JPS59174625A - 重合体ラテツクスの凝固方法 - Google Patents

重合体ラテツクスの凝固方法

Info

Publication number
JPS59174625A
JPS59174625A JP4844783A JP4844783A JPS59174625A JP S59174625 A JPS59174625 A JP S59174625A JP 4844783 A JP4844783 A JP 4844783A JP 4844783 A JP4844783 A JP 4844783A JP S59174625 A JPS59174625 A JP S59174625A
Authority
JP
Japan
Prior art keywords
latex
nozzle
substrate
coagulating
coagulation
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
JP4844783A
Other languages
English (en)
Japanese (ja)
Other versions
JPH0365376B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html
Inventor
Teruhiko Sugimori
輝彦 杉森
Takayuki Tajiri
象運 田尻
Akio Hironaka
弘中 章夫
Hideaki Habara
英明 羽原
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Mitsubishi Chemical Corp
Original Assignee
Mitsubishi Rayon Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Mitsubishi Rayon Co Ltd filed Critical Mitsubishi Rayon Co Ltd
Priority to JP4844783A priority Critical patent/JPS59174625A/ja
Priority to CA000449872A priority patent/CA1241797A/en
Priority to EP84103111A priority patent/EP0120456B1/en
Priority to DE8484103111T priority patent/DE3480991D1/de
Priority to US06/592,365 priority patent/US4744744A/en
Publication of JPS59174625A publication Critical patent/JPS59174625A/ja
Priority to US07/226,526 priority patent/US4910850A/en
Publication of JPH0365376B2 publication Critical patent/JPH0365376B2/ja
Granted legal-status Critical Current

Links

Landscapes

  • Addition Polymer Or Copolymer, Post-Treatments, Or Chemical Modifications (AREA)
  • Processes Of Treating Macromolecular Substances (AREA)
JP4844783A 1983-03-22 1983-03-23 重合体ラテツクスの凝固方法 Granted JPS59174625A (ja)

Priority Applications (6)

Application Number Priority Date Filing Date Title
JP4844783A JPS59174625A (ja) 1983-03-23 1983-03-23 重合体ラテツクスの凝固方法
CA000449872A CA1241797A (en) 1983-03-22 1984-03-19 Method for coagulation of polymer latices and extruder therefor
EP84103111A EP0120456B1 (en) 1983-03-22 1984-03-21 Method for coagulation of polymer latices and extruder therefor
DE8484103111T DE3480991D1 (de) 1983-03-22 1984-03-21 Verfahren zur koagulation von polymerlatex und geeigneter extruder.
US06/592,365 US4744744A (en) 1983-03-22 1984-03-22 Extrusion nozzle for coagulation of polymer latices
US07/226,526 US4910850A (en) 1983-03-22 1988-08-01 Method for coagulation of a polymer latex

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP4844783A JPS59174625A (ja) 1983-03-23 1983-03-23 重合体ラテツクスの凝固方法

Publications (2)

Publication Number Publication Date
JPS59174625A true JPS59174625A (ja) 1984-10-03
JPH0365376B2 JPH0365376B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) 1991-10-11

Family

ID=12803597

Family Applications (1)

Application Number Title Priority Date Filing Date
JP4844783A Granted JPS59174625A (ja) 1983-03-22 1983-03-23 重合体ラテツクスの凝固方法

Country Status (1)

Country Link
JP (1) JPS59174625A (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html)

Also Published As

Publication number Publication date
JPH0365376B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html) 1991-10-11

Similar Documents

Publication Publication Date Title
PL105366B1 (pl) Sposob wytwarzania przedmieszek sadzowo-kauczukowych
US6610798B1 (en) Controlled suspension polymerization process without mechanical agitation
JPS6322805A (ja) ポリオレフィンのガス抜きおよびペレット化の方法および装置
US4429114A (en) Method for treating emulsified latex
US4744744A (en) Extrusion nozzle for coagulation of polymer latices
JPS59174625A (ja) 重合体ラテツクスの凝固方法
EP1389625A1 (en) Method of dispersion of a non-newtonian fluid
JPS6134064A (ja) 水性分散体およびその製法
JPS59199704A (ja) 重合体ラテツクスの凝固方法
US4277426A (en) Method for production of coagulated synthetic polymer latex
JPS59182801A (ja) 重合体ラテツクスの凝固方法
JPS59230004A (ja) 重合体ラテツクスの凝固方法
JPH0365375B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html)
JP3411070B2 (ja) 重合体粉体の製造方法
JPH0457374B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html)
JPH0459010B2 (GUID-C5D7CC26-194C-43D0-91A1-9AE8C70A9BFF.html)
CN111941681A (zh) 一种生产聚苯乙烯均球的装置和方法
JP3970954B2 (ja) ゴム強化スチレン系樹脂の製造方法
US3993536A (en) Method for preparing synthetic powders based on polyvinyl chloride or vinyl chloride copolymers containing emulsifiers
JPS6042427A (ja) 熱可塑性樹脂の製造装置
JPH01123852A (ja) ゴム変性熱可塑性樹脂の製造法
KR19990037423A (ko) 열가소성 고분자와 첨가제의 드라이블랜드 제조방법 및 장치
JPS6042428A (ja) 熱可塑性樹脂の製造装置
JP2560032B2 (ja) 粒状体の製造方法
JPS56106925A (en) Solidification of polymer latex