal articles | |
| US6248403B1 (en) | Environmental wipe solvent processes | |
| JPS60222176A (ja) | 粗悪素地に対する塗装方法 | |
| JP2599467B2 (ja) | 亜鉛めっき鋼材の表面処理方法および表面処理組成物 | |
| CN107552363A (zh) | 一种油漆涂装工艺 | |
| CN102896082B (zh) | 一种涂装工艺 | |
| JPS60232277A (ja) | 粗悪素地に対する塗装法 | |
| US5284510A (en) | Organic solvent based liquid composition for enhancing adherence of coatings to substrates | |
| KR100956841B1 (ko) | 구도막의 재도장방법 및 이를 이용한 도장막 | |
| DE102004007361B4 (de) | Verfahren zur Modifizierung von verzinkten Stahloberflächen und Schwarzstahloberflächen | |
| JPH04283280A (ja) | 金属材の塗装方法及び金属材用塗料 | |
| JPS62168574A (ja) | 水中塗装下地処理方法 | |
| US6379750B1 (en) | Process for enhancing the adhesion of organic coatings to metal surfaces | |
| DE1913588B2 (de) | Verfahren zum entfernen von polierrueckstaenden unter einsatz einer filmbildenden schutzschicht | |
| CN115433504A (zh) | 不锈钢表面防腐处理剂及处理方法 | |
| JPS633024B2 (enExample) | ||
| JPS5913904B2 (ja) | 塗装方法 | |
| GB2138703A (en) | Process for protecting metals against corrosion | |
| JPH09206675A (ja) | 錆面の防食方法 | |
| Christofferson | Coatings for Steel Water Storage Tanks | |
| JPS60197272A (ja) | 塗膜剥離方法 | |
| JP4450588B2 (ja) | 金属面の塗装方法 |